Please wait a minute...
Acta Metall Sin  1996, Vol. 32 Issue (10): 1075-1080    DOI:
Current Issue | Archive | Adv Search |
TRANSITIONAL LAYER OF PHASE INTERFACES IN Ti(C,N)-BASED CERMET
XIONG Weihao;HU Zhenhua;CUI Kun(State Key;Laboratory;of Dies Technology;Huazhong University of Science and Technology;Wuhan 430074)(State Key Laboratory of Dies Technology;Huazhong University of Science and Technology;Wuhan 430074)(Manuscript received 1996-04-26)
Cite this article: 

XIONG Weihao;HU Zhenhua;CUI Kun(State Key;Laboratory;of Dies Technology;Huazhong University of Science and Technology;Wuhan 430074)(State Key Laboratory of Dies Technology;Huazhong University of Science and Technology;Wuhan 430074)(Manuscript received 1996-04-26). TRANSITIONAL LAYER OF PHASE INTERFACES IN Ti(C,N)-BASED CERMET. Acta Metall Sin, 1996, 32(10): 1075-1080.

Download:  PDF(425KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The phase interfacial transition layer in Ti(C,N)-based cermet has been proved systematically by using TEM and EDAX.Experimental results show that there exist obviously a surrounding structure at the edge of carbonitride phase in Ti(C,N)-based cermet,it is a transitional phase.Ti(C,N)/Ni phase interface has no constant orientation relationship.W and Mo are basically concentrated in interface and there is a composition gradient of Ti,Ni,W and Mo in phase interface.HREM observation of interface reveals that in phase interface of Ti(C,N)-based cermet,the transitional layer has width of 8-10 nm and nanocrystalline structure.
Key words:  Ti(C      N)-based cermet      phase interfacial transition layer      composition gradient      nanocrystal.     
Received:  18 October 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I10/1075

1熊惟皓.华中理工大学博士学位论文,19942LaouiT,ZouH,VanderBiestO.RefractMetHardMater.1992;11(1):2073陈世朴,王永瑞.金属电子显微分析.北京:机械工业出版社,1982:1144熊惟皓,胡镇华,崔 .材料导报,1992;5:245张国军.机械工程材料,1990;14(3):4
[1] Mingfang WU,Fei LIU,Fengjiang WANG,Yanxin QIAO. INTERFACIAL REACTION AND STRENGTHENING MECHANISM OF CERAMIC MATRIX COMPOSITE JOINTS USING LIQUID PHASE DIFFUSION BONDING WITH AUXILIARY PULSE CURRENT[J]. 金属学报, 2015, 51(9): 1129-1135.
[2] WU Mingfang, KUANG Hongjin, WANG Fengjiang, LIN Hongxiang, XU Guoxiang. PARTIALLY TRANSIENT LIQUID PHASE-DIFFUSION BONDING ON Ti(C, N)-Al2O3 CERAMIC MATRIX COMPOSITES USING Zr/Cu/Zr AS INTERLAYER[J]. 金属学报, 2014, 50(5): 619-625.
[3] ;. Preparation of Ti(CxN1-x) thick films on titanium by plasma electrolytic carbonitriding[J]. 金属学报, 2008, 44(9): 1105-1110 .
[4] WANG Quanzhao; LIU Yue; GUAN Dehui; YU Baohai; CHEN Zhiliang; BI Jing. Effect of tin content on microstructures and mechanical properties of Ti(C,N)/NiCr cermets[J]. 金属学报, 2005, 41(11): 1121-1126 .
[5] XIONG Weihao;HU Zhenhua;CUI Kun (State Key Laboratory of Dies Technology;Huazhong University of Science and Technology; Wuhan 430074). FORMATION MECHANISM OF MICROCRYSTAL INTERFACE LAYER IN Ti(C, N)-BASED CERMET[J]. 金属学报, 1997, 33(5): 473-478.
[6] LIU Ning; ZHAO Hingzhong; JIANG Laizhu; LUO Huiguo; HU Zhenhua; CUI Kun(Huazhong University of Science and Technology; Wuhan 430074). TRANSVERSE RUPTURE STRENGTH OF Ni BONDED Ti(C, N) CERMET AND FRACTAL DIMENSION ANALYSIS OF ITS FRACTURE SURFACES[J]. 金属学报, 1995, 31(5): 229-235.
[7] XU Kewei; BAI Chendong; HE Jiawen (State Key; Laboratory for Mechanical Behaviour of Materials; Hi'an Jiaotong University;Xi'an 710049)(Manuscript received 1994-08-23; in revised form 1995-01-26). ON THE COMPOSITE AND INTRINSIC HARDNESS OF Ti(C, N) FILMS[J]. 金属学报, 1995, 31(21): 429-434.
[8] DU Hegui;DU Gang Northeast University of Technology; Shenyang. ON THE FORMATION OF Ti(C, N) IN BLAST FURNACE[J]. 金属学报, 1991, 27(3): 89-94.
No Suggested Reading articles found!