| STRESS CORROSION PERFORMANCE OF Al-Li-Cu-Mg ALLOY |
| WANG Zhengfu;ZHU Ziyong;KE Wei;ZHANG Yun;HU Zhuangqi Corrosion Science Laboratory; Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang; Institue of Metal Research; Academia Sinica; Shenyang |
|
Cite this article:
WANG Zhengfu;ZHU Ziyong;KE Wei;ZHANG Yun;HU Zhuangqi Corrosion Science Laboratory; Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang; Institue of Metal Research; Academia Sinica; Shenyang. STRESS CORROSION PERFORMANCE OF Al-Li-Cu-Mg ALLOY. Acta Metall Sin, 1992, 28(4): 58-62.
|
|
|
Abstract Studies were made of the influence of aging conditions and applied potentials onthe stress corrosion cracking (SCC) susceptibility, for an Al-Li-Cu-Mg alloy by slow strainrate technique. The relationship between the relative hydrogen content on specimen surface andthe applied potentials and elapsed time has also been examined. The SCC susceptibility wasfound to be dependent on aging conditions in which the peak aged condition gave the worstSCC resistance and the natural aged condition had the best one. The SCC susceptibility and sur-face hydrogen content are related to the applied potentials. The anodic potentials increase SCCsusceptibility, while the cathodic ones below the critical accelerate SCC. It is considered thatboth the anodic dissolution and hydrogen embrittlement contribute to SCC.
|
|
Received: 18 April 1992
|
1 Gray A. J Phys Colloq, 1987; 48(8) : C3-891 2 Rinker J G, Marek M, Sanders T H Jr. In: Starke E A Jr., Sanders T H Jr. eds., Aluminum-Lithium Alloys Ⅱ, Proc 2nd Int Aluminum-Lithium Conf, TMS-AIME, 1984: 597 3 Braun R, Buhl H. J Phys Colloq, 1987; 48(9) : C3-843 4 Christodulou L, Struble L, Pikens J R. In: Starke E A Jr., Sanders T H Jr. eds., Aluminum-Lithium Alloys Ⅱ, Proc 2nd Int Aluminum-Lithium Conf, TMS-AIME, 1984: 561 5 Balasubramaniam R, Duquette D J. In: Sanders T H Jr,, Starke E A Jr. eds., Aluminum-Lithium Alloys, Proc 5th Int Aluminum-Lithium Conf, Williamsburg, Virginia, March 27--31, 1989, Birmingham, UK: Materials and Component Engineering, 1989: 1271 6 Ahmad M. J Phys Colloq, 1987; 48(9) : C3-871 7 张匀,刘玉林,赵洪恩,胡壮麒,朱自勇,王政富.金属学报,1991;27:B271 8 Holroyd N J H, Gray A, Scainans G M, Heramnn R. In: Baker C, Gregson P J, Harris S J, Peel C J. Proc 3rd Int Aluminum-Lithium Conf, Oxford, UK, July, 1985, London: The Institute of Metals, 1986: 310 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|