Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (1): 46-52    DOI:
Current Issue | Archive | Adv Search |
SHORT FATIGUE CRACK BEHAVIOUR IN ISO-STRESS SPECIMENS
HONG Youshi;LU Yonghua;ZHENG Zhemin C. M. Cheng Institute of Mechanics; Academia Sinica; Beijing Institute of Mechanics;Academia Sinica;Beijing 100080
Cite this article: 

HONG Youshi;LU Yonghua;ZHENG Zhemin C. M. Cheng Institute of Mechanics; Academia Sinica; Beijing Institute of Mechanics;Academia Sinica;Beijing 100080. SHORT FATIGUE CRACK BEHAVIOUR IN ISO-STRESS SPECIMENS. Acta Metall Sin, 1990, 26(1): 46-52.

Download:  PDF(1853KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The fatigue tests were made on the specially designed specimens by avibration testing machine to investigate the initiation and propagation features ofshort fatigue cracks in a weld metal. The specimens were prepared of a kindof triangular shape in which the surface tensile stress is a constant. The resultsshow that the short fatigue cracks originate from the slip bands and initiate insidethe ferrite grains. The development of short fatigue cracks is marked by the grad-ual increase in crack density with fatigue cycles. The coalescence between shortcracks leads to crack propagation and the crack path is predominantly transgranular.
Key words:  iso-stress specimen      short fatigue crack      weld metal     
Received:  18 January 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I1/46

1 Gouda V K, Staehle R W. Br Corros J, 1980; 15: 111--117
2 Timoshenko S,Gere J 著,胡人礼译.材料力学,北京:科学出版社,1978:226--232
[1] Xiaodong LIN,Qunjia PENG,En-Hou HAN,Wei KE. Effect of Annealing on Microstructure of Thermally Aged 308L Stainless Steel Weld Metal[J]. 金属学报, 2019, 55(5): 555-565.
[2] Liming DONG,Li YANG,Jun DAI,Yu ZHANG,Xuelin WANG,Chengjia SHANG. Effect of Mn, Ni, Mo Contents on Microstructure Transition and Low Temperature Toughness of Weld Metal for K65 Hot Bending Pipe[J]. 金属学报, 2017, 53(6): 657-668.
[3] Fengyu SONG,Yanmei LI,Ping WANG,Fuxian ZHU. EFFECTS OF HEAT INPUT ON THE MICROSTRUC-TURE AND IMPACT TOUGHNESS OF WELD METAL PROCESSED BY A NEW FLUXNOVEL FLUX CORED WIRE WELD[J]. 金属学报, 2016, 52(7): 890-896.
[4] Xuelin WANG,Liming DONG,Weiwei YANG,Yu ZHANG,Xuemin WANG,Chengjia SHANG. EFFECT OF Mn, Ni, Mo PROPORTION ON MICRO-STRUCTURE AND MECHANICAL PROPERTIESOF WELD METAL OF K65 PIPELINE STEEL[J]. 金属学报, 2016, 52(6): 649-660.
[5] MO Wenlin, ZHANG Xu, LU Shanping, LI Dianzhong, LI Yiyi. EFFECT OF Nb CONTENT ON MICROSTRUCTURE, WELDING DEFECTS AND MECHANICAL PROPERTIES OF NiCrFe-7 WELD METAL[J]. 金属学报, 2015, 51(2): 230-238.
[6] YANG Chenggong, SHAN Jiguo, REN Jialie. PHASE TRANSFORMATION TEMPERATURE CONTROL OF WELD METAL OF LASER WELDED TiNi SHAPE MEMORY ALLOY JOINT[J]. 金属学报, 2013, 49(2): 199-206.
[7] YANG Chenggong, SHAN Jiguo, REN Jialie. STUDY ON SHAPE RECOVERY TEMPERATURE OF TiNi ALLOY LASER WELD JOINT[J]. 金属学报, 2012, 48(5): 513-518.
[8] PENG Yun WANG Aihua XIAO Hongjun TIAN Zhiling. EFFECT OF Cu ON MICROSTRUCTURE FORMING AND REFINING OF WELD METAL IN 690 MPa GRADE HSLA STEEL[J]. 金属学报, 2012, 48(11): 1281-1289.
[9] WEI Shitong LU Shanping HE Guangzhong ZHAO Xu LI Dianzhong LI Yiyi . EFFECTS OF HEAT TREATMENT ON THE MICROSTRUCTURE AND MECHANICAL PROPERTY OF WELD METAL WITH Nb ADDITION[J]. 金属学报, 2009, 45(9): 1063-1069.
[10] TAO Peng ZHANG Chi YANG Zhigang TAKEDA Hiroyuki. EVOLUTION OF SECOND PHASE IN 2.25Cr-1Mo-0.25V STEEL WELD METAL DURING HIGH TEMPERATURE TEMPERING[J]. 金属学报, 2009, 45(1): 51-57.
[11] XING Li; KE Liming (Nanchang Institute of Aero-Technology; Nanchang 330034). HYDROGEN INDUCED FRACTURE IN WELD METAL OF FERRITE-AUSTENITE DUPLEX STAINLESS STEEL[J]. 金属学报, 1997, 33(3): 297-303.
[12] CUI Zhenqi;XU Kewei; HU Naisai(National Laboratory for Mechanical Behaviour of Metallic Materials;xi'an Jiaotong University). MODEL AND EXPERIMENTS ON FATIGUE SHORT CRACK GROWTH IN RESIDUAL STRESS FIELD[J]. 金属学报, 1994, 30(2): 65-69.
[13] ZANG Qishan;LIU Kang Institute of Metal Research; Academia Sinica; Shenyang; KE Wei; ZHENG Yuli Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang. CORROSION FATIGUE CRACK GROWTH IN WELD METAL OF HOMEMADE OFFSHORE STRUCTURAL STEEL 36Z[J]. 金属学报, 1991, 27(5): 95-99.
[14] CHEN Zheng Northwestern Polytechnical University; Xi'an. THRESHOLD OF SHORT FATIGUE CRACK FOR 8090 Al-Li ALLOY[J]. 金属学报, 1990, 26(5): 62-65.
[15] PEI Hongxun;YANG Jingjun;KE Wei Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang. GROWTH OF SHORT CRACKS OF A537CL1 STEEL UNDER FATIGUE LOADING IN 3.5% NaCl SOLUTICN[J]. 金属学报, 1988, 24(6): 471-475.
No Suggested Reading articles found!