Acta Metall Sin  1991, Vol. 27 Issue (2): 148-150    DOI:
Current Issue | Archive | Adv Search |
A 500℃ ISOTHERMAL SECTION OF Ag-Cu-P SYSTEM
ZENG Lingmin;ZHUANG Yinghong;Ll Dexuan;LIN Weibo Guangxi University; Nanning
Cite this article: 

ZENG Lingmin;ZHUANG Yinghong;Ll Dexuan;LIN Weibo Guangxi University; Nanning. A 500℃ ISOTHERMAL SECTION OF Ag-Cu-P SYSTEM. Acta Metall Sin, 1991, 27(2): 148-150.

Download:  PDF(243KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The 500℃ isothermal section with P up to 23 wt-% and the verticalsections containing 6 wt-%P and 2 wt-%Ag of Cu-rich Ag-Cu-P ternary system weredetermined by X-ray diffraction, μDTA and metallography. The isothermal sectioncontains 3 single-phase regions, 3 two-phase regions and 1 three-phase region. Themaximum solubility of Ag or P in Cu is 1.5 or 1.2 wt-% respectively, while thatof Cu in Ag is 1.8 wt-%. One ternary eutectic reaction of composition, by wt-%,18Ag-74.5Cu-7.5P exists at 650℃.
Key words:  Ag-Cu-P system      isothermal section      vertical section     
Received:  18 February 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I2/148

1 Hansen M. Constitution of Binary Alloys. New York: McGraw-Hill, 1958: 18--19
2 1972; 8(6) : 1015--1018
3 Karakaya I, Thompson W T. Bulletin of Alloy Phase Diagram. 1988; 9: 232--236
4 Лашко Н Ф,Лашко-авакян С В.庄鸿寿,邹僖译.金属的钎接.北京:中国工业出版社,1963:104
[1] LI Juntao; HAO Shiming (Northeastern University; Shenyang 110006). ^^α(α_2)/ PHASE EQUILIBRIA IN Ti-Al-Si SYSTEM[J]. 金属学报, 1996, 32(11): 1171-1176.
[2] QIN Gaowu;HAO Shiming;ZENG Ninghua (Northeastern University;Shenyang 110006)(Manuscript received 1994-11-04;in revised form 1995-05-04). α(α_2)/γ PHASE EQUILIBRIA IN Ti-Al-Ga AND Ti-Al-Nb-Cr SYSTEMS[J]. 金属学报, 1995, 31(23): 484-488.
[3] HAO Shiming; ZENG Ninghua (Northeastern University; Shenyang 110006)(Manuscript received 1994-11-16). ISOTHERMAL SECTION OF PHASE DIAGRAM IN Ti-Al-Cr TERNARY SYSTEM AT 1000℃[J]. 金属学报, 1995, 31(16): 152-158.
[4] WAN Jinglong(Anhui Institute of Technology; Hefei); BI Qinghua(Shanghai University of Science and Technology). Gd-CoAl VERTICAL SECTION OF Gd-Co-Al PHASE DIAGRAM[J]. 金属学报, 1994, 30(17): 204-207.
[5] GONG Fangyue;GOLDSTEIN JI Tianjin University; Lehigh University; Bethlehem; U. S. A. Correspondent associate professor; Department of Materials Science; Tianjin University; Tianjin 300072. 550 AND 450℃ ISOTHERMAL SECTIONS OF Fe-Ni-C PHASE DIAGRAM[J]. 金属学报, 1992, 28(6): 47-51.
[6] ZHANG Kanghou;CHEN Lili Institute of Precious Metals; Kunming. ROOM TEMPERATURE AND 700℃ ISOTHERMAL SECTIONS OF Gd-Pd-Pt(Gd≤33 at. -%) PHASE DIAGRAM[J]. 金属学报, 1991, 27(3): 147-149.
[7] CHEN Rongzhen;ZHANG Hanxing;ZHENG Jianxuan;HE Hanping Guangxi University; Nanning Guangxi Institute of Non-Ferrous Metals Geology; Nanning CHEN Rongzhen;Department of Physics;Guangxi University; Nanning;530009 Guangxi. 410℃ ISOTHERMAL SECTION OF Al-Cu-Sb TERNARY SYSTEM PHASE DIAGRAM[J]. 金属学报, 1989, 25(5): 142-143.
[8] ZHANG Ning;LUO Yang Centrol Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing. PHASE DIAGRAM OF Nd-Fe-B TERNARY SYSTEM II. TWO VERTICAL SECTIONS WITH CONSTANT Nd AND B RESPECTIVELY, PASSING THROUGH Nd_2Fe_(14)B POINT[J]. 金属学报, 1989, 25(2): 121-127.
[9] ZHANG Ning;LUO Yang Central Iron and Steel Research Institute; Ministry of Metallurgical Industry Beijing. PHASE DIAGRAM OF Nd-Fe-B TERNARY SYSTEM I. ISOTHERMAL SECTION AT ROOM TEMPERATURE[J]. 金属学报, 1989, 25(2): 116-120.
No Suggested Reading articles found!