Please wait a minute...
Acta Metall Sin  1989, Vol. 25 Issue (5): 142-143    DOI:
Current Issue | Archive | Adv Search |
410℃ ISOTHERMAL SECTION OF Al-Cu-Sb TERNARY SYSTEM PHASE DIAGRAM
CHEN Rongzhen;ZHANG Hanxing;ZHENG Jianxuan;HE Hanping Guangxi University; Nanning Guangxi Institute of Non-Ferrous Metals Geology; Nanning CHEN Rongzhen;Department of Physics;Guangxi University; Nanning;530009 Guangxi
Cite this article: 

CHEN Rongzhen;ZHANG Hanxing;ZHENG Jianxuan;HE Hanping Guangxi University; Nanning Guangxi Institute of Non-Ferrous Metals Geology; Nanning CHEN Rongzhen;Department of Physics;Guangxi University; Nanning;530009 Guangxi. 410℃ ISOTHERMAL SECTION OF Al-Cu-Sb TERNARY SYSTEM PHASE DIAGRAM. Acta Metall Sin, 1989, 25(5): 142-143.

Download:  PDF(157KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The 410℃ isothermal section of phase diagram of Al-Cu-Sb ternary system hasbeen determined by X-ray powder diffraction method and electron probe. 12 single-phase re-gions, 21 two-phase regions and 10 three-phase regions are found to construct the 410℃ iso-thermal section.
Key words:  Al-Cu-Sb ternary system      phase diagram      isothermal section     
Received:  18 May 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I5/142

1 Smithlls C J. Metals Reference Book, 5th ed., London: Butterworth, 1976: 400, 417, 591
2 Hansen M. Constitution of Binary Alloys, London: McGraw-Hill, 1958: 624, 84
3 Elliott R P. Constitution of Binary Alloys, 1st Suppl., New York: McGraw-Hill 1965: 383--384
4 Donnay J D H, Ondik H M. Crystal Data, Determinative Tables, Vol. Ⅱ: Inorganic Compounds. 3d ed., USA NSRDS & JCPDS, 1973: C-230, H-131, T-52, C-151, H-8. T-112!
[1] GAO Xiang, ZHANG Guikai, XIANG Xin, LUO Lizhu, WANG Xiaolin. Effects of Alloying Elements on the Adsorption of Oxygen on V(110) Surfaces: A First-Principles Study[J]. 金属学报, 2020, 56(6): 919-928.
[2] ZHANG Weibin SHA Chunsheng DU Yong WEN Guanghua XIE Wen WANG Shequan. COMPUTER SIMULATIONS AND VERIFICATION OF GRADIENT ZONE FORMATION IN CEMENTED CARBIDES[J]. 金属学报, 2011, 47(10): 1307-1314.
[3] ZHANG Huawei; LI Yanxiang; LIU Yuan. Study of Metal--Hydrogen Binary Phase Diagram in Gasar Process[J]. 金属学报, 2005, 41(1): 55-.
[4] ZHANG Jian(Metallurgical Engineering School; University of Science and Technology Beijing; Beijing 100083). CONSISTENCY(OR SIMILARITY) OF THERMODYNAMIC PROPERTIES OF METALLURGICAL MELTS WITH THEIR PHASE DIAGRAMS[J]. 金属学报, 1998, 34(7): 742-752.
[5] Zhang Jian (Institute of Metallurgy; University of Science and Technology Beijing; Beijing 100083). CLASSIFICATION OF THERMODYNAMIC PROPERTIES OF BINARY METALLIC MELTS ACCORDING TO THEIR PHASE DIAGRAMS[J]. 金属学报, 1998, 34(1): 75-85.
[6] ZHOU Hong; WANG Jinguo; JIA Shusheng (Jilin University of Technology; Chanerhun 130025) OGIKeisaku(Kyushu Universily; Japan) (Manuscript received 1996-03-22; in revised form 1997-04- 13). SOLIDIFIED MICROSTRUCTURES AND PHASES OF HIGH SPEED STEELS CONTA1NING DIFFERENT V AND C CONTENT[J]. 金属学报, 1997, 33(8): 838-843.
[7] FANG Jianhui; TANG Yun; LI Yu; YAN Licheng; CHEN Nianyi (Shanghai University;Shanghai 201800); WANG Jiyang (Shandong University; Jinan 250012)(Manuscript received 1996-04-08; in revised form 1996-09-10). KPO_3-M0O_3 PHASE DIAGRAM[J]. 金属学报, 1997, 33(4): 395-397.
[8] ZHOU Guozhi(Kuo-Chih Chou) (University of Science and Technology Beijing;Beiing 100083). NEW GENERATION SOLUTION GEOMETRICAL MODEL AND ITS FURTHER DEVELOPMENT[J]. 金属学报, 1997, 33(2): 126-132.
[9] DING Jinjun;ZHAO Gang;HAO Shiming (Northeastern University; Shenyang 110006). PHASE EQUILIBRIUM RELATIONSHIPS AND INTERDIFFUSION COEFFICIENTS OF β,α ANDγIN THE Ti-Al BINARY SYSTEM[J]. 金属学报, 1997, 33(10): 1105-1109.
[10] YUAN Wenxia; MA Shulan; QIAO Hin; ZHUANG Weidong; XING Xianran;QIAO Zhiyu (University of Science and Technology Beijing; Beijing 100083)(General Institute for Non-Ferrous Metals; Beijing 100088)(Manuscript received 1995-04-28; in revised form 1995-11-05). A STUDY ON THE YCl_3-AECl_2(AE=Mg, Ca, Sr, Ba)BINARY PHASE DIAGRAMS[J]. 金属学报, 1996, 32(2): 139-143.
[11] HAO Shiming; ZENG Ninghua (Northeastern University; Shenyang 110006)(Manuscript received 1994-11-16). ISOTHERMAL SECTION OF PHASE DIAGRAM IN Ti-Al-Cr TERNARY SYSTEM AT 1000℃[J]. 金属学报, 1995, 31(16): 152-158.
[12] YAN Licheng;FANG Jianhui;XU Jingyan;YANG Jinxiu(Shanghai University of Science and Technology). PHASE DIAGRAM OF KF-LiCl-CaCl_2 SYSTEM[J]. 金属学报, 1994, 30(19): 301-303.
[13] WAN Jinglong(Anhui Institute of Technology; Hefei); BI Qinghua(Shanghai University of Science and Technology). Gd-CoAl VERTICAL SECTION OF Gd-Co-Al PHASE DIAGRAM[J]. 金属学报, 1994, 30(17): 204-207.
[14] XU Qian;YU Yaxin;QIU Zhuxian(Northeastern University;Shenyang)(Manuscript received 25 June;1993). THERMODYNAMIC PROPERTIES AND PHASE DIAGRAMS OF Li-CaF_2,NaF-CaF_2 AND KF-CaF_2[J]. 金属学报, 1994, 30(16): 150-155.
[15] SHEN Jianyun(General Research Institute for Non-Ferrous Metals;Beijing);CHATILLON C(Laboratoire de Thermodynamique et Physico-chimie Metallurgiques;Fracne)(Manuscript received 16 June;1993). THERMODYNAMICS OF Ga-In-As SYSTEM UNDER LATTICE DEFORMATION[J]. 金属学报, 1994, 30(16): 145-149.
No Suggested Reading articles found!