MULTICOMPONENT SEGREGATION ALONG BOUNDARY AND THERMODYNAMICAL ANALYSIS OF Fe-C-Si-Mn ALLOY
LI Shuchen;LIU Shikai Southwestern Jiaotong University; Chengdu
Cite this article: 

LI Shuchen;LIU Shikai Southwestern Jiaotong University; Chengdu. MULTICOMPONENT SEGREGATION ALONG BOUNDARY AND THERMODYNAMICAL ANALYSIS OF Fe-C-Si-Mn ALLOY. Acta Metall Sin, 1991, 27(3): 101-105.

Download:  PDF(511KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Studies were made of the positive segregation of C and Mn as wellas negative one of Si along the original austenite boundary in 475℃ isothermalFe-C-Si-Mn alloy by means of Auger spectroscopy and SIMS. According to thethermodynamical calculation of partial molar free energy and activity of grainboundary segregation, it was indicated that the Si and Mn may promote the segrega-tion of C along grain boundary and depress its activity. Thus, the shift of theupper bainite TTT diagram to right may be easily explained.
Key words:  Fe-C-Si-Mn alloy      segregation energy      activity     
Received:  18 March 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I3/101

1 Bhadeshia H K D H, Edmonds D V. Metall Trans, 1979; 10A: 895
2 Liu S K, Reynolds W T Jr., Hu H, Shiflet G J, Aaronson H I. Metall Trans, 1985; 16A: 457
3 Enomoto M, White C L, Aaronson H I. Metall Trans. 1988; 19 A: 1807
4 Guttmann M, McLean D. Interfacial Segregation, Metals Park, Ohio: ASM, 1970: 261
5 Foo E-H, Lupis C H L. Acta Metall, 1973; 21: 1409
6 Sigworth G K, Elliott J F. Met Sci, 1974; 8: 298
[1] JU Tianhua, SHU Nian, HE Wei, DING Xueyong. A Predicted Model for Activity Interaction Coefficient Between Solutes in Alloy Solutions[J]. 金属学报, 2023, 59(11): 1533-1540.
[2] Rongyao MA, Lin ZHAO, Changgang WANG, Xin MU, Xin WEI, Junhua DONG, Wei KE. Influence of Hydrostatic Pressure on the Thermodynamics and Kinetics of Metal Corrosion[J]. 金属学报, 2019, 55(2): 281-290.
[3] Xiaofeng LU, Ming XIAO, Yangmei CHEN, Bangcheng YANG. Bioactivity of Titanium Metal Hybridized with Inactivated Bacterial Biofilm[J]. 金属学报, 2017, 53(10): 1402-1412.
[4] Muqin LI, Haitao YAO, Fanghong WEI, Mingda LIU, Zan WANG, Shuhao PENG. The Microstructure and in Vivo and in Vitro Property of Multi-Component Composite Films on the Biomedical Pure Magnesium Surface[J]. 金属学报, 2017, 53(10): 1337-1346.
[5] Xiaoyan CHEN,Zhe JIN,Xuefeng BAI,Yizhou ZHOU,Tao JIN,Xiaofeng SUN. EFFECT OF C ON THE INTERFACIAL REACTION AND WETTABILITY BETWEEN A Ni-BASED SUPERALLOY AND CERAMIC MOULD[J]. 金属学报, 2015, 51(7): 853-858.
[6] Dongsong RONG,Yong JIANG,Jianming GONG. EXPERIMENTAL RESEARCH AND THERMODYNAMIC SIMULATION OF LOW TEMPERATURE COLOSSAL CARBURIZATION OF AUSTENITIC STAINLESS STEEL[J]. 金属学报, 2015, 51(12): 1516-1522.
[7] WU Ling. The improvement of regular solution model based on GA-NN and its application in binary slag system[J]. 金属学报, 2008, 44(7): 799-802 .
[8] Yuan Liu. Improvement of Calculation Method for the Activity Coefficient of Multi-component Alloys[J]. 金属学报, 2007, 43(5): 503-508 .
[9] LE Qichi; CUI Jianzhong. Thermodynamics Properties of Ternary Bath of Coloring Hot--Dip Galvanization[J]. 金属学报, 2006, 42(11): 1182-1186 .
[10] MA Zhongting; J. OHSER; D. JANKE(The Institute of Iron and Steel Technology; Freiberg University of Mining and Technology; Freiberg; Germany). THERMODYNAMIC DESCRIPTION OF MULTICOMPONENT SYSTEMS BY INTERACTION MRAMETERS[J]. 金属学报, 1998, 34(7): 753-762.
[11] LUO Lihua; DING Xueyong; GUO Dan; CAO Wenbin; ZOU Zongshu; WANG Wenzhong (School of Materials and Metallurgy; Northeastern University; Shenyang 110006)( University of Science and Technology Beijing; Beijing 1100083). DATABASE SOFTWARE DEVELOPMENT FOR ACTIVITY AND INTERACTION MRAMETER OF ALLOY SYSTEMS[J]. 金属学报, 1998, 34(4): 388-392.
[12] ZHANG Ziqing(Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015). DISCUSSION ON THE METHOD TO DETERMINE THE ACTIVITY IN SLAGS BY MEANS OF THE SLAGMETAL EQUILIBRIA IN A LIQUID STATE[J]. 金属学报, 1998, 34(3): 299-304.
[13] CHEN Erbao; DONG Yuanchi; GUO Shangxing (EaSt China Institute of Metallurgy; Ma'anshan 243002) (Manuscript received 1996-09-15; in revised form 1996-11-25). STUDY ON THERMODYNAMICAL PROPERTIES IN Mn-Fe ALLOY MELTS[J]. 金属学报, 1997, 33(8): 831-837.
[14] ZHANG Jian (University of Science and Technology Beijing; Beijing 100083). CALCULATING MODELS OF MASS ACTION CONCENTRATIONS FOR SEVERAL MOLTEN BINARY SALTS[J]. 金属学报, 1997, 33(5): 515-523.
[15] ZHANG Xiaobing;JIANG Guochang;XU Kuangdi (Shanghai University; ShanghaiEnhanced Lab of Ferrometallurgy; Shanghai 200072). HIGH ORDER SUB-REGULAR SOLUTION MODEL AND ITS APPLICATIONS IN THE CALCULATION OF COMPONENT ACTIVITIES OF MnO-SiO_2-Al_2O_3-CaO MOLTEN SLAG[J]. 金属学报, 1997, 33(10): 1085-1093.
No Suggested Reading articles found!