NEUTRON DIFFRACTION STUDY OF Y_2 (Fe_(0.95) Al_(0.05))_(14)B
YANG Jilian;ZHANG Baisheng;JIN Lan;DING Yongfan;YE Chuntang;YANG Yingchang;SUN Hong;KONG Linshu Institute of Atomic Energy; Beijing Peking University; Beijing YANG lilian; P. O. Box 275; sub 80; 102413 Beijing
Cite this article: 

YANG Jilian;ZHANG Baisheng;JIN Lan;DING Yongfan;YE Chuntang;YANG Yingchang;SUN Hong;KONG Linshu Institute of Atomic Energy; Beijing Peking University; Beijing YANG lilian; P. O. Box 275; sub 80; 102413 Beijing. NEUTRON DIFFRACTION STUDY OF Y_2 (Fe_(0.95) Al_(0.05))_(14)B. Acta Metall Sin, 1989, 25(5): 152-154.

Download:  PDF(226KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The structure of Y_2 (Fe_(0.95)Al_(0.05))_(14) B is tetragonal Nd_2Fe_(14)B type, its space groupis P42/mnm; Al atoms enter into the Crystal structure and occupy the sites 4c and 8j_2 prefer-entially. The relationship between magnetic properties and the occupancies is discussed prima-rily.
Key words:  neutron diffraction      Y_2(Fe_(0.95)Al_(0.05))_(14)B     
Received:  18 May 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I5/152

1 Lin Chin (林勤), Lan Jian (兰健), Xu Xiaofeng(徐晓凤). J Appl Phys, 1987; 61: 3457
2 Yang Yingchang (杨应昌), Tharp D E, Long G J, Pringle O A, James W J. J Appl Phys, 1987; 61: 4343
3 Ramesh R, Chen J K, Thomas G, Ma B M. J Appl Phys, 1988; 63: 3334
4 Rietveld H M. J Appl Crystallogr, 1974; 7: 96
5 杨继廉,丁永凡,张百生,金兰,周蕙明,叶春堂,杨应昌,邢峰,孔麟书.物理学报,1988;37:1906
6 Givord D, Li H S, Moreau Y N. Solid State Commun, 1984; 50: 49
[1] LI Shilei, LI Yang, WANG Youkang, WANG Shengjie, HE Lunhua, SUN Guang'ai, XIAO Tiqiao, WANG Yandong. Multiscale Residual Stress Evaluation of Engineering Materials/Components Based on Neutron and Synchrotron Radiation Technology[J]. 金属学报, 2023, 59(8): 1001-1014.
[2] GAO Yubi, DING Yutian, LI Haifeng, DONG Hongbiao, ZHANG Ruiyao, LI Jun, LUO Quanshun. Effect of Deformation Rate on the Elastic-Plastic Deformation Behavior of GH3625 Alloy[J]. 金属学报, 2022, 58(5): 695-708.
[3] SHI Zengmin, LIANG Jingyu, LI Jian, WANG Maoqiu, FANG Zifan. In Situ Analysis of Plastic Deformation of Lath Martensite During Tensile Process[J]. 金属学报, 2021, 57(5): 595-604.
[4] LI Yizhuang,HUANG Mingxin. A Method to Calculate the Dislocation Density of a TWIP Steel Based on Neutron Diffraction and Synchrotron X-Ray Diffraction[J]. 金属学报, 2020, 56(4): 487-493.
[5] BI Zhongnan,QIN Hailong,DONG Zhiguo,WANG Xiangping,WANG Ming,LIU Yongquan,DU Jinhui,ZHANG Ji. Residual Stress Evolution and Its Mechanism During the Manufacture of Superalloy Disk Forgings[J]. 金属学报, 2019, 55(9): 1160-1174.
[6] Hailong QIN,Ruiyao ZHANG,Zhongnan BI,Lee Tung Lik,Hongbiao DONG,Jinhui DU,Ji ZHANG. Study on the Evolution of Residual Stress During Ageing Treatment in a GH4169 Alloy Disk[J]. 金属学报, 2019, 55(8): 997-1007.
[7] Zukun YANG, Changsheng ZHANG, Beibei PANG, Yanyan HONG, Fangjie MO, Zhao LIU, Guang'ai SUN. Effect of Initial Microstructures on the Macroscopic Mechanical Properties of Polycrystalline Beryllium[J]. 金属学报, 2018, 54(8): 1150-1156.
[8] Meijuan LI,Xiaolong LIU,Yuntao LIU,Mingyi ZHENG,Chen WANG,Dongfeng CHEN. TEXTURE EVOLUTION AND MECHANICAL PROPER-TIES OF Mg/Al MULTILAYERED COMPOSITE SHEETSPROCESSED BY ACCUMULATIVE ROLL BONDING[J]. 金属学报, 2016, 52(4): 463-472.
[9] Pingguang XU,Jiang YIN,Shuyan ZHANG. TENSILE DEFORMATION BEHAVIOR OF HYDROGEN CHARGED ULTRAHIGH STRENGTH STEEL STUDIED BY IN SITU NEUTRON DIFFRACTION[J]. 金属学报, 2015, 51(11): 1297-1305.
[10] ZHANG Meng, LIU Danmin, LIU Cuixiu, HUANG Qingzhen, WANG Shaobo, ZHANG Hu, YUE Ming. RESEARCH OF THE RELATIONSHIP BETWEEN PHASE TRANSITION PROCESS AND MAGNETIC PROPERTIES IN MAGNETIC REFRIGERATION MATERIAL Mn1.2Fe0.8P0.76Ge0.24[J]. 金属学报, 2013, 49(7): 783-788.
[11] JIANG Wenchun WOO Wanchuck WANG Bingying TU Shan–Tung . A STUDY OF RESIDUAL STRESS IN THE REPAIR WELD OF STAINLESS STEEL CLAD PLATE BY NEUTRON DIFFRACTION MEASUREMENT AND FINITE ELEMENT METHOD[J]. 金属学报, 2012, 48(12): 1525-1529.
[12] WU Erdong GUO Xiumei SUN Kai. NEUTRON DIFFRACTION STUDY OF DEUTERIUM OCCUPANCY OF DEUTERIDE OF LAVES PHASE ALLOY Ti0.68Zr0.32MnCrD3.0[J]. 金属学报, 2009, 45(5): 513-518.
[13] XU Pingguang; TOMOTA Yo. Progress in Materials Characterization Technique Based on in Situ Neutron Diffraction[J]. 金属学报, 2006, 42(7): 681-688 .
[14] PAN Hongge; DU Honglin; CHEN Changpin; HAN Xiufeng; YANG Fuming (Department of Materials Science and Engineering; Zhejiang University; Hangzhou 310027)(State Key Laboratory for Magnetism; Institute of Physics; The Chinese Academy of Sciences; Beijing 100080)(Institute of Chinese Atomic Energy; Beijing 102413). STRUCTURAL CHARACTERIZATION OF THE Y_3(Fe, Mo)_(29) INTERMETALLIC COMPOUND[J]. 金属学报, 1998, 34(5): 473-482.
[15] YANG Wangyue; SHENG Lizhen;SUN Zuqing; HUANG Yuanding; MAO Weimin (University of Science and Technology Beijing; Beijing 100083); ZHANG Baisheng; YE Chuntang (China Institute of Atomic Energy; Beijing 102413)(Manuscript received 1995-11-10; in revised form 1996-04-05). NEUTRON DIFFRACTION STUDY ON SITE OCCUPATION OF SUBSTITUTIONAL ELEMENTS AT SUBLATTICE IN Fe_3Al INTERMETALLICS[J]. 金属学报, 1996, 32(8): 799-804.
No Suggested Reading articles found!