| MATHEMATICAL AND PHYSICAL MODELING OF FLOW AND MIXING IN LADLES STIRRED BY ARGON THROUGH MULTI-TUYERE |
| ZHU Miaoyong; (Department of Ferrous Metallurgy; Northeastern University;Shenyang 110006) INOMOTO Takeo; XIAO Zeqiang(Northeastern University; Shenyang 110006)(Nippon Steel Corporation; Futtsu; Japan) |
|
Cite this article:
ZHU Miaoyong; (Department of Ferrous Metallurgy; Northeastern University;Shenyang 110006) INOMOTO Takeo; XIAO Zeqiang(Northeastern University; Shenyang 110006)(Nippon Steel Corporation; Futtsu; Japan). MATHEMATICAL AND PHYSICAL MODELING OF FLOW AND MIXING IN LADLES STIRRED BY ARGON THROUGH MULTI-TUYERE. Acta Metall Sin, 1995, 31(22): 435-439.
|
|
|
Abstract Mathematical modeling and physical modeling have been conducted to investigate the characteristics of fluid flow and mixing in argon-stirred ladles with six different types of tuyere arrangement. An optimum arrangement of tuyeres considering the various purposes of refining and an empirical correlation for mixing time concerning the number of tuyeres are proposed. The results of mathematical modeling are in good agreement with those of physical modeling.
|
|
|
| 1JooS,GuthrieRIL,KamalG.SteelmakingProc,1989;72:5172HsiaoTC,LehnerT,KjellbergB.ScandJMetall,1980;9:1053JonesWP,LaunderBE,IntJHeatMassTransfer,1972;15:3014PatankarSV.NumericalHeatTransferandFluidFlow,HemisperePubCo,19805朱苗勇,泽田郁夫,肖泽强.金属学报,1995;31:B3466NakanishiK,SaitoK,NozakiT.SteelmakingProc,1982;65:1016 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|