| STUDY OF A NEW TYPE SEMI-LINING ELECTRO-SLAG REMELTING |
| CHEN Chongxi;GAO Rongfu Beijing University of Iron and Steel TechnologyDeft.of Superalloy;Beijing University of Iron and Steel Technology; Beijing |
|
Cite this article:
CHEN Chongxi;GAO Rongfu Beijing University of Iron and Steel TechnologyDeft.of Superalloy;Beijing University of Iron and Steel Technology; Beijing. STUDY OF A NEW TYPE SEMI-LINING ELECTRO-SLAG REMELTING. Acta Metall Sin, 1988, 24(3): 221-228.
|
|
|
Abstract A new type of electroslag refining technique has been proposed andthe influence of superimposed DC density on the contents of active metal elementsas well as on the desulphurization and degassing have been studied. The resultsshow that the enerey consumption may be reduced by 41% by using this technique.During the semi-lining ESR under normal atmosphere, there is no evident loss ofactive metal elements, while the contents of O, N and S can be effectively reducedto 10ppm in superalloys GH49 and GH37. The ingot solidified along its axis andhas a compact microstructure. The secondary dendrite arm spacing of the semiliningESR ingot is about 1/3 shorter than that of tbe general ESR ingot.
|
|
Received: 18 March 1988
|
1 Elienne M, Mitchell A. Oxidation Losses of Low Levels of titanium During Electroslag Remelting, In: Bhat G K ed. Proc of the Second Int Symp on Electroslag Remelting Technology, Part II, Pittsburgh: Mellon Institute, 1969 2 Knights C F, Perkins R. Electroslag Refining, In: Proc of a Conf on Electroslag Refining, London: Iron and Steel Institute, 1973: 35 3 Gill L L, Harris K. Electroslag Refining, In: Proc of a Conf on Electroslag Refining, London: Iron and Steel Institute. 1973: 89 4 陈崇禧,王涌,傅杰,陈恩普.金属学报,1981;17:50 5 陈崇禧,高荣富,赵文祥.金属学报,1984;20:B137 6 Luchok J, Roberts R J. In: Proc of the 4th Int Symp on Electroslag Remelting Processes, Tokyo: The Iron and Steel Institute of Japan, 1973: 149 7 Holzgruber W. In: Bhat G K, Simkovich A eds. Proc of the 5th Int Symp on Electroslag and Other Special Melting Technologies, Pittsburgh: Carnegie-Meooln Institute, 1974: 70 8 Sullivan C P, Giamei A F, Versnyder F L. In: Bhat G K. Simkovich A eds. Proc of the 5th Int Symp on Electroslag and Other Special Melting Technologies. Pittsburgh: Carnegie-Mellon Institute. 1974: 525 9 #12 10 Holzgruber W, Machner P. Ploeckinger E, Boehler G. In: Foster E L ed. Transaction Vacuum Metallurgy Conf 1969, New York: American Vacuum Society, 1969: 415 11 Cordy J T, Kelley S L, Lherbier L W. In: Bhat G K, Lherbier L W eds. Proc Vacuum Metallutgy Conf 1984, Pittsburgh: Iron and Steel Society, 1984: 69 12 Boehler G, GB Pat 1230183, 1971 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|