Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (3): 119-125    DOI:
Current Issue | Archive | Adv Search |
VARIATIONAL CALCULATION OF THERMODYNAMIC PROPERTIES OF SUPERCOOLED LIQUID METALS
SHEN Tao; WANG Jingtang Institute of Metal Research Academia Sinica; Laboratory of Rapidly Solidified Non-Equilibrium Alloys; Shenyang professor
Cite this article: 

SHEN Tao; WANG Jingtang Institute of Metal Research Academia Sinica; Laboratory of Rapidly Solidified Non-Equilibrium Alloys; Shenyang professor. VARIATIONAL CALCULATION OF THERMODYNAMIC PROPERTIES OF SUPERCOOLED LIQUID METALS. Acta Metall Sin, 1990, 26(3): 119-125.

Download:  PDF(569KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  By means of the Gibbs-Bogoliubov (GB) thermodynamical variationalcalculation, the thermodynamical properties of the liquid metals as supercooled sta-te, such as Al, Ga, Tl in the 3rd family of periodic table and transition metal Tiwere calculated using the hard-sphere (HS) system as reference. The values of meanatomic volume, Helmholtz free energy, internal energy and entropy as well asspecific heat at constant volume, isothermal bulk modulus, thermal expansion co-efficient and specific heat under constant pressure were determined. The glass tran-sition temperature, T_g, is easily obtained from c_p-T plot. The glass forming abili-ty for metal can be predicted with T_g/T_m, which is in agreement with the experi-mental results.
Key words:  supercooled metal      hard-sphere system      thermodynamic variational calculation      specific heat      glass transition temperature     
Received:  18 March 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I3/119

1 Klinger M I. Phys Rep, 1988; 165: 275
2 Jaeckle J. Rep Prog Phys, 1986; 49: 171
3 Shimoji M. Liquid Metals, New York: Academic Press, 1977
4 Heine V. Solid State Phys, 1970; 24: 1
5 Li D H, Li X R, Wang S. J Phys, 1986; F16: 309
6 Woo C H, Wang S, Matsuura M. J Phys, 1975; F5: 1836
7 Li D H, Moore R A, Wang S. Can J Phys, 1986; 64: 75 Li D H, Moore R A, Wang S. Can J Phys, 1986; 64: 852
8 Li D H, Moore R A, Wang S. J Chem Phys, 1988; 88: 2700 Li D H, Moore R A, Wang S. J Chem Phys, 1988; 89: 4309
9 Ashcroft N W, Lekner J. Phys Rev, 1966; 145: 83
10 Hultgren R, Desai P D, Hawkins D T, Gleiser M, Kelley K K, Wagman D D. Selected Values of the Thermodynamic Properties of the Elements, Ohio: ASM, 1973
11 Brandes E A. Smithells Metals Reference Book. 6th ed, London: Butterworth, 1983
12 Cohen M H, Grest G S. Phys Rev, 1979; B20: 1077|
[1] Tingting JIA,Zengyun JIAN,Junfeng XU,Man ZHU,Fang'e CHANG. CHARACTERISTIC TEMPERATURE AND PERFOR-MANCE OF THE Ge30Se70 CHALCOGENIDE GLASS[J]. 金属学报, 2016, 52(6): 755-760.
[2] Jiaojiao LI,Zengyun JIAN,Man ZHU,Junfeng XU,Fang'e CHANG,Min XIANG. STUDY ON THERMODYNAMIC PROPERTIES AND KINETICS FRAGILITY OF GexSe90-xSb10 CHALCOGENIDE GLASSES[J]. 金属学报, 2015, 51(11): 1384-1390.
[3] JIANG Qing;XU Xiaoya;ZHAO Ming (Jilin University of Technoloasl; Changchun 130025). RELATIONSHIP BETWEEN VOGELFULCHER LAW AND GLASS TRANSITION TEMPERATURE[J]. 金属学报, 1997, 33(7): 763-768.
[4] JIANG Qing;XU Xiaoya; Li Jianchen (Jilin University of Technology; Changchun130025). SPECIFIC HEAT AND KAUZMANN TEMPERATURE OF PtNiP ALLOY[J]. 金属学报, 1997, 33(6): 660-666.
[5] WEI Bingbo; WANG Bin(Northwestern Polytechnical University; Hi'an)BARTH M;HERLA CH D M(Institut for Raumsimulation; DLR; Germany). THERMODYNAMIC DRIVING FORCE FOR RAPID CRYSTALLIZATION OF LIQUID METALS[J]. 金属学报, 1994, 30(19): 289-293.
[6] TONG Huayu;DING Bingzhe;JIANG Honggang;LI Shuling;LI Gusong;WANG Jingtang State Key Laboratory of RSA; Institute of Metal Research; Academia Sinica; Shenyang Correspondent Research assistant; Institute of Metal Research; Academia Sinica; Shenyang 110015. THERMAL PROPERTIES OF NANOCRYSTALLINE Fe_(78)B_(13)Si_9 ALLOY[J]. 金属学报, 1992, 28(6): 71-75.
[7] WEI Bingbo;YANG Gencong;ZHOU Yaohe Northwestern Polytechnical University; Xi'an. DENUCLEATION AND HIGH UNDERCOOLING OF Ni-32.5%Sn EUTECTIC ALLOY[J]. 金属学报, 1990, 26(5): 119-124.
No Suggested Reading articles found!