| HOMOGENIZATION TREATMENT OF ALLOY GH169 |
| NING Xiuzhen;ZHANG Tianxiang;TONG Yingjie;ZHU Yaoxiao Institute of Metal Research; Academia Sinica; Shenyang |
|
Cite this article:
NING Xiuzhen;ZHANG Tianxiang;TONG Yingjie;ZHU Yaoxiao Institute of Metal Research; Academia Sinica; Shenyang. HOMOGENIZATION TREATMENT OF ALLOY GH169. Acta Metall Sin, 1989, 25(3): 40-44.
|
|
|
Abstract A new point of view on the homogenization treatment has been pro-posed. It is supposed that a little liguid in the alloy may promote the homogenizationprocess in some aspects and reduce the time for eliminating the laves-phase in alloyGH169. The microprocess of the elimination of Laves-phase in the case of a littleliguid existing in the alloy has also been described.
|
|
Received: 18 March 1989
|