Abstract The morphology of the retained austenite in the carburized case overthe 20CrNiMo steel and its transformation during fatigue crack propagation throughthe case were investigated by using X-ray and TEM analysis. In the carburizedcase, both film and block shared retained austenite were found. The fatigue crackis inclined to pass through the block shaped retained austenite and thereby stimu-lates its strain-induced martensitic transformation, due to the effect of the orienta-tion relationship between the surfaces. During the process of the fatigue fracture,most of the retained austenite on the crack path are transformed into the marten-site, and the untransformed amounts on the fracture are remained less than 6%. Thetransformation of retained austenite, which is restricted mainly within the plasticzone, occurs only in the time of the fracture, and is independent of external stressesand stress ratios and cyclic numbers. The volume expansion accompanided by itstransformation creates an additional residual displacement of about 0.44μm oncracked surfaces, which is relevent in the magnitude to the plasticity-induced residualdisplacement. The phase transformation induced fatigue crack closure is believed tobe an important factor affecting the fatigue crack behaviors in the high carbonlayer of the carburized case.
|
|
Received: 18 January 1990
|
1 Webster D. ASM Trans Q, 1968; 61: 816 2 Lou Bingzhe (楼秉哲), Averbach B L. Metall Trans, 1983; 14A: 1899 3 井晓天,楼秉哲,沈福三.陕西机械学院学报,1988;(4) :27 4 Gu Chenqing (谷臣清), Lou Bingzhe (楼秉哲), Jing Xiaotian (井晓天), Shen Fusan (沈福三). In: Krauss G ed. Heat Treatment and Surface Engineering, Proc of the 6th International Congress on Heat Treatment of Materials, Chicago: ASM International, 1988: 331 5 Brown W F, Strawley J E. ASTM STP410, 1966: 6 Jing Xiaotian(井晓天), Lou Bingzhe(楼秉哲), Shen Fusan(沈福三). In: Salamak et al., eds. Advance in Fracture Reseach. Vol 11. Huston: Pergamon Press, 1989: 1187--1194 7 徐祖耀.马氏体相变与马氏体,北京:科学出版社,1980 8 Naylor J P, Krahe P R. Metall Trans, 1975; 6A: 594 9 Lindborg U H, Averbach B L. Acta Metall. 1966; 14: 1583 10 田村今男,藤原茂,下冈贞正,成吉幸雄.日本金属学会志,1977;41:280 11 田中実.见:日本热处理技术协会编,热处理基础(Ⅱ),日刊工业新闻社.1970:161 12 Flcck N A. C?ED/C-MATS/TR, 104, Cambridge University, 1984_ |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|