Please wait a minute...
Acta Metall Sin  1995, Vol. 31 Issue (4): 165-169    DOI:
Current Issue | Archive | Adv Search |
IN SITU RECRYSTALLIZATION DURING ELEVATED TEMPERATURE DEFORMATION IN Fe_3Al BASED ALLOY
CHEN Mingwei; SHAN Aidang; LIN Dongliang(Shanghai Jaiotong University Shanghai 200030); LIANG Wei(Taiyuan University of Technology; Taiyuan 030024)
Cite this article: 

CHEN Mingwei; SHAN Aidang; LIN Dongliang(Shanghai Jaiotong University Shanghai 200030); LIANG Wei(Taiyuan University of Technology; Taiyuan 030024). IN SITU RECRYSTALLIZATION DURING ELEVATED TEMPERATURE DEFORMATION IN Fe_3Al BASED ALLOY. Acta Metall Sin, 1995, 31(4): 165-169.

Download:  PDF(393KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  篒n situ recrystallization (ISR) during elevated temperature deformation was found in a Fe3AI based alloy by TEM observation and metallographic examination. Good elevated temperature ductility of the Fe3Al alloy is closely related to ISR. Through olimb or cross slip, the dislocations created in deformation process change into a dislocation array, which attracts lattice dislocations and increases the misorientation between crystals at the both sides of itself during further deformation, and gradually evolves into a subboundary and even a high-angle boundary.
Key words:  intermetallics      Fe_3Al      in situ recrystallization     
Received:  18 April 1995     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I4/165

1MckameyCG,MaziaszPJ,GoodwinGM,ZachariaTMaterSciEng,1994;A174:592ShanAidang,ChenMingwei,LinTLInt.(ConfonSuperlasticityinAdvanceMaterials(ICSAM'94)Moscow.19943HanadaS.SatoT.WatanabeS.IzumiOJJpnInstMet.198112:12854单爱党,林栋梁,陈明伟,郦定强.金属学报.1995:31B355LloydDJ,MooreDM.SuperplasticFormingofstructureAlloyMetallSoc,Warrendal,1982:1476WadsworthJ.SuperplasticForming.MetalPrark.Ohio:ASM1985:437GudmundssonH,BrooksD,WertJActaMetall1991:1:198BricknellRH,EdingtonJW.ActaMetall.197927:13039BricknellRH,EdingtonJW.MetallTrans.1979:10A:125710NesE.MetSci1979:13:21111McNelleyTLeeEW,MillsME.MetallTrans,1986:17A:103512LeeEW,McNelleyTR,StengelAF.MetallTrans、1986:17A:104313HalesSJ.McNelleyTRActaMetall,1988:36:122914LinTL,ChenMingwei.ShanAidang.IntConfonSuperlasticityinAdvanceMaterials(ICSAM'94),Moscow,1994:515Friede1J,王煜译.位错.北京:科学出版社,1984:192D
[1] GONG Shengkai, SHANG Yong, ZHANG Ji, GUO Xiping, LIN Junpin, ZHAO Xihong. Application and Research of Typical Intermetallics-Based High Temperature Structural Materials in China[J]. 金属学报, 2019, 55(9): 1067-1076.
[2] Lin GENG, Hao WU, Xiping CUI, Guohua FAN. Recent Progress on the Fabrication of TiAl-Based Composites Sheet by Reaction Annealingof Elemental Foils[J]. 金属学报, 2018, 54(11): 1625-1636.
[3] Xuan YU, Zhihao ZHANG, Jianxin XIE. Microstructure, Ordered Structure and Warm TensileDuctility of Fe-6.5%Si Alloy with Various Ce Content[J]. 金属学报, 2017, 53(8): 927-936.
[4] Li ZHOU,Chao CUI,Qing JIA,Yingshi MA. Experimental and Finite Element Simulation of Milling Process for γ-TiAl Intermetallics[J]. 金属学报, 2017, 53(4): 505-512.
[5] Jihou LIU,Hongyun ZHAO,Zhuolin LI,Xiaoguo SONG,Hongjie DONG,Yixuan ZHAO,Jicai FENG. Microstructures and Mechanical Properties of Cu/Sn/Cu Structure Ultrasonic-TLP Joint[J]. 金属学报, 2017, 53(2): 227-232.
[6] Guotian WANG, Hongsheng DING, Ruirun CHEN, Jingjie GUO, Hengzhi FU. Effect of Current Intensity on Microstructure of Ni3Al Intermetallics Prepared by Directional Solidification Electromagnetic Cold Crucible Technique[J]. 金属学报, 2017, 53(11): 1461-1468.
[7] Tong LIU,Liangshun LUO,Yanning ZHANG,Yanqing SU,Jingjie GUO,Hengzhi FU. MICROSTRUCTURE EVOLUTION AND GROWTH BEHAVIORS OF FACETED PHASE IN DIRECTIONALLYSOLIDIFIED Al-Y ALLOYS II. Microstructure Evolution of Directionally Solidified Al-53%Y Peritectic Alloy[J]. 金属学报, 2016, 52(7): 866-874.
[8] Rui YANG,Yan PAN,Wei CHEN,Qiaoyan SUN,Lin XIAO,Jun SUN. DEFORMATION BEHAVIOR AND THE MECHANISM OF MICRO-SCALE Ti-10V-2Fe-3Al PILLARSIN COMPRESSION[J]. 金属学报, 2016, 52(2): 135-142.
[9] PENG Yingbo, CHEN Feng, WANG Minzhi, SU Xiang, CHEN Guang. RELATIONSHIP BETWEEN MECHANICAL PROPERTIES AND LAMELLAR ORIENTATION OF PST CRYSTALS IN Ti-45Al-8Nb ALLOY[J]. 金属学报, 2013, 49(11): 1457-1461.
[10] LIANG Yongchun GUO Jianting; SHENG Liyuan; ZHOU Lanzhang. EFFECTS OF RARE EARTH ELEMENT Gd ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF NiAl-Cr(Mo)-Hf EUTECTIC ALLOY[J]. 金属学报, 2010, 46(5): 528-532.
[11] ZHOU Minbo LI Xunping MA Xiao ZHANG Xinping. EARLY INTERFACIAL REACTION AND UNDERCOOLING SOLIDIFICATION BEHAVIOR  OF Sn-3.5Ag/Cu SYSTEM[J]. 金属学报, 2010, 46(5): 569-574.
[12] ZHOU Dianwu XU Shaohua ZHANG Fuquan PENG Ping LIU Jinshui. FIRST-PRINCIPLES CALCULATIONS OF STRUCTURAL STABILITIES AND ELASTIC PROPERTIES OF AB2 TYPE INTERMETALLICS IN ZA62 MAGNESIUM ALLOY[J]. 金属学报, 2010, 46(1): 97-103.
[13] HE Hongwen XU Guangchen GUO Fu. FORMATION OF WHISKER AND HILLOCK IN Cu/Sn--58Bi/Cu SOLDERED JOINT DURING ELECTROMIGRATION[J]. 金属学报, 2009, 45(6): 744-748.
[14] HU Jing LIN Dongliang WANG Yan. EBSD ANALYSES OF THE MICROSTRUCTURAL EVOLUTION AND CSL CHARACTERISTIC GRAIN BOUNDARY OF COARSE--GRAINED NiAl ALLOY DURING PLASTIC DEFORMATION[J]. 金属学报, 2009, 45(6): 652-656.
[15] ;. MICROSTRUCTURE AND MECHANICAL PROPERTIES OF A CAST NiAl-Cr(Mo)-Ti EUTECTIC ALLOY[J]. 金属学报, 2006, 42(10): 1031-1035 .
No Suggested Reading articles found!