| EFFECT OF STRUCTURE IN WHITE IRON ON GRAPHITIZATION OF MALLEABLE CAST IRON |
| ZHANG Xijun;CHEN Yongmin Kunming Institute of Technology |
|
Cite this article:
ZHANG Xijun;CHEN Yongmin Kunming Institute of Technology. EFFECT OF STRUCTURE IN WHITE IRON ON GRAPHITIZATION OF MALLEABLE CAST IRON. Acta Metall Sin, 1989, 25(2): 128-132.
|
|
|
Abstract The structure of white iron treated with Si-Bi-Al complex inoculanthas been observed by means of SEM and TEM. The results show that, in compari-son with the samples treated with ordinary inoculants, disorder, overlapping andinflexion of the pearlitic lamella appear, besides, the dislocation density increasesapparently. The graphitization can be quickly realized at the temperature lower thanthat of austenitic transition (720℃)
|
|
Received: 18 February 1989
|
1 Roy P L, Chakrabarti A K, Banerjee P. 49th Int Foundry Congress, Chicago, 1982: 9 2 郎本智,陈永民,何民奕,吴勇生.铸造,1988;(2) :17 3 张希俊,何芸.第4届中国体视学及图像分析学术会议论文集,昆明,1987 4 雷永泉,铸造过程物理化学,北京:新时代出版社,1982:55 5 Рулцов Н Н,苑吉春,肖柯则译.可锻铸铁,北京:机械工业出版社,1960:13 6 Parent-Simonin S, Moreaux C. Founderie, 1979; 34 (385) : 3 7 Рулцов Н Н ,苑吉春,肖柯则译。可锻铸铁,北京:机械工业出版社,1960:54 8 Hillert M,赖和怡,刘国勋译.合金扩散及热力学,北京:冶金工业出版社,1984:79Y |
| No Suggested Reading articles found! |
|
|