Abstract The effect of austenitizing temperature on segregation of impurities alonggrain boundaries in 4330M steel has been examined by AES. The impurities segregation wascomputed quantitatively. Sulphur is revealed to segregate along austenite grain boundarieswhen steel quenched at 870 or 1000℃. No segregation will occur at quenching temperatureup to 1100 or 1200℃. However, the segregation becomes quite serious under stepped quenchingfrom 1200 to 870℃. The limitation of the Maclean expression for equilibrium segregation wasdiscussed.
1 McMahon C J Jr., Briant C L, Banerji S K. In: Taplin C M R ed, Fracture 1977, Advances in Research on the Strength and Fracture of Materials, Vol. Ⅰ, Int Conf on Fracture, 4th, Waterloo, Canada, June 19--24, 1977, New York: Pergamon, 1978: 363 2 新君和嘉.国外金属材料,1982;(2) :18 3 Briant C L, Banerji S K. Metall Trans, 1982; 13A: 827 4 Clayton J Q, Knott J F. Met Sci, 1982; 16: 145 5 McLean D. Grain Boundaries in Metals, Oxford University Press, 1957
ZHU Yuru; GUO Shuqiang; XU Jianlun; JIANG Guochang (Shanghai Enhanced Laboratory of Ferrometallurgy; Shanghai University; Shanghai 200072); YU Diwei;PAN Liying; WANG Yueqiang (Institule of Iron & Steel; Baoshan Iron & Steel Corporatton; Shanghai 201900)(Manuscript received 1995-10-20; in revised form 1996-02-08). FORMATION OF INTRAGRANULAR FERRITE PLATES AND THEIR EFFECT ON HEAT AFFECTED ZONE OF STEEL X-60[J]. 金属学报, 1996, 32(8): 891-89.
YUE Kexiang;DONG Yuanchi East China Institute of Metallurgy; Maanshan Department of Metallurgy;East China Institute of Metallurgy; Maanshan 243004. EQUILIBRIA OF Sr, Ba AND O, S IN LIQUID Fe[J]. 金属学报, 1990, 26(4): 98-102.
[10]
JIANG Guochang;XU Kuangdi;DENG Jianxiong Shanghai University of Technology GUO Zhancheng; GUAN Yulong University of Science and Technology Beijing Institute of Metallurgy and Materials;Shanghai University of Technology; Shanghai 200072. KINETIC STUDY OF DESULPHURIZATION ALONG METAL-SLAG INTERFACE[J]. 金属学报, 1990, 26(1): 113-119.