KINETICS OF STRAIN-INDUCED PRECIPITATION OF (Nb,V) CARBONITRIDE IN A MICROALLOYED STEEL
XU Wenchong;SUN Fuyu;ZHAO Peixiang Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing
Cite this article: 

XU Wenchong;SUN Fuyu;ZHAO Peixiang Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing. KINETICS OF STRAIN-INDUCED PRECIPITATION OF (Nb,V) CARBONITRIDE IN A MICROALLOYED STEEL. Acta Metall Sin, 1988, 24(5): 331-335.

Download:  PDF(446KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The kinetics of the isothermal precipitation of (Nb, V) CN in Nb-Valloys has been investigated by using the Formastor-press simalator and the extrac-tion replica method. Under four deformation amount (0%, 10%, 30%, 50%) and threetemperatures (1100℃, 1000℃, 850℃), four types of kinetic curve were found.
Key words:  kinetics of precipitation      isothermal      particle size     
Received:  18 May 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I5/331

1 Wagner C. Z Elektrochem, 1961; 65: 581
2 Lifshitz I M, Slyozov V V, J Phys Chem Solids, 1961; 19: 35
3 Ardell A J. Acta Metall, 1972; 20: 601
4 Kreye H. Z Metallk, 1970; 61: 108
5 Sauthoff G, Kahlweit M. Acta Metall, 1969; 17: 1501
6 Bjorklund S, Donaghey L F, Hillert M. Acta Metall, 1972; 20: 867
7 Myeong Yong Wey, Taketo Sakuma. Taiji Nishizawa, Trans Jpn Inst Met, 1981; 22: 733
8 Weiss I, Jonas J J. Metall Trans, 1980; 11A: 403
9 Chandra T, Weiss I, Jonas J J. Met Sci, 1982; 16: 97
10 徐温崇,马翔,电子显微学报,1985;4(2) :67
11 徐温崇,马翔,孙福玉.钢铁,1985;20(3) :34
[1] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[2] ZHANG Qiliang, WANG Yuchao, LI Guangda, LI Xianjun, HUANG Yi, XU Yunze. Erosion-Corrosion Performance of EH36 Steel Under Sand Impacts of Different Particle Sizes[J]. 金属学报, 2023, 59(7): 893-904.
[3] WANG Meng, YANG Yongqiang, Trofimov Vyacheslav, SONG Changhui, ZHOU Hanxiang, WANG Di. Effects of Particle Size on Processability of AlSi10Mg Alloy Manufactured by Selective Laser Melting[J]. 金属学报, 2023, 59(1): 147-156.
[4] GUO Lu, ZHU Qianke, CHEN Zhe, ZHANG Kewei, JIANG Yong. Non-Isothermal Crystallization Kinetics of Fe76Ga5Ge5B6P7Cu1 Alloy[J]. 金属学报, 2022, 58(6): 799-806.
[5] YUAN Bo, GUO Mingxing, HAN Shaojie, ZHANG Jishan, ZHUANG Linzhong. Effect of 3%Zn Addition on the Non-Isothermal Precipitation Behaviors of Al-Mg-Si-Cu Alloys[J]. 金属学报, 2022, 58(3): 345-354.
[6] ZHOU Hongyu, RAN Minrui, LI Yaqiang, ZHANG Weidong, LIU Junyou, ZHENG Wenyue. Effect of Diamond Particle Size on the Thermal Properties of Diamond/Al Composites for Packaging Substrate[J]. 金属学报, 2021, 57(7): 937-947.
[7] DAI Jincai, MIN Xiaohua, ZHOU Kesong, YAO Kai, WANG Weiqiang. Coupling Effect of Pre-Strain Combined with Isothermal Ageing on Mechanical Properties in a Multilayered Ti-10Mo-1Fe/3Fe Alloy[J]. 金属学报, 2021, 57(6): 767-779.
[8] LIU Guanxi, HUANG Guanghong, LUO Xuekun, SHEN Zaoyu, HE Limin, LI Jianping, MU Rende. The Influence of Surface Shot Peening on the Isothermal Oxidation Behavior of NiCrAlYSi Coating[J]. 金属学报, 2021, 57(5): 684-692.
[9] LI Jichen, FENG Di, XIA Weisheng, LIN Gaoyong, ZHANG Xinming, REN Minwen. Effect of Non-Isothermal Ageing on Microstructure and Properties of 7B50 Aluminum Alloy[J]. 金属学报, 2020, 56(9): 1255-1264.
[10] ZHU Liang, GUO Mingxing, YUAN Bo, ZHUANG Linzhong, ZHANG Jishan. Effect of Ageing Routes on Precipitation Behaviors of Al-0.7Mg-0.5Si-0.2Cu-0.5Zn Alloy[J]. 金属学报, 2020, 56(7): 997-1006.
[11] LI Jichen, FENG Di, XIA Weisheng, GUO Weimin, WANG Guoying. The Non-Isothermal Double Ageing Behaviour of 7055 Aluminum Alloy[J]. 金属学报, 2020, 56(11): 1495-1506.
[12] Xiaohua MIN, Li XIANG, Mingjia LI, Kai YAO, Satoshi EMURA, Congqian CHENG, Koichi TSUCHIYA. Effect of {332}<113> Twins Combined with Isothermal ω-Phase on Mechanical Properties in Ti-15Mo Alloy with Different Oxygen Contents[J]. 金属学报, 2018, 54(9): 1262-1272.
[13] Di FENG, Xinming ZHANG, Hongmei CHEN, Yunxue JIN, Guoying WANG. Effect of Non-Isothermal Retrogression and Re-Ageing on Microstructure and Properties of Al-8Zn-2Mg-2Cu Alloy Thick Plate[J]. 金属学报, 2018, 54(1): 100-108.
[14] LIU Quan, YANG Yingfei, BAO Zebin, ZHU Shenglong, WANG Fuhui. OXIDATION PROPERTY AND FAILURE MECHANISM OF A SINGLE PHASE PtAl2 COATING[J]. 金属学报, 2014, 50(9): 1102-1108.
[15] LIU Xiaobo, ZHAO Yuguang. MICROSTRUCTURE EVOLUTION AND WEAR RESISTANCE OF IN SITU Mg2Si/Al COMPOSITES UNDER DIFFERENT PREPARATION CONDITIONS[J]. 金属学报, 2014, 50(6): 753-761.
No Suggested Reading articles found!