Please wait a minute...
Acta Metall Sin  1996, Vol. 32 Issue (12): 1244-1247    DOI:
Current Issue | Archive | Adv Search |
MECHANISM OF SUPERPLASTIC DEFORMATION IN ALUMINIUM ALLOY 2214
LIU Runguang;JIANG Haomin;JIANG Yong(Harbin Institute of Technology;Harbin 150001);PENG Fulin;YIN Fulin;ZHANG Hongzheng(Harbin Aeroplane Manufacture Coporation;Harbin 150066)(Manuscript received 1995-01-31;in revised form 1996-03-25)
Cite this article: 

LIU Runguang;JIANG Haomin;JIANG Yong(Harbin Institute of Technology;Harbin 150001);PENG Fulin;YIN Fulin;ZHANG Hongzheng(Harbin Aeroplane Manufacture Coporation;Harbin 150066)(Manuscript received 1995-01-31;in revised form 1996-03-25). MECHANISM OF SUPERPLASTIC DEFORMATION IN ALUMINIUM ALLOY 2214. Acta Metall Sin, 1996, 32(12): 1244-1247.

Download:  PDF(329KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  During the superplastic deformation of warm-rolled aluminium alloy 2214,the dislocation density in the grain remains equilibration to some extent because of the effect of dynamic recovery and recrystallization. The dominant deformation mechanism is grain-boundary sliding.The dislocation sliding in grain and diffusion creep, as two kinds of important coordination mechanism,promote the development of grain-boundary sliding.The superplastic deformation mechanism accords with the model of dislocation coordinating grain-boundary sliding.
Key words:  aluminium alloy      superplasticity      grain-boundary sliding     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I12/1244

1LiuQ,YaoM.ScrMetatll,1995;32:18572SrinivasanMN,GoforthRE.ScFMetall,1995;32:18613陈浦泉.组织超塑性.哈尔滨:哈尔滨工业大学出版社,1988:394高维林,白光润,栾瑰馥.东北工学院学报,1993;13:825高翔,沈豫立,黄承智.武汉工学院学报,1991:13:27V
[1] CHEN Junzhou, LV Liangxing, ZHEN Liang, DAI Shenglong. Precipitation Strengthening Model of AA 7055 Aluminium Alloy[J]. 金属学报, 2021, 57(3): 353-362.
[2] WANG Huiyuan, XIA Nan, BU Ruyu, WANG Cheng, ZHA Min, YANG Zhizheng. Current Research and Future Prospect on Low-Alloyed High-Performance Wrought Magnesium Alloys[J]. 金属学报, 2021, 57(11): 1429-1437.
[3] Guangming XIE, Zongyi MA, Peng XUE, Zongan LUO, Guodong WANG. Effects of Tool Rotation Rates on Superplastic Deformation Behavior of Friction Stir Processed Mg-Zn-Y-Zr Alloy[J]. 金属学报, 2018, 54(12): 1745-1755.
[4] Huiyuan WANG, Hang ZHANG, Xinyu XU, Min ZHA, Cheng WANG, Pinkui MA, Zhiping GUAN. Current Research and Future Prospect on Microstructure Stability of Superplastic Light Alloys[J]. 金属学报, 2018, 54(11): 1618-1624.
[5] Fenjun LIU, Li FU, Haiyan CHEN. Microstructures and Mechanical Properties of Thin Plate Aluminium Alloy Joint Prepared by High Rotational Speed Friction Stir Welding[J]. 金属学报, 2017, 53(12): 1651-1658.
[6] Wei GU,Jingyuan LI,Yide WANG. EFFECT OF GRAIN SIZE AND TAYLOR FACTOR ON THE TRANSVERSE MECHANICAL PROPERTIES OF 7050 ALUMINIUM ALLOY EXTRUSION PROFILE AFTER OVER-AGING[J]. 金属学报, 2016, 52(1): 51-59.
[7] Chao YANG,Jijie WANG,Zongyi MA,Dingrui NI,Mingjie FU,Xiaohua LI,Yuansong ZENG. FRICTION STIR WELDING AND LOW-TEMPERATURE SUPERPLASTICITY OF 7B04 Al SHEET[J]. 金属学报, 2015, 51(12): 1449-1456.
[8] FU Mingjie, HAN Xiuquan, WU Wei, ZHANG Jianwei. SUPERPLASTICITY RESEARCH OF Ti-23Al-17Nb ALLOY SHEET[J]. 金属学报, 2014, 50(8): 955-961.
[9] WANG Bo, WANG Xiaojiao, SONG Hui, YAN Jujie, QIU Tao, LIU Wenqing, LI Hui. STRENGTHENING EFFECTS OF MICROSTRUCTURE EVOLUTION DURING EARLY AGEING PROCESS IN Al-Mg-Si ALLOY[J]. 金属学报, 2014, 50(6): 685-690.
[10] ZHANG Yanbin, ZHANG Limin, ZHANG Jiwang, ZENG Jing. EFFECT OF ANODIZING TREATMENT ON BENDING FATIGUE PROPERTIES OF 2014-T6 ALUMINIUM ALLOY[J]. 金属学报, 2014, 50(6): 715-721.
[11] MA Pinkui, SONG Yuquan. BINOCULAR STEREO VISION MEASUREMENT RESEARCH FOR SUPERPLASTIC FREE BULGING[J]. 金属学报, 2014, 50(4): 471-478.
[12] GUAN Zhiping, MA Pinkui, SONG Yuquan. ANALYSIS OF FRACTURE DURING SUPERPLASTIC TENSION[J]. 金属学报, 2013, 49(8): 1003-1011.
[13] SHEN Jun, FENG Aihan. RECENT ADVANCES ON MICROSTRUCTURAL CONTROLLING AND HOT FORMING OF Ti2AlNb-BASED ALLOYS[J]. 金属学报, 2013, 49(11): 1286-1294.
[14] HOU Jieshan, ZHOU Lanzhang, GUO Jianting, YUAN Chao. APPLICATION OF ARTIFICIAL NEURAL NETWORK FOR PREDICTION OF SUPERPLASTIC  BEHAVIOUR IN NiAl ALLOYS[J]. 金属学报, 2013, 49(11): 1333-1338.
[15] SHENG Hai, DONG Chaofang, XIAO Kui, LI Xiaogang. LOCALIZED ELECTROCHEMICAL CHARACTERIZATION OF HIGH STRENGTH ALUMINIUM ALLOY AT THE CRACK TIP IN 3.5NaCl SOLUTION[J]. 金属学报, 2012, 48(4): 414-419.
No Suggested Reading articles found!