Abstract The fracture surface of the normalized steel 55SiMnMo was observed, under tensile testing device equipped on SEM, to be of ductile dimple feature in the bainite which are composed of austenite and ferrite. The dimple is almost nucleated in the ferrite. Because the austenitic plastic deformation is remarkable during fracturing, the tear ridge of dimple is very sharp.
|
|
Received: 18 October 1992
|
1 刘正义,黄振宗,林鼎文.金属学报,1981;17:148 2 刘正义,李祖鑫,林鼎文.金属学报,1986;22:69 3 Sasaki G, Yokota M J. Metallography, 1975; 8: 265 4 Shechtman D. Metall Trans, 1976; 7A: 151 5 上海交通大学《金属断口分析》编写组.金属断口分析.北京:国防工业出版社,1976:80 6 徐永波,刘民治.金属学报,1982;18:58 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|