| FIXATION OF HYDROGEN BY RARE EARTH IN Al-Si ALLOY |
| ZHAO Yuguang;LI Daoyun;WANG Shoushi;HE Zhenming Jilin University of Technology; Changchun |
|
Cite this article:
ZHAO Yuguang;LI Daoyun;WANG Shoushi;HE Zhenming Jilin University of Technology; Changchun. FIXATION OF HYDROGEN BY RARE EARTH IN Al-Si ALLOY. Acta Metall Sin, 1993, 29(1): 16-20.
|
|
|
Abstract Occurrence of RE hydride was identified in the Al-Si alloy containing RE andenrichment of hydrogen in polynary RE intermetallic compound was determined by means ofEPMA, secondary ion mass spectrography, Hg-free vacuum drivepipe hydrogen-meter to-gether with metallography and porosity measurement. The relative contents of various formsof hydrogen before and after RE added in Al-Si alloy have been qualitatively analysed. Aconcept about firm fixation of hydrogen by RE was suggested. It is believed that the hydrogenfixation is the major cause of reducing free hydrogen content and decreasing hydrogen-in-duced defects.
|
|
Received: 18 January 1993
|
1 李道韫,何镇明,赵宇光,主守实,刘振东.中国稀土学报,1987;5(4) :39 2 何镇明,李道韫,赵宇光.中国稀土学报,1988;6(1) :47 3 Вассерми АМ著,张中豪,金钦漧译,金属中气体的测定.上海:上海科学技术出版社,1981( |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|