GROWTH MODE AND MODIFICATION OF GRAPHITE IN CAST IRON MELT
LIU Yongkun;YANG Shihao Southwestern Institute of Technology and Engineering; Chongqing; Shandong Polytechnical University; Jinan
Cite this article: 

LIU Yongkun;YANG Shihao Southwestern Institute of Technology and Engineering; Chongqing; Shandong Polytechnical University; Jinan. GROWTH MODE AND MODIFICATION OF GRAPHITE IN CAST IRON MELT. Acta Metall Sin, 1992, 28(1): 85-89.

Download:  PDF(620KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Using liquid quenching technique, the change of growth mode of graphite in cast iron melt was analysed. Based on the interface structure theory of crystal growth, the concept of multiplication of spiral growth steps was advanced and two basic multiplication models were given out. It was proposed that multiplication of spiral steps is responsible for the changeof growth mode of graphite in cast iron melt. The modifying elements such as cerium promote multiplication of spiral steps, which is regarded as the core of modification. Origination of screwdislocation and branch of the sector blocks in radius direction, both of which are essential to spheroidization of graphite in the melt, are caused by multiplication of spiral steps; and so is thickening of graphite plates.
Key words:  graphite      crystallization morphology      growth mode      spiral growth steps     
Received:  18 January 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I1/85

1 Hillert M, Lindblom Y. J Iron Steel Inst, 1954; 176: 388
2 Minkoff I, Nixon W C. J Appl Phys, 1966; 37: 4848--4855
3 陈熙琛.机械工程学报,1979;15(2) :122--152
4 Minkoff I,Lux B.见:Lux B, Minkoff I, Mollark F主编,上海工业大学,华中工学院,浙江大学合译.铸铁冶金学.北京:机械工业出版社,1983:315--328
5 Liu P C, Loper C R Jr., Kimura T, Park H K. Trans Am Foundrymen's Soc, 1980; 88: 97--118
6 刘永坤.山东工业大学硕士学位论文,1987
7 Jackson K A. In: Doremus R H, Robert B W, Turnbull D eds., Growth and Perfection of Crystals, Proc Int Conf on Crystal Growth, held Cooperstown, New York, August 27--29, 1958, New York: John Wiley Sons, 1958: 319
8 Purdy G R, Audier M. In: Fredriksson H, Hillert M eds., The Physical Metallurgy of Cast Iron. Proc 3rd Int Symp on the Physical Metalluregy of Cast Iron, Stockholm, Sweden, August 29--31, 1984. Elsevier Science, 1985: 13--24
9 Double D D, Hellawell A. Acta Metall, 1974; 22: 481--487
10 宋维锡,杨文英.金属学报,1987;23:B324
[1] HAN Ruyang, YANG Gengwei, SUN Xinjun, ZHAO Gang, LIANG Xiaokai, ZHU Xiaoxiang. Austenite Grain Growth Behavior of Vanadium Microalloying Medium Manganese Martensitic Wear-Resistant Steel[J]. 金属学报, 2022, 58(12): 1589-1599.
[2] YANG Gaolin, LIN Xin, LU Xiangang. Crystallization Morphology and Evolution Mechanism of Laser Multiple Remelting of Zr55Cu30Al10Ni5 Metallic Glass[J]. 金属学报, 2019, 55(12): 1544-1550.
[3] Xiaoyun LIU,Wenguang WANG,Dong WANG,Bolv XIAO,Dingrui NI,Liqing CHEN,Zongyi MA. Effect of Graphite Flake Size on the Strength and Thermal Conductivity of Graphite Flakes/Al Composites[J]. 金属学报, 2017, 53(7): 869-878.
[4] Junhui YAN,Zengyun JIAN,Man ZHU,Fang'e CHANG,Junfeng XU. SOLIDIFICATION CHARACTERISTICS AND MICRO-STRUCTURE OF HIGH UNDERCOOLED Al-70%Si ALLOY[J]. 金属学报, 2016, 52(8): 931-937.
[5] Wei FU,Xiaoguo SONG,Long LONG,Jianhang CHAI,Jicai FENG,Guodong WANG. INTERFACIAL MICROSTRUCTURE AND MECHANI-CAL PROPERTIES OF INDIRECT BRAZED GRAPHITE/COPPER JOINT[J]. 金属学报, 2016, 52(6): 734-740.
[6] Changjun WANG,Jianxiong LIANG,Zhenbao LIU,Zhiyong YANG,Xinjun SUN,Qilong YONG. EFFECT OF METASTABLE AUSTENITE ON MECHANI-CAL PROPERTY AND MECHANISM IN CRYOGENICSTEEL APPLIED IN OCEANEERING[J]. 金属学报, 2016, 52(4): 385-393.
[7] ZHANG Lei, ZHAO Honglei, ZHU Mingfang. SIMULATION OF SOLIDIFICATION MICROSTRUC-TURE OF SPHEROIDAL GRAPHITE CAST IRON USING A CELLULAR AUTOMATON METHOD[J]. 金属学报, 2015, 51(2): 148-158.
[8] XUE Yingyu, TANG Jiancheng, ZHUO Haiou, YE Nan, WU Tong, ZHOU Xusheng. MICROSTRUCTURES AND PROPERTIES OF LEAD-FREE FREE-CUTTING GRAPHITE-BRASS PREPARED BY GRAPHITIZATION OF CEMENTITE[J]. 金属学报, 2015, 51(2): 223-229.
[9] Xinning ZHANG,Yingdong QU,Rongde LI,Junhua YOU. MECHANISM OF CRACK NUCLEATION AND PROPA- GATION OF FERRITE DUCTILE IRON DURING IMPACT FRACTURE UNDER LOW TEMPERATURES[J]. 金属学报, 2015, 51(11): 1333-1340.
[10] CHEN Liqing SUI Fengli LIU Xianghua. GRAIN GROWTH MODEL OF INCONEL 718 ALLOY FORGED SLAB IN REHEATING PROCESS PRIOR TO ROUGH ROLLING[J]. 金属学报, 2009, 45(10): 1242-1248.
[11] JIANG Jianqing(Southeast University;Nanjing). EFFECTS OF GRAPHITE MORPHOLOGY AND MATRICES ON FRACTURE BEHAVIOUR OF CAST IRONS[J]. 金属学报, 1994, 30(8): 374-379.
[12] YANG Haining; GU Mingyuan;JIANG Weiji;ZHANG Guoding(Shanghai Jiaotong University). INTERFACIAL REACTION IN GRAPHITE FIBRES REINFORCED Al ALLOY COMPOSITES[J]. 金属学报, 1994, 30(20): 379-384.
[13] JIAO Yuning;LIU Qingmin;YANG Yuansheng; HU Zhuangqi (Institute of Metal Research;Chinese Academy of Sciences;Shenyang). MICRODYNAMICAL MECHANISM OF DYNAMIC SOLIDIFICATION OF ALLOYS[J]. 金属学报, 1994, 30(12): 540-544.
[14] YANG Jiguang Tianjin UniversityWANG Chumpi.associare professor;Faculty of Foundry.Tianjin Unicersity .Tianjin 300072. GRAPHITE NUCLEI IN CAST IRON UNDER INOCULATION TREATMENT[J]. 金属学报, 1993, 29(5): 63-67.
[15] ZHU Ruihui;WANG Yu;HAN Qiyong;SONG Weixi University of Science and Technology Beijing; Correspondent engineer; Institute of precise and Special New Materials; University of Science and Technology Beijing; Beijing 100083). DISTRIBUTION AND BEHAVIOUR OF Ce IN RE NODULAR CAST IRON[J]. 金属学报, 1992, 28(5): 26-31.
No Suggested Reading articles found!