LOW ENERGY DISLOCATION STRUCTURES DUE TO FATIGUE SOFTENING
CHAI Huifen;WANG Liqin;C. LAIRD Xi'an Jiaotong University University of Pennsylvania; U. S. A
Cite this article: 

CHAI Huifen;WANG Liqin;C. LAIRD Xi'an Jiaotong University University of Pennsylvania; U. S. A. LOW ENERGY DISLOCATION STRUCTURES DUE TO FATIGUE SOFTENING. Acta Metall Sin, 1989, 25(3): 45-50.

Download:  PDF(1944KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The evolution of dislocation structures in 6% prestrained steel 1018during fatigue has been studied by TEM. The dislocations are quite movable, theloose cells quickly change to "checkboard" structures, in which the main cell wallslie about{100}. Then, the low energy dislocation structures-dipolar walls and laby-rinth structures are evolved. The characteristic of labyrinth and the orientation of di-polar walls are quite similar to f. c. c. crystal, it indicates the energy state of systemand the moving ability of dislocations are important factors affecting softening pro-cess, rather than the slip geometric characters of dislocations and details of disloca-tions. The decreasing in misorientation between adjoining cells and internal stressare discussed.
Key words:  steel 1018      fatigue softening      dislocation configuration     
Received:  18 March 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I3/45

1 Ramaswami B, Lau T W F. Mater Sci Eng, 1980; 46: 221
2 Kuhlmann-Wilsdorf D. Metall Trans, 1985; 16A: 2091
3 Chai Huifen (柴惠芬), Laird C. Mater Sci Eng, 1987; 93: 159
4 Foxall R A, Duesbery M S, Hitsch P B. Can J Phys, 1967; 45: 607
5 Kuhlmann-Wilsdorf D. In: Thompson A W ed, Workhardening in Tension and Fatigue. AIME, 1977: 1
6 Ackermann F, Kubin L P, Lepinoux J, Mughrabi H. Acta Metall, 1984; 32: 715
7 Charsley P. Mater Sci Eng, 1981; 47: 181
8 Jin N Y, Winter A T. Acta Metall, 1984; 32: 1173
9 Dickson J I, Boutin J, Lesperance G. Acta Metall, 1986; 34: 150
[1] Kan SONG,Kai YU,Xin LIN,Jing CHEN,Haiou YANG,Weidong HUANG. MICROSTRUCTURE AND MECHANICAL PROPERTIES OF HEAT TREATMENT LASER SOLID FORMING SUPERALLOY INCONEL 718[J]. 金属学报, 2015, 51(8): 935-942.
[2] PAN Kunming, ZHANG Laiqi, WANG Meng, LIN Junpin. BRITTLE-TO-DUCTILE TRANSITION FOR T2 IN THE Mo-Si-B SYSTEM[J]. 金属学报, 2013, 49(11): 1392-1398.
[3] DING Zhi ZHANG Jun WANG Changshuai SU Haijun LIU Lin FU Hengzhi. DISLOCATION CONFIGURATION IN DZ125 Ni-BASED SUPERALLOY AFTER HIGH TEMPERATURE STRESS RUPTURE[J]. 金属学报, 2011, 47(1): 47-52.
[4] GUO Xiaolong; SHEN Yongfeng; LU Lei; LI Shouxin. EFFECTS OF TWINS ON THE FATIGUE BEHAVIOR OFPOLYCRYSTALLINE COPPER[J]. 金属学报, 2004, 40(12): 1281-1284 .
[5] LIU Guodong; ZHU Zhengang; WANG Jing (Institute of Solid State Physics; ChineseAcademy of Sciences; Hefei 230031)(Manuscript received 1995-08-22; in revised form 1995-12-14). BEHAVIOUR OF AI-SINGLE CRYSTAL DURING EARLY STAGE OF PUSH-PULL FATIGUE[J]. 金属学报, 1996, 32(5): 510-515.
[6] CHAI Huifen;RUAN Zheng;FAN Qunchen Xi'an Jiaotong University associate professor; Department of Materials; Xi'an Jiaotong University; Xi'an 710049. EFFECT OF SLIP MODE ON CYCLIC BEHAVIOUR OF PRESTRAINED MATERIALS[J]. 金属学报, 1993, 29(4): 7-12.
[7] FAN Quncheng;CHAI Huifen;TONG Mingxin Xi'an Jiaotong University. FATIGUE SOFTENING BEHAVIOUR AND ITS THRESHOLD OF COLD STRAINED POLYCRYSTALLINE Cu[J]. 金属学报, 1990, 26(5): 56-61.
[8] YAO Kefu;TANG Naiyong;CHEN Nanping Tsinghua University. IN SITU OBSERVATION OF CRACK TIP DEFORMATION IN A DUPLEX STAINLESS STEEL[J]. 金属学报, 1989, 25(3): 57-62.
[9] JIN Nengyun Shanghai Jiaotong University. CYCLIC DEFORMATION OF FCC CRYSTALS AND ITS DISLOCATION INTERACTION MODEL Ⅰ. CYCLIC DEFORMATION OF COPPER SINGIE CRYSTALS[J]. 金属学报, 1988, 24(5): 299-310.
No Suggested Reading articles found!