RELATIONSHIP BETWEEN FRACTAL DIMENSION AND CYCLIC CREEP PROPERTIES OF 34CrMoA ROTOR STEEL
YI Jianzhang (Shenyang Instituteal of Aeronautical Engineering); YANG Zhi'an; ZHU Shijie; WANG Zhongguang (Institute of Metal Research; Academia Sinica; Shenyang)
Cite this article: 

YI Jianzhang (Shenyang Instituteal of Aeronautical Engineering); YANG Zhi'an; ZHU Shijie; WANG Zhongguang (Institute of Metal Research; Academia Sinica; Shenyang). RELATIONSHIP BETWEEN FRACTAL DIMENSION AND CYCLIC CREEP PROPERTIES OF 34CrMoA ROTOR STEEL. Acta Metall Sin, 1992, 28(12): 18-22.

Download:  PDF(907KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Vertical section method has been used to measure the fractal dimension of cyclic creep fracture surfaces of 34CrMoA rotor steel at 550℃. The relationship between fractal dimension and cyclic creep properties has been analyzed. The fractal dimension is dependent upon the power product of minimum creep rate and rupture time, and satisfies the linear function with rupture strain.
Key words:  cyclic creep      fractal dimension      creep property      34CrMoA rotor steel     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I12/18

1 Mandelbrot B B, Passoja D E, Paullay A J. Natrure, 1984; 308:721
2 Wang Z G, Chen D L, Jiang Ⅹ Ⅹ, Ai S H, Shih C H. Scr Metall, 1988; 22:827
3 苏辉,张玉贵,阎振启.材料科学进展,1990;4:339
4 Huang Z H, Tian J F, Wang Z G. Mater Sci Eng, 1990; A129(2) : L1
5 Yang Z A, Bai Y L, Wang Z G, Zhou N B, Proc of C-MRS 90, Beijing: Elsevier Science Publishers,1991; 5:153
6 Dobes F, Milicka K. Mater Sci, 1976; 10:382
7 Pande C S, Ricchards L E, Louat N, Dempsey B D, Schwoeble A J. Acta Metall, 1987; 35:1633
[1] YANG Du, BAI Qin, HU Yue, ZHANG Yong, LI Zhijun, JIANG Li, XIA Shuang, ZHOU Bangxin. Fractal Analysis of the Effect of Grain Boundary Character on Te-Induced Brittle Cracking in GH3535 Alloy[J]. 金属学报, 2023, 59(2): 248-256.
[2] YANG Zhikun, WANG Hao, ZHANG Yiwen, HU Benfu. Effect of Ta Content on High Temperature Creep Deformation Behaviors and Properties of PM Nickel Base Superalloys[J]. 金属学报, 2021, 57(8): 1027-1038.
[3] CAO Jianghai, HOU Zibing, GUO Zhongao, GUO Dongwei, TANG Ping. Effect of Superheat on Integral Morphology Characteristics of Solidification Structure and Permeability in Bearing Steel Billet[J]. 金属学报, 2021, 57(5): 586-594.
[4] Zibing HOU,Jianghai CAO,Yi CHANG,Wei WANG,Han CHEN. Morphology Characteristics of Carbon Segregation in Die Steel Billet by ESR Based on Fractal Dimension[J]. 金属学报, 2017, 53(7): 769-777.
[5] Zheng LIU,Jiayi ZHANG,Haolin LUO,Keyue DENG. RESEARCH ON MORPHOLOGY EVOLUTION OF PRIMARY PHASE IN SEMISOLID A356 ALLOY UNDER CHAOTIC ADVECTION[J]. 金属学报, 2016, 52(2): 177-183.
[6] Yongchang LIU, Qianying GUO, Chong LI, Yunpeng MEI, Xiaosheng ZHOU, Yuan HUANG, Huijun LI. RECENT PROGRESS ON EVOLUTION OF PRECIPI-TATES IN INCONEL 718 SUPERALLOY[J]. 金属学报, 2016, 52(10): 1259-1266.
[7] DU Beining, YANG Jinxia, CUI Chuanyong, SUN Xiaofeng. EFFECTS OF GRAIN REFINEMENT ON CREEP PROPERTIES OF K417G SUPERALLOY[J]. 金属学报, 2014, 50(11): 1384-1392.
[8] YANG Jinxia ZHENG Qi SANG Zhiru LANG Haixia SUN Xiaofeng HU Zhuangqi. EFFECTS OF MELTING TREATMENTS ON THE MECHANICAL PROPERTIES OF REVERTED DZ40M ALLOY[J]. 金属学报, 2010, 46(12): 1511-1516.
[9] WU Xiaojun CHENG Wen QIAO Shengru ZOU Wu ZHANG Peng ZHANG Xiaohu. EVOLUTION OF PORES IN C/C COMPOSITE DURING RESIN IMPREGNATION-CARBONIZATION[J]. 金属学报, 2009, 45(11): 1402-1408.
[10] LIU Pilin;WANG Zhongguang(State Key Laboratory for Fatigue and Fracture of Materials;Institute of Metal Research;The Chinese Academy of Sciences;Shenyang 110015); WANG Wenlong (Shanghai Jiaotong University;Shanghai 200030);TODA Hiroyuki(Suzuki Motor Corp.Hamamatsu-nishi;P. O. Box 1;432-91 Hamamatsu; Japan);KOBA YASHI Toshiro(Toyohashi University of Technology;Toyohashi 441; Japan). STATIC CREEP AND CYCLIC CREEP BEHAVIOUR OF SiC_w/6061Al AND SiC_p/2024Al COMPOSITES AT ELEVATED TEMPERATURE[J]. 金属学报, 1997, 33(11): 1227-1232.
[11] LIU Ning; ZHAO Hingzhong; JIANG Laizhu; LUO Huiguo; HU Zhenhua; CUI Kun(Huazhong University of Science and Technology; Wuhan 430074). TRANSVERSE RUPTURE STRENGTH OF Ni BONDED Ti(C, N) CERMET AND FRACTAL DIMENSION ANALYSIS OF ITS FRACTURE SURFACES[J]. 金属学报, 1995, 31(5): 229-235.
[12] LI Xiaowu; TIAN Jifeng; KANG Yan; WANG Zhongguang(State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuscript received 1994-11-23; in revised form 1995-03-03). QUANTITATIVE ANALYSIS ON SURFACE ROUGHNESS OF FRACTURE[J]. 金属学报, 1995, 31(19): 311-317.
[13] LI Xueliang;LIN Jianxin (Hefei Polytechnical University). RANDOM FRACTAL STUDY OF FRACTURE SURFACE OF FREE-MACHINING STEELS[J]. 金属学报, 1994, 30(8): 380-384.
[14] LEI Weisheng;CHEN Bingsen(Tsinghua University;Beijing)(Manuscript received 4 November;1993). SELECTION OF MECHANICAL PARAMETERS IN APPLICATION OF FRACTAL TO FRACTURE RESEARCH[J]. 金属学报, 1994, 30(6): 269-273.
[15] LI Yunqing; TANG Xiangyun; M A Jusheng; HUANG Le(Tsinghua University; Beijing)(Manuscript received 19 July; 1993: in revised form 18 October; 1993). ISOTHERMAL SHEAR LOW-CYCLE FATIGUE BEHAVIOUR OF 62Sn-36Pb-2Ag SURFACE MOUNT SOLDER JOINTS[J]. 金属学报, 1994, 30(4): 164-169.
No Suggested Reading articles found!