DEFORMATION AND DAMAGE AT GRAIN BOUNDARY ON FATIGUED ALUMINUM BICRYSTALS
WANG Mingzhang;LIN Shi;XIAO Jimei(University of Science and Technology Beijing;Beijing 100083)(Departiment of Material Physics;University of Science and Technology Beijing;Beijing 100083)(Manuscript received 1996-01-18;in revised form 1996-06-20)
Cite this article: 

WANG Mingzhang;LIN Shi;XIAO Jimei(University of Science and Technology Beijing;Beijing 100083)(Departiment of Material Physics;University of Science and Technology Beijing;Beijing 100083)(Manuscript received 1996-01-18;in revised form 1996-06-20). DEFORMATION AND DAMAGE AT GRAIN BOUNDARY ON FATIGUED ALUMINUM BICRYSTALS. Acta Metall Sin, 1996, 32(10): 1049-1055.

Download:  PDF(612KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Fatigue tests were performed on specimens P(horizontal grain boundary) and V(vertical grain boundary) which were cut from the same aluminum bicrystal but their orientations are vertical to each other.It is shown that there are remarkable differences in the deformation behaviour and failure mechanisms between specimens P and V.In specimen P,more than two secondary slip systems are activated and primary slip band is repressed in the grain boundary effect zone,it is found that microcracks initiate along grain boundary where deformation is more severe than that in slip band and not uniform. In specimen V,however,the deformation at grain boundary is very small,it can be seen that damage occur only in primary slip bands which reach grain boundary.By considering the same grain boundary structures in specimens P and V,it seems that the effects of grain boundary structure(e.g.∑ value) on the deformation of grain boundary itself are less important.In addition,contrast experiments were done,and it is found that the fatigue cracks growing along the oblique grain boundary and the grain boundary with greater orientation difference between neighboring grains can be obviously accelerated.
Key words:  grain boundary      fatigue damage      crack initiation      bicrystal.     
Received:  18 October 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I10/1049

1LimLC,RajR.ActaMetall,1984;32:11832夏月波,王中光.金属学报.1992;28.A513NeumannP,TonnessenA.StrengthofMetalsandAlloys(ICSMA8).Oxford:PergamonPress,1989:7434KimWH,LairdC.ActaMetall,1978;26:7775MimaG,InokoF,AtagiK.JJpnInstMel,1979,43:536MimaG,InokoF,AtagiK.TransJIM,1980;21:897王明章,林实,钱仁根,肖纪美.金属学报、1995;31:B778WeiC,LinS,QianRG,HsiaoJM.ActaMetallMater.1991;39:2051
[1] XU Yongsheng, ZHANG Weigang, XU Lingchao, DAN Wenjiao. Simulation of Deformation Coordination and Hardening Behavior in Ferrite-Ferrite Grain Boundary[J]. 金属学报, 2023, 59(8): 1042-1050.
[2] ZHANG Haifeng, YAN Haile, FANG Feng, JIA Nan. Molecular Dynamic Simulations of Deformation Mechanisms for FeMnCoCrNi High-Entropy Alloy Bicrystal Micropillars[J]. 金属学报, 2023, 59(8): 1051-1064.
[3] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
[4] WANG Zongpu, WANG Weiguo, Rohrer Gregory S, CHEN Song, HONG Lihua, LIN Yan, FENG Xiaozheng, REN Shuai, ZHOU Bangxin. {111}/{111} Near Singular Boundaries in an Al-Zn-Mg-Cu Alloy Recrystallized After Rolling at Different Temperatures[J]. 金属学报, 2023, 59(7): 947-960.
[5] LI Fulin, FU Rui, BAI Yunrui, MENG Lingchao, TAN Haibing, ZHONG Yan, TIAN Wei, DU Jinhui, TIAN Zhiling. Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy[J]. 金属学报, 2023, 59(7): 855-870.
[6] LI Xin, JIANG He, YAO Zhihao, DONG Jianxin. Theoretical Calculation and Analysis of the Effect of Oxygen Atom on the Grain Boundary of Superalloy Matrices Ni, Co and NiCr[J]. 金属学报, 2023, 59(2): 309-318.
[7] CHANG Litao. Corrosion and Stress Corrosion Crack Initiation in the Machined Surfaces of Austenitic Stainless Steels in Pressurized Water Reactor Primary Water: Research Progress and Perspective[J]. 金属学报, 2023, 59(2): 191-204.
[8] YANG Du, BAI Qin, HU Yue, ZHANG Yong, LI Zhijun, JIANG Li, XIA Shuang, ZHOU Bangxin. Fractal Analysis of the Effect of Grain Boundary Character on Te-Induced Brittle Cracking in GH3535 Alloy[J]. 金属学报, 2023, 59(2): 248-256.
[9] LIU Lujun, LIU Zheng, LIU Renhui, LIU Yong. Grain Boundary Structure and Coercivity Enhancement of Nd90Al10 Alloy Modified NdFeB Permanent Magnets by GBD Process[J]. 金属学报, 2023, 59(11): 1457-1465.
[10] WANG Jiangwei, CHEN Yingbin, ZHU Qi, HONG Zhe, ZHANG Ze. Grain Boundary Dominated Plasticity in Metallic Materials[J]. 金属学报, 2022, 58(6): 726-745.
[11] LI Haiyong, LI Saiyi. Effect of Temperature on Migration Behavior of <111> Symmetric Tilt Grain Boundaries in Pure Aluminum Based on Molecular Dynamics Simulations[J]. 金属学报, 2022, 58(2): 250-256.
[12] LIU Zhongwu, HE Jiayi. Several Issues on the Development of Grain Boundary Diffusion Process for Nd-Fe-B Permanent Magnets[J]. 金属学报, 2021, 57(9): 1155-1170.
[13] HU Biao, ZHANG Huaqing, ZHANG Jin, YANG Mingjun, DU Yong, ZHAO Dongdong. Progress in Interfacial Thermodynamics and Grain Boundary Complexion Diagram[J]. 金属学报, 2021, 57(9): 1199-1214.
[14] NI Ke, YANG Yinhui, CAO Jianchun, WANG Liuhang, LIU Zehui, QIAN Hao. Softening Behavior of 18.7Cr-1.0Ni-5.8Mn-0.2N Low Nickel-Type Duplex Stainless Steel During Hot Compression Deformation Under Large Strain[J]. 金属学报, 2021, 57(2): 224-236.
[15] SUN Jia, LI Xuexiong, ZHANG Jinhu, WANG Gang, YANG Mei, WANG Hao, XU Dongsheng. Phase Field Modeling of Formation Mechanism of Grain Boundary Allotriomorph in β→α Phase Transformation in Ti-6Al-4V Alloy[J]. 金属学报, 2020, 56(8): 1113-1122.
No Suggested Reading articles found!