| CRYSTALLIZATION OF AMORPHOUS ALLOY Fe_(78)B_(13)Si_9 INDUCED BY SHOCK WAVE |
| LIU Zuoquan; ZHAO Heyun; LU Yusong; LI Dexiu; LI Hin; ZHANG Shubo (Yunnan Univereity; Kunming 650091)(Manuscript received 1995-11-13; in revised form 1996-04-04) |
|
Cite this article:
LIU Zuoquan; ZHAO Heyun; LU Yusong; LI Dexiu; LI Hin; ZHANG Shubo (Yunnan Univereity; Kunming 650091)(Manuscript received 1995-11-13; in revised form 1996-04-04). CRYSTALLIZATION OF AMORPHOUS ALLOY Fe_(78)B_(13)Si_9 INDUCED BY SHOCK WAVE. Acta Metall Sin, 1996, 32(8): 862-866.
|
|
|
Abstract The effect of shock wave on the structure of amorphous alloy Fe78B13Si9 has been studied by means of XRD and DTA. It has been found that under the effect of some strong shock wave, this amorphous alloy has been transformed into a crystailine phase with nanometer sized grains. Corresponaent:(LIU Zuoquan, professor, Department of Physics, Yunnan University , Kunming 650091)
|
|
Received: 18 August 1996
|
| 1ChaoECT.Science.1967:156:1922BancroftD,PetersonEL,MinshallFS.JApplPhys,1956;27:2913ZukasEG.MetEngQ,1966;6:164MahajanS.PhysStatusSolid,1970;2a:1865LeslieWC.In:RohdeRW,ButcherBM,HollandJR,KarnesCHeds.,MetallurgicalEffectsatHighStrainRates,NewYork:Plenum1973:5716MurrLE.In:MeyerMA,MuirLEeds.,ShockWavesandHikhStrainRatePhenomenainMetals,NewYork:Plenum,1981:6077MurrLE.In:BlaznskiTZed.,MaterialsatHighStrainRates,London:AppliedScience,1987:18StandhammerKP.In:ChiemCY,KunzeHD,MeyerLWeds.,IMPACT1987,Oberursel,WestGermany:DuetscheGesellkundefurMetallkunde,1988:839DonnevalR,PerraudJ,RemiotC.In:SawaokaABed.,ShockWavesinMaterialScience,Heidelberg,Germany:Springer-Verlag,1993:99710NesterenkoVF.In:MeyerMA,MurrLEeds.,ShockWavesandHighStrainRatePhenomenainMetals,Chap75,NewYork:Plenum,1981:80911KippME,GradyDE,WiseJL.In:MeyerMA,MurrLEeds.,ShockWavesandHighStrainRatePhenomenainMetals,Chap103,NewYork:Plenum1981:108312DreminAN,BreusovON.In:SawaokaABed.,ShockWavesinMaterialScience.Heidelberg,Germany:Springer- |