MICROSTRUCTURE AND REVERSE SHAPE MEMORY EFFECT IN A Cu-Zn-Al ALLOY
DONG Jianxin;CHEN Fumin;CHEN Jinming;LIU Wenxi Tianjin University
Cite this article: 

DONG Jianxin;CHEN Fumin;CHEN Jinming;LIU Wenxi Tianjin University. MICROSTRUCTURE AND REVERSE SHAPE MEMORY EFFECT IN A Cu-Zn-Al ALLOY. Acta Metall Sin, 1990, 26(6): 81-83.

Download:  PDF(1081KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The bainite structure related to the reverse shape memory effect has been observ-ed by means of TEM in a Cu-Zn-Al alloy. The reverse memory effect may be improved upto one order of magnitude under applied constraint stress. The widespread propagation of bai-nite was confirmed to be the diffusion controlled shear process by phenomina observed both theparabolic configuration of side interface of bainite plate and the twisting of intersected bainiteplates.
Key words:  Cu-Zn-Al memory alloy      reverse shape memory effect      bainitic transformation     
Received:  18 June 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I6/81

1 Reyhani M M, McCormick P G. Scr Metall, 1986; 20: 571
2 Takezawa K, Sato S. Trans Jpn Inst Met., 1988; 29: 894
3 Koyama Y, Nittono O. Scr Metall, 1984; 18: 1075
4 韩明,陈复民,陈金铭,陈玉如,刘文西.金属学报,1990;26:A81
5 Papapetrou A. Z Krist, 1935; 92: 108
6 Trivedi R. Metall Trans, 1970; 1: 921
[1] WAN Xiangliang, HU Feng, CHENG Lin, HUANG Gang, ZHANG Guohong, WU Kaiming. Influence of Two-Step Bainite Transformation on Toughness in Medium-Carbon Micro/Nano-Structured Steel[J]. 金属学报, 2019, 55(12): 1503-1511.
[2] WANG Changjun, SUN Xinjun, YONG Qilong, LI Zhaodong, ZHANG Xi, JIANG Lu. EFFECT OF BAINITIC TRANSFORMATION TEMPERATURE ON THE MICROSTRUCTURES AND MECHANICAL PROPERTIES OF THE HOT ROLLED TRIP STEEL CONTAINING Ti AND Mo AND ITS PRECIPITATION CHARACTERISTICS[J]. 金属学报, 2013, 29(4): 399-407.
[3] XU Zuyao T. Y. Hsu. Effect of Stress on Bainitic Transformation in Steel[J]. 金属学报, 2004, 40(2): 113-119 .
[4] J.W.Christian FRS(Department of Materials; Oxford University; Parks Road; Oxford OX1 3PH; UK). INTERFACES IN PHASE TRANSFORMATIONS[J]. 金属学报, 1997, 33(2): 150-156.
[5] FANG Hongsheng;WANG Jiajun(Tsinghua University; Beijing)(Manuscript received 20 July; 1994). SYMPATHETIC-LEDGEWISE MECHANISM OF BAINITIC TRANSFORMATION[J]. 金属学报, 1994, 30(11): 491-501.
[6] FANG Hongsheng;LI Chunming;WANG Jiajun Tsinghua University; Beijing100084. INITIAL α_1 PLATES AND THREE-DIMENSIONAL LEDGES OF BAINITE IN A Cu-Zn-Al ALLOY[J]. 金属学报, 1993, 29(9): 1-5.
[7] XU Zuyao;ZHOU Xiaowang T. Y. Hsu; Shanghai Jiaotong University Correspondent professor; Department of Materials Science; Shanghai Jiaotong University; Shanghai 200030. THERMODYNAMICS OF BAINITIC TRANSFORMATION IN A Cu-24at.-%Al ALL0Y[J]. 金属学报, 1992, 28(6): 26-28.
[8] CAO Renhuan;MA Hongti Northest University of Technology;ShenyangYAN Zhenqi Professor;Depariment of Metallic Materials;Northeast University of Technology;Wenhua Rood;Shenyang. BAINITIC TRANSFORMATION IN LOW CARBON Mn-Nb-V AND Mn-Mo-Nb-V STEELS[J]. 金属学报, 1988, 24(2): 135-138.
No Suggested Reading articles found!