M SSBAUER SPECTRA OF FOUR Fe-BASED ALLOYS
WANG Kuixiang; HAO Zhaoyin; DENG Jingchuan; LIU Milan; LU Guohui(Jilin University; Changchun 130073)(Manuscript received 1995-06-19; in revised form 1995-09-16)
Cite this article: 

WANG Kuixiang; HAO Zhaoyin; DENG Jingchuan; LIU Milan; LU Guohui(Jilin University; Changchun 130073)(Manuscript received 1995-06-19; in revised form 1995-09-16). M SSBAUER SPECTRA OF FOUR Fe-BASED ALLOYS. Acta Metall Sin, 1996, 32(5): 469-473.

Download:  PDF(372KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Mssbauer spectra of four Fe-based alloys before and after quenching at high temperature and high pressure were studied and the relationships of the hyporfine field H(nf),magnetization M and correlated parametiers to electron concentration of alloys have been obtained. Based on Stoner's rigid band model the variational regulations of H(nf)and M for the carburized alloys were discussed. It was revealed that the 2p electrons of carbon atom filled the 3d holes of iron atom, and there exists Fe-C bond.
Key words:  Mssbauer spectrum      Fe-based alloy      high temperature and high pressure     
Received:  18 May 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I5/469

1GonserU著,徐英庭,李哲,李国栋,应育浦译.穆斯堡尔谱学.北京:科学出版社,1979:1082HaoZhaoyin,HeYixing,ChenYufei,WanDerong.JCrystGrowth.,1994;140:4413HuckB,SaurenbachF,HesseJ.HyperfineInteract,1986;28:4794郝兆印,王魁香.高压物理学报,1991;5:1775LomerWM,MarshallW.PhilosMag.1958;3:1856SonmuraT,FujitaFE.JMagnMagnMater,1979;10:2557AdachiH,ImotoS.JPhysSocJpn,1979;46:1194T
[1] Li FAN, Haiyan CHEN, Yaohua DONG, Xueying LI, Lihua DONG, Yansheng YIN. Corrosion Behavior of Fe-Based Laser Cladding Coating in Hydrochloric Acid Solutions[J]. 金属学报, 2018, 54(7): 1019-1030.
[2] Lining XU,Bei WANG,Minxu LU. CORROSION BEHAVIOR OF 6.5%Cr STEEL IN HIGH TEMPERATURE AND HIGH PRESSURE CO2 ENVIRONMENT[J]. 金属学报, 2016, 52(6): 672-678.
[3] ZHANG Litao,WANG Jianqiu. STRESS CORROSION CRACK PROPAGATION BEHAVIOR OF DOMESTIC FORGED NUCLEAR GRADE 316L STAINLESS STEEL IN HIGH TEMPERATURE AND HIGH PRESSURE WATER[J]. 金属学报, 2013, 49(8): 911-916.
[4] LI Xiaohui WANG Jianqiu HAN En–Hou KE Wei. CORROSION BEHAVIOR OF NUCLEAR GRADE ALLOYS 690 AND 800 IN SIMULATED HIGH TEMPERATURE AND HIGH PRESSURE PRIMARY WATER OF PRESSURIZED WATER REACTOR[J]. 金属学报, 2012, 48(8): 941-950.
[5] LI Xiaohui HUANG Fa WANG Jianqiu HAN En-Hou KE Wei. INFLUENCES OF TiN INCLUSION ON CORROSION AND STRESS CORROSION BEHAVIORS OF ALLOY 690 TUBE IN HIGH TEMPERATURE AND HIGH PRESSURE WATER[J]. 金属学报, 2011, 47(7): 847-852.
[6] XU Bin; CUI Jianjun; WANG Shuhua; LI Musen; LI Chengmei; FENG Liming. Fine Structures Of The Fe--Based Metal Film Covering Synthetic Diamond Single Crystal[J]. 金属学报, 2005, 41(4): 444-448 .
No Suggested Reading articles found!