| EFFECT OF FINE PRECIPITATES ON PROPAGATION OF MICRO-CRACKS IN LOW CARBON LOW VANADIUM STEEL |
| CHEN Mengzhe;KE Jun University of Science and Technology BeijingWANG Siqing;engineer;Changsha Institute of Mining and Metallrugy;Ministry of Metallurgical Industry.Changsha 410012 |
|
Cite this article:
CHEN Mengzhe;KE Jun University of Science and Technology BeijingWANG Siqing;engineer;Changsha Institute of Mining and Metallrugy;Ministry of Metallurgical Industry.Changsha 410012. EFFECT OF FINE PRECIPITATES ON PROPAGATION OF MICRO-CRACKS IN LOW CARBON LOW VANADIUM STEEL. Acta Metall Sin, 1993, 29(5): 23-27.
|
|
|
Abstract The fine second phase particles, average size about 86 nm, precipitating inferrite matrix of low carbon low vanadium steel will hinder the movement of dislocations infront of crack-tip, retard the thinning process in local area, and then proceed to impede theinitiation and propagation of micro-cracks. The propagating path of micro-cracks is control-led partly by the distribution of precipitates, a single particle has the action aforementionedweakly.
|
|
Received: 18 May 1993
|
1 Gladman T. Effect of Second-Phase Particles on the Mechanical Properties of Steel. London: The Iron and Steel Institute, 1971: 68 2 Fisher J R. Gurland J. Met Sci, 1981; 15: 185 3 Inoue T, Kinoshita S. Trans Iron Steel Inst Jpn. 1977: 17: 523 4 Ritchie R O. Thompson A W. Metall Trans, 1986; 16A: 233 5 Chan I Y. Wilsdorf H G F. Acta Metall, 1981; 29: 1221 6 Benson J P, Edmonds D V. In: Taplin DMR ed., Fracture 1977. Vol. Ⅱ, Proc 4th Int Conf on Fracture, New York: Pergamon, 1978: 65 7 张以增.戴蜀娟.邹鸿承,苗丕峰.金属学报,1987;23:A403 8 Jagannadham K, Wilsdorf H G F. Mater Sci Eng, 1986: A81: 273 9 Ohr S M. Mater Sci Eng, 1985; A72: 1= |
| No Suggested Reading articles found! |
|
|