EFFECTS OF GRAPHITE MORPHOLOGY AND MATRICES ON FRACTURE BEHAVIOUR OF CAST IRONS
JIANG Jianqing(Southeast University;Nanjing)
Cite this article: 

JIANG Jianqing(Southeast University;Nanjing). EFFECTS OF GRAPHITE MORPHOLOGY AND MATRICES ON FRACTURE BEHAVIOUR OF CAST IRONS. Acta Metall Sin, 1994, 30(8): 374-379.

Download:  PDF(420KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The fracture behaviour of cast irons with graphite irregularity S=0 and spheroidal graphite iron under three different stress modes was investigated.When the crack was parallel or vertical to the graphite flakes,it would be developed along inside the graphite flakes,i, e the cleavage of(0001) plane of graphite flakes,or propagated along the matrix/graphite interface,i, e decohension between graphite flake and matrix respectively.In the case of spheroidal graphite cast iron with ferrite-bainite matrix,the crack would propagate mainly in ferrite and secondary graphite.
Key words:  Fe-C alloy      flake graphite      spheroidal graphite      crack propagation      cast iron     
Received:  18 August 1994     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I8/374

1蒋建清.金属学报,1993;29:A4172蒋建清浙江大学硕士学位论文,19863蒋建清,舒光冀.钢铁研究学报,1993;5(2):534ChouJaw-Min,HonMin-Hsiung,LeeJye-logJMaterSci,1990;25:19655JiangJianqingJMaterSciLett,1993.12:1861
[1] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[2] ZHOU Hongwei, BAI Fengmei, YANG Lei, CHEN Yan, FANG Junfei, ZHANG Liqiang, YI Hailong, HE Yizhu. Low-Cycle Fatigue Behavior of 1100 MPa Grade High-Strength Steel[J]. 金属学报, 2020, 56(7): 937-948.
[3] ZHANG Xiaochen, MENG Weiying, ZOU Defang, ZHOU Peng, SHI Huaitao. Effect of Pre-Cyclic Stress on Fatigue Crack Propagation Behavior of Key Structural Al Alloy Materials Used in High Speed Trains[J]. 金属学报, 2019, 55(10): 1243-1250.
[4] Jin WANG, Liming YU, Yuan HUANG, Huijun LI, Yongchang LIU. Effect of Crystal Orientation and He Density on Crack Propagation Behavior of bcc-Fe[J]. 金属学报, 2018, 54(1): 47-54.
[5] Shu GUO,En-Hou HAN,Haitao WANG,Zhiming ZHANG,Jianqiu WANG. Life Prediction for Stress Corrosion Behavior of 316L Stainless Steel Elbow of Nuclear Power Plant[J]. 金属学报, 2017, 53(4): 455-464.
[6] Zhiyong LIU,Zongshu LI,Xiaolin ZHAN,Wenzhu HUANGFU,Cuiwei DU,Xiaogang LI. GROWTH BEHAVIOR AND MECHANISM OF STRESS CORROSION CRACKS OF X80 PIPELINE STEEL IN SIMULATED YINGTAN SOIL SOLUTION[J]. 金属学报, 2016, 52(8): 965-972.
[7] ZHANG Lei, ZHAO Honglei, ZHU Mingfang. SIMULATION OF SOLIDIFICATION MICROSTRUC-TURE OF SPHEROIDAL GRAPHITE CAST IRON USING A CELLULAR AUTOMATON METHOD[J]. 金属学报, 2015, 51(2): 148-158.
[8] YU Long, SONG Xiping, ZHANG Min, LI Hongliang, JIAO Zehui, YU Huichen. CRACK INITIATION AND PROPAGATION OF HIGH Nb-CONTAINING TiAl ALLOY IN FATIGUE-CREEP INTERACTION[J]. 金属学报, 2014, 50(10): 1253-1259.
[9] JIANG Bing XING Xianran GUO Zhimeng. CRACK PROPAGATION AND DOMAIN SWITCHING IN BaTiO3 SINGLE CRYSTALS UNDER EXTERNAL FIELD[J]. 金属学报, 2011, 47(5): 605-610.
[10] GAO Ao WANG Qiang LI Dejun CHAI Haishan ZHAO Lijia HE Jicheng. STATE OF Fe-C ALLOY IN THE ELECTROMAGNETIC STEEL-TEEMING SYSTEM[J]. 金属学报, 2011, 47(2): 219-223.
[11] ZHOU Yanlei XU Yang CHEN Jun LIU Zhenyu. EXPERIMENTAL STUDY OF THE IMPACT FRACTURE BEHAVIOR OF FH550 OFFSHORE PLATFORM STEEL[J]. 金属学报, 2011, 47(11): 1382-1387.
[12] WANG Li-Min SUN Ming-Yuan. Electronical measurement of incision iron specimens’ fracture proceeding and calculation of the structure bearing capacity[J]. 金属学报, 2008, 44(7): 853-858 .
[13] Xiang Zhao; Shoujing WANG; GONG Ming-Long; liang zuo. Influence of austenization temperature on the morphology of pearlite in Fe-0.12%C alloy under high magnetic field[J]. 金属学报, 2008, 44(11): 1305-1309 .
[14] YANG Jie; DONG Huaiyu; XIONG Shoumei. PREDICTION OF SHRINKAGE CAVITY AND POROSITY IN GRAY CAST IRON DURING SOLIDIFICATION[J]. 金属学报, 2005, 41(9): 929-932 .
[15] YU Huichen; SUN Yanguo; XIE Shishu; K. TANAKA. Low Cycle Fatigue Crack Propagation in Stainless Steel Under Combined Torsion and Tension[J]. 金属学报, 2005, 41(1): 73-.
No Suggested Reading articles found!