| SCALING LAW OF IRREGULAR EUTECTIC IN DIRECTIONAL SOLIDIFICATION |
| LIU Junming;LIU Zhiguo;WU Zhuangchun Nanjing University Lecturer;National Laboratory of Solid State Microstructures;Nanjing University; Nanjing 210008 |
|
Cite this article:
LIU Junming;LIU Zhiguo;WU Zhuangchun Nanjing University Lecturer;National Laboratory of Solid State Microstructures;Nanjing University; Nanjing 210008. SCALING LAW OF IRREGULAR EUTECTIC IN DIRECTIONAL SOLIDIFICATION. Acta Metall Sin, 1993, 29(3): 11-18.
|
|
|
Abstract The profile features of solidifying interface of irregular Al-Si eutectic duringdirectional solidification were studied by solving a nonlinear coupling equation of directionalsolidification of Ai-Si eutectic. The critical splitting point of the solidifying interface coin- cides with the maximum value of its position and corresponds to the marginal stability point.Argument is presented that the interlamellar spacing for local regular structure selects the crit-ical splitting state of α(Al)-liquid interface as its operating point, and the operating point ofaverage interflake spacing for irregular structure is the critical splitting state of β(Si)-liquidinterface. The scaling laws derived, which have more general forms than the classicJackson-Hunt scaling, gained support from the experimental results.
|
|
Received: 18 March 1993
|
1 Sprenger H J, Potschke J, Potard C, Rogge V. In: Walter H U eds., Fluid Science and Materials Science in Space, Berlin: Springer-Verlag, 1987: 569 2 Elliott R. Eutectic Solidification Processing, Crystalline and Glassy Alloys, London: Butterworths, 1983 3 Muller-Krumbhaar H, Kurz W. In: Cahn R W, Hassen P, Kramer E J. eds., Materials Science and Technology: A Comprehensive Treatment, Vol .V, New York: VCH Publishers Inc., 1991: 554 4 Liu J M, Zhou Y H, Shang B L. J Mater Sci, 1992; 27: 2067 5 Jackson K A, Kunt J D. Trans AIME, 1966; 236: 1129 6 Langer J S. Phys Rev Lett, 1980; 44: 1023 7 Liu J M, Zhou Y H, Shang B L. Acta Metall, 1990; 38: 1625 8 Kurz W, Fisher D J. Fundamentals of Solidification, Aedermannsdorf: Trans Tech, 1984: 220 9 Gundez M, Hunt J D. Acta Met, 1985; 33: 1651 10 Liu J M, Zhou Y H, Shang B L. Acta Met, 1990; 38: 1651 11 Langer J S. Rev Mod Phys, 1980; 52: 1 12 Hohenberger P C, Langer J S. J Soli Stat Phys 1982; 28: 193 13 Hogen L M, Song H. Metall Trans, 1987: 18A: 707 14 Kassner K, Misbah C. Phys Rev Lett, 1991; 66: 445i |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|