Please wait a minute...
Acta Metall Sin  1988, Vol. 24 Issue (5): 311-316    DOI:
Current Issue | Archive | Adv Search |
CYCLIC DEFORMATION OF FCC CRYSTALS AND ITS DISLOCATION INTERACTION MODEL Ⅱ. DISLOCATION INTERACTION MODEL OF CYCLIC DEFORMATION
JIN Nengyun Shanghai Jiaotong University
Cite this article: 

JIN Nengyun Shanghai Jiaotong University. CYCLIC DEFORMATION OF FCC CRYSTALS AND ITS DISLOCATION INTERACTION MODEL Ⅱ. DISLOCATION INTERACTION MODEL OF CYCLIC DEFORMATION. Acta Metall Sin, 1988, 24(5): 311-316.

Download:  PDF(561KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A dislocation interaction model has been proposed for cyclic deforma-tion. According to this model, cyclic stress-strain responses and dislocation structuresof a crystal are associated with the modes and intensities of dislocation interac-tions between slip systems active in the crystal; and, hence, may be predicted bythe location of its axis in the crystallographic triangle. This model has successfullyexplained the different behaviouls of double-slip crystals and multi-slip behavioursof some crystals with orientations usually considered as singleslip ones.
Key words:  face centered cubic crystal      dislocation interaction      model      multi-slip      cyclic deformation     
Received:  18 May 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I5/311

1 Jin N Y. (金能韫) Ph. D. Thesis, Cambridge University, U. K., 1983
2 Jin N Y (金能韫), Winter A T. Acta Metall, 1984; 32: 989
3 Hirth J P, Lothe J. Theory of Dislocations, 2nd ed., Wiley, Interscience, 1982
4 Jin N Y (金能韫). 中日金属物理讨论会, 北京, 1984年
5 Cheng A S, Laird C. Mater Sci Eng, 1981; 51: 111
6 Ackermann F, Kubin L P, Lepinoux J, Mughrabi H. Acta Metall, 1984; 32: 715
7 Lepisto T, Kuokkala V-T, Kettunen P. Scr Metall, 1984; 18: 245
8 Tabata T, Fujita H, Hiraoka M, Onishi K. Philos Mag, 1983; 47: 841
9 Wang R (王仁卉), Mughrabi H, McGovern S, Rapp M. Mater Sci Eng, 1984; 65: 219
10 Jin N Y (金能韫). Certificate of Post-Graduate Study Thesis, Cambridge University, U. K., 1980
11 Jin N Y (金能韫), Winter A T. In: Fong J. T, Wei R P eds., Fundamental Questions and Critical Experiments in Fatigue, Vol. 1, ASTM Int Symp on Fatigue, Dallas, 1984m
[1] XU Yongsheng, ZHANG Weigang, XU Lingchao, DAN Wenjiao. Simulation of Deformation Coordination and Hardening Behavior in Ferrite-Ferrite Grain Boundary[J]. 金属学报, 2023, 59(8): 1042-1050.
[2] ZHANG Lu, YU Zhiwei, ZHANG Leicheng, JIANG Rong, SONG Yingdong. Thermo-Mechanical Fatigue Cycle Damage Mechanism and Numerical Simulation of GH4169 Superalloy[J]. 金属学报, 2023, 59(7): 871-883.
[3] WANG Hanyu, LI Cai, ZHAO Can, ZENG Tao, WANG Zumin, HUANG Yuan. Direct Alloying of Immiscible Tungsten and Copper Based on Nano Active Structure and Its Thermodynamic Mechanism[J]. 金属学报, 2023, 59(5): 679-692.
[4] ZHANG Zhidong. Exact Solution of Ferromagnetic Three-Dimensional (3D) Ising Model and Spontaneous Emerge of Time[J]. 金属学报, 2023, 59(4): 489-501.
[5] ZHU Zhihao, CHEN Zhipeng, LIU Tianyu, ZHANG Shuang, DONG Chuang, WANG Qing. Microstructure and Mechanical Properties of As-Cast Ti-Al-V Alloys with Different Proportion of α / β Clusters[J]. 金属学报, 2023, 59(12): 1581-1589.
[6] JU Tianhua, SHU Nian, HE Wei, DING Xueyong. A Predicted Model for Activity Interaction Coefficient Between Solutes in Alloy Solutions[J]. 金属学报, 2023, 59(11): 1533-1540.
[7] WANG Nan, CHEN Yongnan, ZHAO Qinyang, WU Gang, ZHANG Zhen, LUO Jinheng. Effect of Strain Rate on the Strain Partitioning Behavior of Ferrite/Bainite in X80 Pipeline Steel[J]. 金属学报, 2023, 59(10): 1299-1310.
[8] CHEN Huabin, CHEN Shanben. Key Information Perception and Control Strategy of Intellignet Welding Under Complex Scene[J]. 金属学报, 2022, 58(4): 541-550.
[9] WU Guohua, TONG Xin, JIANG Rui, DING Wenjiang. Grain Refinement of As-Cast Mg-RE Alloys: Research Progress and Future Prospect[J]. 金属学报, 2022, 58(4): 385-399.
[10] HAN Ruyang, YANG Gengwei, SUN Xinjun, ZHAO Gang, LIANG Xiaokai, ZHU Xiaoxiang. Austenite Grain Growth Behavior of Vanadium Microalloying Medium Manganese Martensitic Wear-Resistant Steel[J]. 金属学报, 2022, 58(12): 1589-1599.
[11] LUO Wenze, HU Long, DENG Dean. Numerical Simulation and Development of Efficient Calculation Method for Residual Stress of SUS316 Saddle Tube-Pipe Joint[J]. 金属学报, 2022, 58(10): 1334-1348.
[12] LIU Zhongqiu, LI Baokuan, XIAO Lijun, GAN Yong. Modeling Progress of High-Temperature Melt Multiphase Flow in Continuous Casting Mold[J]. 金属学报, 2022, 58(10): 1236-1252.
[13] HU Biao, ZHANG Huaqing, ZHANG Jin, YANG Mingjun, DU Yong, ZHAO Dongdong. Progress in Interfacial Thermodynamics and Grain Boundary Complexion Diagram[J]. 金属学报, 2021, 57(9): 1199-1214.
[14] WANG Youde, ZHOU Xiaodong, MA Rui, XU Shanhua. Stochastic Model for Surface Characterization of Structural Steel Corroded in Simulated Offshore Atmosphere[J]. 金属学报, 2021, 57(6): 811-821.
[15] XU Kun, WANG Haichuan, KONG Hui, WU Zhaoyang, ZHANG Zhan. Precipitation Kinetics of Al3Sc in Aluminum Alloys Modeled with a New Grouping Cluster Dynamics Model[J]. 金属学报, 2021, 57(6): 822-830.
No Suggested Reading articles found!