Please wait a minute...
Acta Metall Sin  1991, Vol. 27 Issue (3): 106-110    DOI:
Current Issue | Archive | Adv Search |
DIFFUSION COEFFICIENTS IN α(δ)-PHASE OF Fe-Mn-Si TERNARY SYSTEM AT 1000℃
ZHU Xiaohe;YU Yongning University of Science and Technology Beijing
Cite this article: 

ZHU Xiaohe;YU Yongning University of Science and Technology Beijing. DIFFUSION COEFFICIENTS IN α(δ)-PHASE OF Fe-Mn-Si TERNARY SYSTEM AT 1000℃. Acta Metall Sin, 1991, 27(3): 106-110.

Download:  PDF(366KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The diffusion coefficients of Mn and Si in α(δ)-phase in an Fe-Mn-Siternary system have been determined at 1000℃. The composition profiles of Mnand Si at 1000℃ were made on the diffusion couples which composed of the alloyswith different compositions. Based on the composition profiles, the diffusion coeffi-cients of 18 compositions were obtained by using the Boltzmann-Matano method.The principal diffusion coefficients, D_(MnMn)~(Fe) and D_(SiSi)~(Fe) about 10~(-9) cm~2s~(-1), were foundto be fairly close each other, while the cross ones, D_(SiMn)~(Fe) and D_(MnSi)~(Fe), are less thanthe principal ones in one order of magnitude. D_(SiSi)~(Fe) increases slightly with the in-crease of Si and Mn compositions. And D_(MnMn)~(Fe) increases with the increase of Si com-position, but does not be affccted by Mn composition.
Key words:  diffusion coefficient      Fe-Mn-Si system     
Received:  18 March 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I3/106

1 Onsager L. Phys Rev, 1931; 37: 405
2 Onsager L. Phys Rev, 1932; 38: 2265
3 Rivlin V G. Int Met Rev, 1983; 28: 309
4 Roper G W, Whittle D P. Met Sci, 1980; 14: 541
5 Heyward T R, Goldstein J I. Metall Trans. 1973; 4: 2335
6 Kirkaldy J S, In: Advances in Materials Research, Vol. 4, New York: Interscience, 1970: 55
7 Malik M T, Bergner D. Cryst Res Technol, 1985: 20: 1283
[1] Yuanrong LIU,Weimin CHEN,Ying TANG,Yong DU,Lijun ZHANG. APPLICATION OF PRAGMATIC NUMERICAL INVERSE METHOD IN COMPUTATION OF INTERDIFFUSION COEFFICIENTS IN Al TERNARY ALLOYS[J]. 金属学报, 2016, 52(8): 1009-1016.
[2] Zujiang HUANG, Min ZHOU, Yang YANG, Quanzhi CHEN, Shiguang TANG, Weizhou LI. STUDY OF ANODIC ALUMINUM OXIDE FILM AS AN INTERLAYER TO SUPPRESS ELEMENT DIFFUSION[J]. 金属学报, 2016, 52(3): 341-348.
[3] ZHANG Jinling1,2,3, FENG Zhiyong1, HU Lanqing1,2,3,WANG Shebin1,2,3, XU Bingshe1,2,3. PRECIPITATION BEHAVIOR OF AZ91 MAGNESIUM ALLOYS WITH DIFFERENT La CONTENTS[J]. 金属学报, 2012, 48(5): 607-614.
[4] . PHASE FIELD SIMULATION OF SINTERING PROCESS IN BIPHASIC POROUS MATERIAL[J]. 金属学报, 2012, 48(10): 1207-1214.
[5] CHEN Yexin CHANG Qinggang. EFFECT OF TRAPS ON DIFFUSIVITY OF HYDROGEN IN 20g CLEAN STEEL[J]. 金属学报, 2011, 47(5): 548-552.
[6] . The distribution and diffusion of carbon atoms during deformation of undercooled austenite in medium carbon steel[J]. 金属学报, 2007, 43(8): 785-790 .
[7] LIU Shi; ZHENG Hua; GUI Quanhong; MA Aihua; YU Hongbo; WANG Longbao. MEASUREMENTS OF HYDROGEN DIFFUSION COEFFICIENT FOR TUBE SAMPLES AT MEDIUM AND HIGH TEMPERATURES[J]. 金属学报, 2004, 40(4): 393-398 .
[8] DING Jinjun;ZHAO Gang;HAO Shiming (Northeastern University; Shenyang 110006). PHASE EQUILIBRIUM RELATIONSHIPS AND INTERDIFFUSION COEFFICIENTS OF β,α ANDγIN THE Ti-Al BINARY SYSTEM[J]. 金属学报, 1997, 33(10): 1105-1109.
[9] YANG Qiqin; (Department of Chemistry; Zhongshan University; Guangzhou 510275) QIU Kairong; LIU Guankun; GUAN Tong(Zhongshan University;Guangzhou 510275). ELECTROCHEMICAL BEHAVIOUR FOR REDUCTION OF Tm~(3+) IN MOLTEN CHLORIDES[J]. 金属学报, 1995, 31(22): 445-450.
[10] WANG Wendong; ZHANG Sanhong; HE Xinlai(University of Science and Technology Beijing; 100083)(Manuscript received 93-09-21. in revised form 94-01-26). DIFFUSION OF BORON IN Fe-BASE AND Ni-BASE ALLOYS[J]. 金属学报, 1995, 31(2): 56-63.
[11] WU Zhichun Institute of Chemical Metallurgy; Academia Sinica; Beijing. DETERMINATION OF DIFFUSION COEFFICIENT OF CuCl_2 IN AQUEOUS SOLUTIONS[J]. 金属学报, 1991, 27(4): 93-99.
[12] YANG Zhen'guo;DU Weixi;DU Senlin;LIU Sulan Jilin University of Technology; Changchun Changchun Institute of Applied Chemistry; Academia Sinica. DIFFUSION OF La IN LIQUID Al-Si ALLOY[J]. 金属学报, 1989, 25(2): 104-108.
No Suggested Reading articles found!