| A Zr-RICH LOW MELTING POINT PHASE IN Ni_3 Al WITH Zr |
| ZHANG Jishan;TANG Yajun;ZHANG Jinghua;ZHANG Zhiya;YU Yang;LI Ying'ao; HU Zhuangqi Institute of Metal Research; Academia Sinica; Shenyang ZHANG Jishan; Institute of Metal Rescarch; Academia Sinica; 110015 Shenyong |
|
Cite this article:
ZHANG Jishan;TANG Yajun;ZHANG Jinghua;ZHANG Zhiya;YU Yang;LI Ying'ao; HU Zhuangqi Institute of Metal Research; Academia Sinica; Shenyang ZHANG Jishan; Institute of Metal Rescarch; Academia Sinica; 110015 Shenyong. A Zr-RICH LOW MELTING POINT PHASE IN Ni_3 Al WITH Zr. Acta Metall Sin, 1989, 25(5): 76-78.
|
|
|
Abstract A Zr-rich phase, Ni_5Zr, with low melting point has been found in a Ni_3Alalloy doped with Zr (1.2at.-%). It will cause the incipient melt of the alloy after homogeniz-ing at 1300℃. This makes it difficult to homogenize the coarse casting structures completelyand limits further impovement of the properties.
|
|
Received: 18 May 1989
|
1 马淑琴,郑运荣,蔡玉林.金属学报,1981;17:522 2 Murata Y, Yukawa N. Scr Metall, 1986; 20: 693 3 Liu C T, Sikka V K. J Met, 1986; 38: 19 4 Hsu S E, Hsu N N, Tong C H, Ma C Y, Lee S Y. High Temberature Ordered Intermetallic Alloys Ⅱ, Boston: Materials Research Society, 1986: 507 5 Kirkpatrick M E, Larsen W L. Trans ASM, 1961; 54: 580 6 Zhang Jishan, Zhang Zhiya, Tang Yajun, Zhang Jinghua, Yu Yang, Li Yingao, Ding Dongsheng, Hu Zhuangqi. High Temperature Ordered Intermetallic Alloys Ⅲ, Boston: Materials Research Society, 1988 (in Press) |
| No Suggested Reading articles found! |
|
|