| CHARACTERISTICS OF INTERNAL FRICTION AND MODULUS ASSOCIATED WITH NON-EQUILIBRIUM DIFFUSION-TYPE PHASE TRANSFORMATION IN EUTECTOID Al-Zn ALLOY |
| ZHU Xianfang;ZHANG Lide Institute of Solid State Physics; Academia Sinica; Hefei |
|
Cite this article:
ZHU Xianfang;ZHANG Lide Institute of Solid State Physics; Academia Sinica; Hefei. CHARACTERISTICS OF INTERNAL FRICTION AND MODULUS ASSOCIATED WITH NON-EQUILIBRIUM DIFFUSION-TYPE PHASE TRANSFORMATION IN EUTECTOID Al-Zn ALLOY. Acta Metall Sin, 1989, 25(2): 10-14.
|
|
|
Abstract The characteristics of the low freqency internal friction and moduluseffect associated with the non-equilibrium spinodal pretransformation and the follow-ing discontinuous transformation was investigated in an as-quenched eutectoid Al-Zn alloy. It was observed that the loss of the stability in the Iattice, which corre-sponded to the large-amplitude long-wavelength static concentration wave in thenon-equilibrium spinodal pretransformation, did not induce any effect of localizedsoft modulus. Although there are two aging internal friction peaks in phase transfor-mation which correspond to the appearance and disappearance of the coherency andthe maximum of the interface area in the discontinuous transformation, respectively,the effect of localized soft modulus did not take place yet.
|
|
Received: 18 February 1989
|
1 朱贤方,文亦汀,谢存毅.第二届全国马氏体相变会议文集,(第二册),大连工学院,中国金属学会,1987 2 Defoutaine D. Metall Trans, 1981; 12A: 559 3 Clapp P C. Metall Trans, 1981; 12A: 589 4 Ju C P, Fournelle R A. Acta Metall, 1985; 33: 71 5 Zhu Y H, Murphy S. Chin J Met Sci Technol, 1986; 2: 105 6 Shoeck G. Phys Status Solidi, 1969; 32: 651 7 刘国勋主编,金属学原理,冶金工业出版社,1980:391 8 冯端.金属物理学,(第一卷),科学出版社,1987:469 9 Clapp P C. Phys Status Solidi, (b) 1973; 57: 561 10 杨照金,邹一峰,张志方,王业宁.金属学报.1982;18:21 11 加藤光治,河合栄一郎,六碕贤亮,宫川松男.日本金属学会志,1974;38:539 |