CORRELATION OF ION-CLUSTER STRUCTURE WITH BULK VISCOSITY AND DENSITY OF TiO_2-BEARING MOLTEN SLAG |
DIAO Risheng;WANG Xiqing;WANG Huaiyong;ZHANG Rong;DU Hegui Iron and Steel Research Institute; Panzhihua Iron and Steel Company; Northeast University of Technology; Shenyang |
|
Cite this article:
DIAO Risheng;WANG Xiqing;WANG Huaiyong;ZHANG Rong;DU Hegui Iron and Steel Research Institute; Panzhihua Iron and Steel Company; Northeast University of Technology; Shenyang. CORRELATION OF ION-CLUSTER STRUCTURE WITH BULK VISCOSITY AND DENSITY OF TiO_2-BEARING MOLTEN SLAG. Acta Metall Sin, 1992, 28(3): 55-59.
|
Abstract An approach was made to correlate the proposed model of ion--cluster structureand structural parameter of TiO_2--bearing pentary system of molten slag with properties. Re-sults showed that an increase of ions with 4--coordination number in molten slag makes the in-crease of bulk viscosity and the decrease of density, while that with 6-coordination number iscontrary. The structural parameter proposed is so fairly interrelated to the properties of slag,that it may be available for the prediction about properties. In comparison with ions of4-coordination number, Ti is more effective than Al and Si.
|
Received: 18 March 1992
|
1 森永健次,杉之原幸夫,柳濑勉.日本金属学会志,1974;38:658--662 2 沟口数一,冈本一德,杉之原幸夫.日本金属学会志,1982;46:1055--1060 3 刁日升.东北工学院博士学位论文,1990 4 楠田泰敏,中村崇,柳濑勉.日本金属学会志,1977;41:160--164 5 谢冬生,毛裕文,郭昭信,朱元凯.钢铁,1986;21(1) :6--11 6 Van Der Colf J, Howat D D. J S Afr Inst Min Metall, 1979; 79: 255 7 边茂恕,马禄铭,王景唐.金属学报,1986;22:B90 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|