Please wait a minute...
Acta Metall Sin  1993, Vol. 29 Issue (2): 83-87    DOI:
Current Issue | Archive | Adv Search |
CORRELATION BETWEEN GRAIN BOUNDARY CORROSION AND MISORIENTATION IN Nb BICRYSTALS
QIAN Xiangrong;ZHOU Yicang;ZHANG Dongbin;MA Ruzhang Shanghai Iron and Steel Research Institute; Y. T. Chou Lehigh University; U. S. A.; University of Science and Technology Beijing
Cite this article: 

QIAN Xiangrong;ZHOU Yicang;ZHANG Dongbin;MA Ruzhang Shanghai Iron and Steel Research Institute; Y. T. Chou Lehigh University; U. S. A.; University of Science and Technology Beijing. CORRELATION BETWEEN GRAIN BOUNDARY CORROSION AND MISORIENTATION IN Nb BICRYSTALS. Acta Metall Sin, 1993, 29(2): 83-87.

Download:  PDF(376KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Grain boundary corrosion of oriented Nb bicrystals with symmetric tiltboundaries has been investigated by use of interference microscope. The corrosion depth, d,increases with misorientation angle, θ, except near some coincidence-site-lattice boundarieswhere minimum cusps appear. For small-angle boundaries, d depends on θ following aRead-Shockley type relationship. The atomistic structure and the local expansion of grainboundaries were calculated using a computer simulation method. The structure dependence ofgrain boundary corrosion is explained in terms of variation in free volume.
Key words:  coincidence-site-lattice boundary      small angle boundary      grain boundary corrosion      misorientation      free volume     
Received:  18 February 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I2/83

1 Arora O P, Metzger M. Trans AIME, 1966; 236: 1205
2 Boos J Y, Goux C. Compt Rend Acad Sci Paris, 1970; 271C: 978
3 Froment M, Vignaud C. Compt Rend Acad Sci Paris, 1971; 272C: 165 Blondeau G, Froelicher M, Froment M, Goff A H-L. Compt Rend Acad Sci Paris, 1972; 275C: 25
4 Pande C S, Lin L S, Butler S R, Chou Y T. J Cryst Growth, 1973; 19: 209
5 Qian X R, Chou Y T. Philos Mag, 1982; A45: 1075
6 Qian X R, Chou Y T. J Less-Common Met, 1987; 134: 179
7 Vitek V, Sutton A P, Smith D H, Pond R C. In: Balluffi R W ed., Grain Boundary Structure and Kinetics, Metals Park, Ohio: ASM, 1980: 115
8 Aaron H B, Bolling G F. Surf Sci, 1972; 31: 27
9 Kamenetzky E A, Gronsky R, Chou Y T. Trans Jpn Inst Met, 1986; 27 (Suppl): 293
10 Vitek V, Smith D A, Pond R C. Philos Mng, 1980; A41: 649
11 Fujiwara T, Ishii Y. J Phys F: MetaI Phys, 1980; 10: 1901
12 Girifalco L A, Weizer V G. Phys Rev, 1959; 114: 687\
[1] LI Xiucheng,SUN Mingyu,ZHAO Jingxiao,WANG Xuelin,SHANG Chengjia. Quantitative Crystallographic Characterization of Boundaries in Ferrite-Bainite/Martensite Dual-Phase Steels[J]. 金属学报, 2020, 56(4): 653-660.
[2] Jianguo WANG,Dong LIU,Yanhui YANG. MECHANISMS OF NON-UNIFORM MICROSTRUC-TURE EVOLUTION IN GH4169 ALLOYDURING HEATING PROCESS[J]. 金属学报, 2016, 52(6): 707-716.
[3] LI Xiaoyang, LI Peng, ZHOU Yizhou, JIN Tao, ZHANG Zhefeng. EFFECT OF MISORIENTATION ON THE TENSILE PROPERTIES OF SRR99 SUPERALLOY BICRYSTALS[J]. 金属学报, 2013, 49(3): 351-357.
[4] CHENG Junye, ZHAO Aimin, CHEN Yinli, DONG Rui, HUANG Yao. EBSD STUDIES OF 30MnB5 HOT STAMPING STEEL TEMPERED AT DIFFERENT TEMPERATURE[J]. 金属学报, 2013, 49(2): 137-145.
[5] HU Qiang ZENG Xierong QIAN Haixia XIE Shenghui SHENG Hongchao. CORRELATION BETWEEN THE GLASS-FORMING ABILITY AND CHARACTERISTIC FREE VOLUMES OF THE IRON BASE BULK METALLIC GLASSES[J]. 金属学报, 2012, 48(11): 1329-1334.
[6] YANG Ping LU Fayun MENG Li CUI Feng’e. CRYSTALLOGRAPHIC BEHAVIORS OF COMPRESSED HIGH MANGANESE TRIP/TWIP STEELS ANALYZED BY EBSD TECHNIQUES
II. MartensiticMisorientations, the Evolution of Martensitic Orientations and the Influence of Austenitic Orientations
[J]. 金属学报, 2010, 46(6): 666-673.
[7] FANG Xiaoying WANG Weiguo Rohrer G S ZHOU Bangxin. GRAIN BOUNDARY PLANE DISTRIBUTIONS IN THE COLD–ROLLED AND ANNEALED FERRITIC STAINLESS STEEL[J]. 金属学报, 2010, 46(4): 404-410.
[8] LI Jianmin;SUN Wensheng;QUAN Mingxiu; HU Zhuangqi(State Key Laboratory for RSA;Institute of Metal Research; Chinese Academy of Sciences;Shenyang 110015);WANG Yongzhong;QIAO Guiwen(Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015) (Manuscript received 1994-05-04;in revised form 1995-03-28). DUCTILE-BRITTLE TRANSITION OF(Fe_0.99)Mo_(0.01))_(78)Si_9B_(13) AMORPHOUS ALLOY[J]. 金属学报, 1995, 31(23): 493-498.
[9] ZHANG Junshan Associate Professor;Department of Materiats Seience and Engineering;Dattan Institute of Technology;CAO Zhiben Dalian Institute of Technology. RELATIONSHIP BETWEEN CREEP BEHAVIOR AND DISLOCATION SUBSTRUCTURE IN Ni-20Cr ALLOYS[J]. 金属学报, 1988, 24(2): 111-118.
No Suggested Reading articles found!