Please wait a minute...
Acta Metall Sin  1996, Vol. 32 Issue (2): 187-190    DOI:
Current Issue | Archive | Adv Search |
STUDY ON THE OXIDATION KINETICS OF WS_2 IN OPEN AIR
XING Pengfei; ZHAI Yuchun; TIAN Yanwen; GENG Yan; CHEN Feng(Northeastern University; Shenyang 110006)(Manuscript received 1995-04-24; in revised form 1995-10-16)
Cite this article: 

XING Pengfei; ZHAI Yuchun; TIAN Yanwen; GENG Yan; CHEN Feng(Northeastern University; Shenyang 110006)(Manuscript received 1995-04-24; in revised form 1995-10-16). STUDY ON THE OXIDATION KINETICS OF WS_2 IN OPEN AIR. Acta Metall Sin, 1996, 32(2): 187-190.

Download:  PDF(259KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The DTA and XRD techniques were employed to study the oxidation process of highly pure WS_2. The activation energy, 100.l kJ / mol, and the orders of oxidation reaction, 0.80,have been obtained according to Doyle-Ozawa and Kissinger methods.The oxidation reaction occurs mainly in steps of:WS_2→W_3O→WO_2→W_(18)O_(49)→WO_(2.9)→WO_3(Correspondent: XING Pengfei, Department of Non-Ferrous Metallurgy, Northeastern University, Shenyang 110006)
Key words:  WS_2      oxidation kinetics      DTA      XRD     
Received:  18 February 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I2/187

1津谷裕子,北村守:润滑.1974.19.8432JonesJK,GardosM.LubEng,1973:29:473邢鹏飞,翟玉春,田彦文.化工冶金.1995:16:2194OzawaT,BullChemSocJpn.1965;38:18815DoyleCD,JapplPolymerSci,1965;5:2886KissingerHE.JResNatBurStand,1965;57:2177KissingerHE.AnalChem,1957;29:1702
[1] Yin BAI, Zhengdong LIU, Jianxin XIE, Hansheng BAO, Zhengzong CHEN. Effect of Pre-Oxidation Treatment on the Behavior of High Temperature Oxidation in Steam of G115 Steel[J]. 金属学报, 2018, 54(6): 895-904.
[2] Jintao SHI,Longgang HOU,Jinrong ZUO,Lin LU,Hua CUI,Jishan ZHANG. QUANTITATIVE ANALYSIS OF THE MARTENSITE TRANSFORMATION AND MICROSTRUCTURE CHARACTERIZATION DURING CRYOGENIC ROLLING OF A 304 AUSTENITIC STAINLESS STEEL[J]. 金属学报, 2016, 52(8): 945-955.
[3] Wenying ZHANG, Jun LI, Bo ZHOU. OXIDATION KINETICS BEHAVIOR AND ELECTRICAL PROPERTY OF MnCO2O4 SPINEL AS A COATING MATERIAL FOR METALLIC INTERCONNECTS[J]. 金属学报, 2016, 52(3): 355-360.
[4] MA Ping, WU Erdong, LI Wuhui, SUN Kai, CHEN Dongfeng. MICROSTRUCTURES AND HYDROGEN STORAGE PROPERTIES OF Ti0.7Zr0.3(Cr1-xVx)2 ALLOYS[J]. 金属学报, 2014, 50(4): 454-462.
[5] QIU Jun ZHAO Wenjin Thomas Guilbert Jean-Luc Bechade. HIGH TEMPERATURE OXIDATION BEHAVIOURS OF THREE ZIRCONIUM ALLOYS[J]. 金属学报, 2011, 47(9): 1216-1220.
[6] WANG Youdao WU Erdong WANG Sucheng LI Wuhui. X-RAY DIFFRACTION ANALYSIS ON THE THICKNESS EFFECT OF γ/γ' LATTICE MISMATCHE IN NICKEL BASE SINGLE CRYSTAL SUPERALLOY DD10[J]. 金属学报, 2011, 47(11): 1418-1425.
[7] . [J]. 金属学报, 2007, 43(6): 625-630 .
[8] Hui XU. CU/AL INTERMETALLIC COMPOUNDS FORMATION ON CU BALL AND AL ALLOY PAD BONDING JOINT DURING THERMAL AGING[J]. 金属学报, 2007, 43(2): 125-130 .
[9] HONG Bo; JIANG Chuanhai; WANG Xinjian; WU Jiansheng. Phase transformation behaviour and kinetics of electrodeposition Ni-P amorphous alloys by X-ray analysis[J]. 金属学报, 2006, 42(7): 699-702 .
[10] LI Xiangyang;ZHANG Yonggang;CHEN Changqi(Beijing University of Aeronautics andAstronautics; Beijing 100083); ZHANG Xiaoji;ZHANG Tonghe;ZHANG Huixing (Beijing Normal University; Beiing 100875). OXIDATION MECHANISM OF BINARY Ti-Al ALLOYS AT ELEVATED TEMPERATURE[J]. 金属学报, 1997, 33(9): 964-970.
[11] TAO Kun;LI Bin;LUO Jian (Tsinghua University; Beijing 100084). A STUDY OF INTERDIFFUSION OF Pd/Ag BILAYER THIN FILMS BY X-RAY DIFFRACTION STRUCTURE DEPTH PROFILING[J]. 金属学报, 1997, 33(7): 742-748.
[12] WEI Jihe (Shanghai Univereity.of Technology);LIU Zongyuan(Xi'van Institute of Metallurgy Construction Engineering). STUDY ON OXYGEN TRANSFER THROUGH MOLTEN SLAGS OF CaF_2+Al_2O_3 AND CaF_2+Al_2O_3+CaO SYSTEMS FOR ESR[J]. 金属学报, 1994, 30(20): 350-360.
[13] LIU Shuqi;YI Tao Department of Chemistry; Peking University; Beijing. LIQUIDUS OF Au-Cu-Si SYSTEM[J]. 金属学报, 1990, 26(4): 153-154.
No Suggested Reading articles found!