| 应变方式对Al-Li合金超塑变形中空洞生长的影响 |
| 刘玉梅;赵友昌;于文学;高玉芹;郭昕昱;周海鹏;毛文锋;朱义元 |
| 吉林大学;中国航空工业总公司六二五研究所 |
|
| EFFECT OF STRAIN MODES ON CAVITY GROWING IN Al-Li ALLOY DURING SUPERPLASTIC DEFORMATION |
| LIU Yuniei;ZHAO Youchang;YU Wenxue;GAO Yuqin;GUO Hinyu; ZHOU Haipeng (Jilin University; Changchun 130023);MAO Wenfeng;ZHU Hiyuan(625 Institute Aviation Industries of China; Beijing 100024)(Manuscript received 1996-01-30; in revised form 1996-08-27) |
引用本文:
刘玉梅;赵友昌;于文学;高玉芹;郭昕昱;周海鹏;毛文锋;朱义元. 应变方式对Al-Li合金超塑变形中空洞生长的影响[J]. 金属学报, 1996, 32(12): 1238-1243.
,
,
,
,
,
,
,
.
EFFECT OF STRAIN MODES ON CAVITY GROWING IN Al-Li ALLOY DURING SUPERPLASTIC DEFORMATION[J]. Acta Metall Sin, 1996, 32(12): 1238-1243.
| 1PandeyMC.WadsworthJ,MukherjeeAK.MaterSciEng,1986;78:1152HancockJW.MetSci,1976;10:3193StowellMJ.MetSci,1980;14:2674MandelbrotBB,PassojaDE,PaullayAJ.Nalure,1984;308:721. |
|