Please wait a minute...
Acta Metall Sin  1991, Vol. 27 Issue (2): 27-32    DOI:
Current Issue | Archive | Adv Search |
BORON DISTRIBUTION IN BCCINTERMETALLIC COMPOUND Fe_3(Si,Al) AND IMPROVEMENT ON ITS BRITTLENESS
SHAO Yuanzhi;GU Shouren;CHEN Nanping Tsinghua University; Beijing
Cite this article: 

SHAO Yuanzhi;GU Shouren;CHEN Nanping Tsinghua University; Beijing. BORON DISTRIBUTION IN BCCINTERMETALLIC COMPOUND Fe_3(Si,Al) AND IMPROVEMENT ON ITS BRITTLENESS. Acta Metall Sin, 1991, 27(2): 27-32.

Download:  PDF(1610KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Studies were made of the influence of B distribution in bcc lattice in-termetallic compound Fe_3(Si, Al) on the long range order and the improvement onits brittleness. A new mechanism concerning weakening of grain interiors is put for-ward. Based on this mechanism, the brittleness improvement of the bcc intermetallicswith B addition could be well explained.
Key words:  Fe(Si      Al)      brittleness      boron      long range order      microenvironment     
Received:  18 February 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I2/27

1 Liu C T, White C L, Horton J A. Acta Metall, 1985; 33: 213
2 Stoloff N S. High-Temperature Ordered Intermetallic Alloys, Vol. 39. Pittsburgh, Penneylvania: Materials Reseach Society, 1985: 3
3 邵元智,顾守仁,陈南平,清华大学学报(自然科学版), 1989; 29(5) : 25
4 Shao Yuanzhi, Gu Shouren, Chen Nanping. In: C-MRS International'90 Abstracts, June 18--22, 1990, Beijing, China, 1990: 116
5 Koch C C. High-Temperature Ordered Intermetallic Alloys, Vol. 39, Pittsburgh, Penneylvania: Materials Reseach Society, 1985: 397
6 Marcinkowski MJ, Taylor M F. J Mater Sci, 1975; 10: 406
7 Ehlers S K, Mendiratta M G. J Mater Sci, 1984; 19: 2203
8 Crawford R C, Ray I L F, Cockayne D J H. Philos Mag, 1973; 27: 1
9 Marcinkowski M J. In: Thomas G, Washburn J eds., Electron Microscopy and Strength of Crystals, New York: Interscience, 1963: 333
10 Athanassiadis G, Le Caer G, Feet J, Rirnlinger L. Phys Status Solid, 1977; 40A: 425
11 Mendiratta M G. Lipsitt H A. In: C-MRS International'90 Abstracts, June 18--22, 1990, Beijing, China. 1990: 155
[1] Kejian LI,Zhipeng CAI,Yao WU,Jiluan PAN. Research on Austenite Transformation of FB2 Heat-Resistant Steel During Welding Heating Process[J]. 金属学报, 2017, 53(7): 778-788.
[2] LUO Xinmin, CHEN Kangmin, ZHANG Jingwen, LU Jinzhong,REN Xudong,LUO Kaiyu, ZHANG Yongkang. DISLOCATION MECHANISM OF SURFACE MODIFICATION FOR COMMERCIAL PURITY ALUMINUM  AND ALUMINUM ALLOY BY LASER SHOCK PROCESSING[J]. 金属学报, 2013, 49(6): 667-674.
[3] PENG Yingbo, CHEN Feng, WANG Minzhi, SU Xiang, CHEN Guang. RELATIONSHIP BETWEEN MECHANICAL PROPERTIES AND LAMELLAR ORIENTATION OF PST CRYSTALS IN Ti-45Al-8Nb ALLOY[J]. 金属学报, 2013, 49(11): 1457-1461.
[4] ZHAO Shengsheng CHENG Yu CHANG Zhengkai WANG Tiegang SUN Chao. MODIFICATION OF STRESS DISTRIBUTION ALONG THE THICKNESS OF (Ti, Al)N COATINGS AND PREPARATION OF THE COATINGS WITH LARGE THICKNESS[J]. 金属学报, 2012, 48(3): 277-282.
[5] FAN Yongzhong ZHANG Shujuan TU Jinwei SUN Xia LIU Fang LI Mingsheng. INFLUENCE OF DOPING WITH Si AND Y ON STRUCTURE AND PROPERTIES OF (Ti, Al)N COATING[J]. 金属学报, 2012, 48(1): 99-106.
[6] . Effect of boron on the microstructure and mechanical properties of as-cast TiAl alloy[J]. 金属学报, 2007, 43(5): 487-492 .
[7] ;. Effect of Solidification Condition on Structure and Properties of High Boron Iron-Base Alloy[J]. 金属学报, 2007, 43(5): 477-481 .
[8] QIU Shengtao; XIAO Lijun; LIU Jiaqi; GAN Yong. Softening Mechanism of Boron—Bearing Low--Carbon Hot Strips Produced by TSCR Route[J]. 金属学报, 2006, 42(11): 1202-1206 .
[9] TANG Bei; LIU Yongli; ZHENG Hong; LI Feng; CONG Hongtao; CHENG Huiming. MICROSCOPIC CHARACTERIZATION AND HRTEM IMAGES OF BORON NITRIDE NANOTUBES[J]. 金属学报, 2005, 41(9): 905-909 .
[10] CHEN Guosheng; JIN Xin; ZHOU Dianhua; WANG Shipu; XIE Wei; WANG Lintao. Effects of Boron Content on Boundaries Precipitates in Ni Base Alloy GH4049 and Its High Temperature Properties[J]. 金属学报, 2005, 41(6): 622-626 .
[11] ZHENG Jingdi; ZOU Yousheng; SONG Guihong; GONG Jun; LIU Yue; SUN Chao; WEN Lishi. STUDY OF (Ti,Al)N COATINGS ON SiCp/Al SUBSTRATE[J]. 金属学报, 2004, 40(7): 745-748 .
[12] MA Shengli; XU Jian; JIE Wanqi; XU Kewei; M. G. J. Veprek--Heijman; S. Veprek. Characterization of Microstructure and Hardness of PCVD DepositedTi1-xAlx N Hard Coatings[J]. 金属学报, 2004, 40(6): 669-.
[13] LI Fan; ZHANG Dengjun; LI Baohou; LUO Shimin. Chemical Plating Nickel on the Surface of Hexagonal Boron Nitride Micro-Particles and Its Kinetic Model[J]. 金属学报, 2004, 40(2): 173-178 .
[14] WANG Yu; LIN Dongliang(T. L. Lin)(Department of Materials Science; the Open Laboratory of Education Ministry for High-Temperature Materials and Test; Shanghai Jiao Tong University; Shanghai 200030)ZHOU Yuanxin; XIA Yuanming (Department of Morden Dynamics; University of Science and Technology of China; Hefei 230026)C. C. Law (Materials and Mechanics Engineering; United Technologies Company-Pratt & Whittney 400 Main Street; East Hartford; CT 06108; U. S. A.)Correspondent: LIN Dongliang; professon Tel: (021)62812544(O); (021)62835352(H);Fax: (021)62820892; E-mail: dllin@ mail. sjtu. edu. cn.. THE EFFECT OF MINOR BORON ADDITION ON DYNAMIC TENSILE PROPERTIES OF WROUGHT Ti-47Al-2Mn-2Nb ALLOY[J]. 金属学报, 1998, 34(9): 915-918.
[15] WU Zhengan; GU Mingyuan; CHEN Yu; ZHANG Gooding (The State Key Laboratory of MMCs; Shanghai Jiaotong University; Shanghai 200030). THE INTERFACE MICROSTRUCTURE OF A B_4C_p +SiC_w/MB15 MAGNESIUM BASED COMPOSITE[J]. 金属学报, 1998, 34(4): 443-448.
No Suggested Reading articles found!