| STUDY OF CLEAVAGE FRACTURE SURFACE OF TiAl ALLOYS IN NANOMETER SCALE |
| ZHANG Yue; CHU Wuyang; WANG Yanbin; QIAO Lijie; XIAO Jimei(Universityof Science and Technology Beijing; Beijing 100083); WANG Zhonghuai; BAI Chunli)(Institute of Chemistry; Chinese Academy of Sciences; Beijing 100080) |
|
Cite this article:
ZHANG Yue; CHU Wuyang; WANG Yanbin; QIAO Lijie; XIAO Jimei(Universityof Science and Technology Beijing; Beijing 100083); WANG Zhonghuai; BAI Chunli)(Institute of Chemistry; Chinese Academy of Sciences; Beijing 100080). STUDY OF CLEAVAGE FRACTURE SURFACE OF TiAl ALLOYS IN NANOMETER SCALE. Acta Metall Sin, 1995, 31(5): 191-196.
|
|
|
Abstract The cleavage fracture surfaces of Ti_3Al and Ti-24Al-11Nb samples after tensile tests in air were studied with a scanning tunnel microscope(STM). Many details in nanometer scale were revealed on the fracture surfaces by STM, such as nanometer scale steps, dimples and vacancies. The study of the details on the fracture surfaces will be helpful to the study of the mechanism of fracture.
|
|
Received: 18 May 1995
|
| 1Masuda-JindoK,TewaryVK,ThomsonR.MaterSciEng,1991;A146:2732张跃,王燕斌,褚武扬,肖纪美.科学通报,1994;39:1173ZhangY,WangYB,ChuWY,HsiaoJM.JVacSciTechnol,1994;12B(4)4BinningG,RohreH,GerberC.SurfSci,1983;137:L3795HallmarkVM,ChiangS,RaboltJF.,SwalenJD,WilsonRJ.PhysRevLett,1987;59:28796 SamsavarA,HirschornE S,MillerT.PhysRevLett,1990;65:16077Gomez-RodriguezJM,AsenjoA,SalvarezzaRC,BaroAM.Ultramicroscopy,1992;42:13218SastrySML,LipsittHA.In:KimuroH,Izumi,Oeds.,Titanium'80,Vol.II,Proc4thIntConfonTitaninum,Warrendale,PA:TMS-AIME,1980:12319LipsittHA,ShechtmanD,SchafrikRE.MelallTrans,1980:11A:136910WangXS,GoldbergJL,BarteltNC.Phys Rev Lett,1990;65:243011KaiserWJ,JaklcvicRC.SurfSci,1987;182:L22712OcalC,VazquezdePargaAL,JMicroscopy,1988;152:69713ThibaudauF,CoustyJ.Ultramicroscopy,1992;42:51114BesenbacherF,JensenF.JVacSciTechnol,1991:9B:87415NiehusH,KohlerUK.JMicroscopy,1988;152:73516SalmeronM,OgeltreeDF,OcalC.JVacSciTechnol,1991;98:134717WhitmanLJ,StroscioJA,DragosetRA,CelottaRJ.Science,1991;251:120618ChenCJ.PhysRevLett,1990;65:448 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|