Please wait a minute...
Acta Metall Sin  1992, Vol. 28 Issue (8): 77-83    DOI:
Current Issue | Archive | Adv Search |
CRYSTAL STRUCTURE OF γ-Li_xFe_2O_3 WITH ELECTROCHEMICAL INSERTION OF Li
HUANG Jianshun; CHEN Junming (Shanghai Institute of Metallurgy; Academia Sinica)
Cite this article: 

HUANG Jianshun; CHEN Junming (Shanghai Institute of Metallurgy; Academia Sinica). CRYSTAL STRUCTURE OF γ-Li_xFe_2O_3 WITH ELECTROCHEMICAL INSERTION OF Li. Acta Metall Sin, 1992, 28(8): 77-83.

Download:  PDF(579KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Crystal structure of γ-Li_xFe_2O_3, inserted Li electrochemically, was studied by Mossbauer spectroscopy together with X-ray diffraction, XPS and electrochemical method. On the insertion of Li with low current density, the crystal structure is keeping original spinel; while with higher current desity or by thermal activation, owing to violent movement of Li~+ ions, part of crystal structure transforms into rock type similar to face—centered cubic structure of ferrous oxide. The transition channel during insertion of Li and limitation of Li~+ ions to be inserted were discussed.
Key words:  crystal structure      γ-Li_xFe_2O_3       Li cell      Mossbauer spectroscopy     
Received:  18 August 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I8/77

1 ThaEkceray M M, David W IF, Goodenough J B. Mater Res Bull, 1982; 17:785
2 Morzilli S, Scrosati B, Sgarlata F. Electrochim Acta, 1985; 30: 1271
3 Abraham K M, Pasquariello D M, Willstaedt E B. J Electrochem Soc, 1990; 137:743
4 黄建顺.中国科学院上海冶金研究所硕士学位论文,1988
5 陈俊明,王才虎,王戈.金属学报,1985;22:B66
6 黄建顾,陈俊明,王戈.应用科学学报,1988;6(4) :140
7 Armstrong R J, Morrish A H, Sawatzky G A. Phys Lett, 1966; 23: 414.
8 Pattek-JanczykA, Sepidol B, Grenier J C, FournesL. Mater Res Bull, 1986; 21:1083
9 陈俊明,黄建顺.化学学报,待发表C
[1] Ying LI,Chao SUN,Jun GONG. Performance Research of Magnesium Base Lanthanum Hexaaluminate Prepared by Co-Precipitation[J]. 金属学报, 2019, 55(5): 657-663.
[2] YAO Meiyi, LIN Yuchen, HOU Keke, LIANG Xue, HU Pengfei, ZHANG Jinlong, ZHOU Bangxin. Effect of Sn on Initial Corrosion Behavior of Zirconium Alloy in 280 ℃ LiOH Aqueous Solution[J]. 金属学报, 2019, 55(12): 1551-1560.
[3] Zhen WANG,Bangxin ZHOU,Boyang WANG,Jiao HUANG,Meiyi YAO,Jinlong ZHANG. SECOND PHASE PARTICLES AND THEIR CORROSION BEHAVIOR OF Zr-0.72Sn-0.32Fe-0.15Cr-0.97Nb ALLOY[J]. 金属学报, 2016, 52(1): 78-84.
[4] ZHANG Haixia, LI Zhongkui, ZHOU Lian, XU Bingshe, WANG Yongzhen. EFFECTS OF STRUCTURE AND INTERNAL STRESSES IN OXIDE FILMS ON CORROSION MECHANISM OF NEW ZIRCONIUM ALLOY[J]. 金属学报, 2014, 50(12): 1529-1537.
[5] LI Qiang LIANG Xue PENG Jianchao LIU Renduo YU Kang ZHOU Bangxin. OXIDATION BEHAVIOR OF THE β-Nb PHASE PRECIPITATED IN Zr-2.5Nb ALLOY[J]. 金属学报, 2011, 47(7): 893-898.
[6] PAN Hongge; DU Honglin; CHEN Changpin; HAN Xiufeng; YANG Fuming (Department of Materials Science and Engineering; Zhejiang University; Hangzhou 310027)(State Key Laboratory for Magnetism; Institute of Physics; The Chinese Academy of Sciences; Beijing 100080)(Institute of Chinese Atomic Energy; Beijing 102413). STRUCTURAL CHARACTERIZATION OF THE Y_3(Fe, Mo)_(29) INTERMETALLIC COMPOUND[J]. 金属学报, 1998, 34(5): 473-482.
[7] WANG Rongming; LI Chunzhi; PING Dehai; YAN Minggao (Beijing Institute of Aeronautical Materials; Beijing 100095)(Laboratory of Atomic Imaging of Solids; Institute of Metal Research; The Chinese Academy of Sciences;Shenyang 110015)(Beijing Laboratory of Electron Microscopy; The Chinese Academy of Sciences; Beijing 100080). STUDY ON THE PLATELET PHASE IN AN YTTRIUM-CONTAINING LOW EXPANSION SUPERALLOY[J]. 金属学报, 1998, 34(4): 367-372.
[8] XIONG Weihao;HU Zhenhua;CUI Kun (State Key Laboratory of Dies Technology;Huazhong University of Science and Technology; Wuhan 430074). FORMATION MECHANISM OF MICROCRYSTAL INTERFACE LAYER IN Ti(C, N)-BASED CERMET[J]. 金属学报, 1997, 33(5): 473-478.
[9] XING Xiusan (Beijing Institute of Technology;Beijing 100081)(Manuscript received 1996-01-08;in revised form 1996-06-21). DIAGRAM OF MICRO-MESO-MACRO MULTILEVEL CONNECTED THEORY OF FRACTURE[J]. 金属学报, 1996, 32(12): 1265-1269.
[10] YANG Xiaoguang; LEI Yongquan; ZHANG Wenkui; ZHU Guangming; WANG Qidong(Zhejiang University; Hangzhou 310027). RELATIONSHIP BETWEEN CRYSTAL CHARACTERISTICS AND ELECTROCHEMICAL PROPERTIES OF Zr BASED HYDROGEN STORAGE ALLOY[J]. 金属学报, 1996, 32(11): 1194-1198.
[11] MAO Jian.fu;HE Liantong;YE Hengqiang(Laboratory of Atomic Imaging of Solids;Ihstitute of Metal Research;Chinese Academy of Sciences;Shenyang 110015) YANG Dezhuang;TANG Zhixiu(Harbin Institute of Technotogy;Harbin 150001)(Manuscript received 1994-07-05;in revised form 1995-02-24). HRTEM STUDY ON CRYSTAL STRUCTURE OF Zr_4Co_4Si_7 COMPOUND[J]. 金属学报, 1995, 31(7): 289-293.
[12] LIU Xuedong;ZHU Jie;JIANG Jian;DING Bingzhe;WANG Jingtang Institute of Metal Research. Academia Sinica; Shenyang. STRUCTURE OF NANOCRYSTALLINE Fe-Cu-Si-B ALLOYS[J]. 金属学报, 1993, 29(9): 72-76.
[13] ZHENG Yasgzeng;ZHANG Fucheng Yanshan University; Qinhuangdao. EFFECT OF HETEROGENEOUS DISTRIBUTION OF C AND ALLOYING ELEMENTS ON γ/α′ TRANSFORMATION IN A Fe-Mn-Cr-C ALLOY[J]. 金属学报, 1991, 27(3): 82-85.
[14] XU Zuxiong;MA Ruzhang;HAN Yongzhu University of Science and Technology Beijing Beijing Institute of Metallurgy. MSSBAUER STUDY ON MAGNETIC ANISOTROPY OF AMORPHOUS ALLOY Fe_(71)Ni_(10)B_(13)Si_4C_2[J]. 金属学报, 1989, 25(3): 143-145.
[15] XU Zuxiong;MA Ruzhang;ZHU Yongquan;ZHAO Zhongtao;FENG Yongrong Beijing University of Iron and Steel Technology. MSSBAUER INVESTIGATION ON QUENCHED STRUCTURES OF 40CrNiMo STEEL[J]. 金属学报, 1988, 24(5): 436-440.
No Suggested Reading articles found!