| SECONDARY RECRYSTALLIZATION TEXTURE IN 50%Ni-Fe ALLOY WITH CUBIC ORIENTATION |
| ZHANG Yumei;JIANG Wenhui Northeast University of Technology; ShenyangDept.of Materials Science and Engineering;Northeast University of Technology;Shenyang |
|
Cite this article:
ZHANG Yumei;JIANG Wenhui Northeast University of Technology; ShenyangDept.of Materials Science and Engineering;Northeast University of Technology;Shenyang. SECONDARY RECRYSTALLIZATION TEXTURE IN 50%Ni-Fe ALLOY WITH CUBIC ORIENTATION. Acta Metall Sin, 1988, 24(3): 217-220.
|
|
|
Abstract The crystal texture of secondary recrystallization of 50%Ni-Fe alloy has been inves-tigated quantitatively with X-ray Laue method. The samples used throughout the investigationwere several sheets of 50%Ni-Fe alloy cold rolled with 98% thickness reduction. Samples annealedbelow 1000℃ produced a cubic texture with fine grain size, while samples annealed at highertemperatures (1070, 1150, 1250, and 1240℃) produced secondary recrystallization, the ori-entation of which are different from the cubic one but belong to several definite types of orien-tations. For each annealing temperature, about 30 crystals were selected from a sample sheet forthe orientation determination with Laue method. The percent abundance of the texture componentsat several annealing temperatures has been calculated according to the relative volume of the crys-tals with the different orientations.
|
|
Received: 18 March 1988
|
1 Crede J H, Martin J P. J Appl Phys, 1949 20: 966 2 戴礼智,张信钰,刘壬宝.金属学报,1959;4:52 3 Ward C E, Littman M R. Trans AIME. 1955; 74: 422 4 Rathenau G M, Custer J F H. Philips Res Rep, 1949; 4: 241 5 Pfeifer F, Radeloff C. J Magn Magn Mater, 1980; 19: 190 6 Fahlenbrach H. Metallography. 1967; 21: 904 7 何开元.见:精密合金文集,上海:上海科学技术文献出版社,1980:1 8 Kang I K, Scholffield H H, Martin A P. J Appl Phys, 1967; 38: 1178 9 Aspden R G, Colling D A. Trans Metall Soc AIME, 1969; 245: 259 |