| DRAWING PREDOMINANCE DIAGRAM OF M_1-M_2-x-y SYSTEM AND ITS APPLICATION |
| WANG Longzhang;HUANG Kexiong;LUO Rutie;YAO Yu;YE Dalu;CHEN Xinmin Central South University of Technology; Changsha Department of Chemistry;Central South University of Technology;Changsha 410083 |
|
Cite this article:
WANG Longzhang;HUANG Kexiong;LUO Rutie;YAO Yu;YE Dalu;CHEN Xinmin Central South University of Technology; Changsha Department of Chemistry;Central South University of Technology;Changsha 410083. DRAWING PREDOMINANCE DIAGRAM OF M_1-M_2-x-y SYSTEM AND ITS APPLICATION. Acta Metall Sin, 1990, 26(3): 113-118.
|
|
|
Abstract Discussions were made of the principle, method and computerizedprogram for drawing the predominance diagrams of the bi-metal co-existed systemM_1-M_2-x-y in which the multimetallic compounds may be produced by interactionbetween compounds of both metals. The formation of zinc ferrite and its stableregion have been analyzed through drawing Zn-Fe-S-O system predomincance dia-gram. The availability of the diagram is given the direction to roast the zinc sul-fide ore as well.
|
|
Received: 18 March 1990
|
1 Sohn Hongyong. Miner Sci Eng, 1979; 11 (3) : 24 2 Turkdogan E T. Physical Chemistry of High Temperature Technology, New York: Academic Press, 1980 3 王龙章,陈新民.中南矿冶学院学报,待发表 4 东北工学院有色重金属冶炼教研室等.锌冶金,北京:冶金工业出版社,1978:15+ |