COLD ROLLING TEXTURE AND RECRYSTALLIZATION TEXTURE OF CROSS SHEAR ROLLED COMMERCIAL COPPER
LIU Yansheng;ZHAO Xiong;LIANG Zhide Northeast University of Technology; Shenyang Department of Materials Science and Engineering;Northeast University of Technology;Shenyang 110006
Cite this article:
LIU Yansheng;ZHAO Xiong;LIANG Zhide Northeast University of Technology; Shenyang Department of Materials Science and Engineering;Northeast University of Technology;Shenyang 110006. COLD ROLLING TEXTURE AND RECRYSTALLIZATION TEXTURE OF CROSS SHEAR ROLLED COMMERCIAL COPPER. Acta Metall Sin, 1990, 26(3): 126-130.
Abstract The texture change along the normal direction to rolling plane ofcross shear rolled commercial copper has been studied by means of the two-stepmethod for ODF calculation and computer simulation. The texture of cross shearrolling of copper is similar in primary components to that of conventional coldrolling, but the scattering degree and direction of the texture are different due to theresidual shear strain change in different position along the normal to rolling plane.It seems that no more effect of the shear strain upon the recrystallization texture.
1 朱泉.钢铁,1980;15:1 2 梁志德,徐家桢,王福.织构材料的三继取向分析术,沈阳:东北工学院出版社,1986:108 3 Taylor G I. J Inst Met. 1938; 62: 307 4 Houtte P V, Aernoudt E. Z Metallk. 1975; 66: 202 5 刘燕声,梁志德.科学通报,1989;6:471]
LIU Gang (School of Materials and Metallurgy; Northeastern University; Shenyang 110006; School of Chemical Science and Engineering; Liaoning University; Shenyang 110036)QI Kemin; WANG Fu; WANG Gang; LIANG Zhide (School of Materials and Metallurgy; Northeastern University; Shenyang 110006). THE INFLUENCE OF MISMATCH SPEED RATIO ON TEXTURE DEVELOPMENT IN CROSS SHEAR ROLLED 3% SILICON STEEL[J]. 金属学报, 1998, 34(4): 400-405.