Please wait a minute...
金属学报  1997, Vol. 33 Issue (1): 54-68    
  论文 本期目录 | 过刊浏览 |
金属缺陷能量学基础及掺杂晶界电子结构
王崇愚
冶金工业部钢铁研究总院;北京;100081
ENERGETICS OF METALLIC DEFECT AND ELECTRONIC STRUCTURE OF DOPED GRAIN BOUNDARY
WANG Chongyu (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing 100081)
引用本文:

王崇愚. 金属缺陷能量学基础及掺杂晶界电子结构[J]. 金属学报, 1997, 33(1): 54-68.
. ENERGETICS OF METALLIC DEFECT AND ELECTRONIC STRUCTURE OF DOPED GRAIN BOUNDARY[J]. Acta Metall Sin, 1997, 33(1): 54-68.

全文: PDF(2394 KB)  
摘要: 本文综述了我们发展建立的第一原理原子间相工作用势及原子间相互作用能的理论计算方法同时报告了在金属缺陷、掺杂晶界电子结构及晶体基本性质的研究中,能量函数作为理论基础的里要应用另一方面、基于第一原理及Green函数方法研究了具有重要应用潜势的金属间化合物的电子结构及掺杂效应,揭示了杂质-晶界复合的量子效应及其与合金特性及位错反应的相关机制;指出B,N等元素具有强化晶界作用,P,S为脆化元素,MI影响Ti—Al合金形变机制
关键词 : 原子间相互作用,  掺杂晶界,  电子结构    
Abstract:In this paper, we reviewed that a first principles interatomic potential and the theoretical calculation method of interaction energy between atoms, which are developed by us. Meanwhile, the important role of the energetic functions in the studies of the electronic structure of the impurity-grain boundary complexes and the basic properties of the crystal are reported. On the other hand, the electronic structure and the doping effect of intermetallic compound are studied by the use of first principles method and Green function method. The quantum effect of impurity-grain boundary complexes and the correlation mechanism between the electronic structure with the property of a1loy and dislocation reaction are explored.We find that Boron and Nitrogen have strengthening effect for the cohesion of grain boundary, and the phosphorous and sulphur are embrittle exements in the grain boundary of Ni-base alloy. Molybdemum influence the deformation mechanism of Ti-Al intermetallic compound.
Key words: interaction of atoms    doped grain boundary    electronic structure
收稿日期: 1997-01-18     
基金资助:国家自然科学基金
1 Wigner E P, Seitz F. Solid State Phys, 1995:95
2 Seitz F. Modern Theory of Solid. New York: McGraw-Hill, 1940
3 Callway J. Quantum Theory of the Solid StaIe, London: Academic Press INC, 1976
4 Hume Rothery W, Raynor G V. The Structure of Metals and AHoys. London: Inst Met, 1954
5 Hume Rothery W, Coles B R. Adv Phys, 1954; 149:3
6 Pauling L. Proc Nat Acad Sci USA, 195f; 533:36
7 Pauling L. The Nature of the Chemical Bond Third Edition, Ithaca N Y: Cornell University Press,1960
8 Eberhardt J J. MRS, 1995; 191:63
9 Ashby M F. Philos Trans Res Soc L0ndon, 1987; 393:A322
10 Wang Chongyu. Defecl Diffusion Forum, 1995; 125-126:79
11Wang Chongyu, An Feng. Gu Binling et al. Phys Rev, 1988; B38:3905
12Chen Ying, Wang Chongyu, Liu Fusui. Phys Rev, 1988; B37: 10510
13 Wang Chongyu, Liu Shenying, Han Linguang. Phys Rev, 1990; B41: 1359
14 Wang Chongyu, Wang Bing, Feng Peng et al. Phys Rev, 1992; B46:2693
15 Wang Chongyu, Chen Liqun et al. J Appl Phys, 1992; 71(1):239
16 Cao Junchu, Liu Fusui, Chongyu Wang. J Phys F: Met Phys, 1988; 18: 1839
17 Zeng Yueping, Wang Chongyu et al. Solid State Commun, 1990; 73:643
18 Wang Fuhe, Wang Chongyu, Yang Jinlong, J Phys Condens Matter, 1996; 8: 1
19 Wang Chongyu, Yue Yong, Liu Shenying. Phys Rev, 1990; B41:6591
20 Wang Huaiyu, Liu Fusui, Wang Chongyu. J Phys Con dens Matter, 1989; 1: 1983
21 Wang Chongyu, Li Junqing et al. Chin Sci Bulletin, 1990; 35: 197
22 Wang Bing, Wang Chongyu et al. Chin Sci Bulletin, 1992; 37: 189
23 Wang Chongyu, Zeng Yueping. Sci China, 1992; A35:1466
24 Wang Chongyu Zhao Dongliang. Mater Res Soc Sym Proc, 1994; 318:571
25 Wang Chongyu, Yue Yong et al. Sci China, l993; A36:1261
26 Wang Chongyu, Liu Shenying, Han Lingguang. Defect Dthesion Forum, 1996; 134-135:73
27 Wang Chongyu. Prog Nat Sci, 1996; 6:490
28 Yu Tao, Wang Chongyu, Wang Bing. J Mater Sci Technol, 1996; 12:427
29 Wang Chongyu, Dou Chuanyi, Zeng Yueping, Gao Lin. Proceedtw of International workshop onPhysics of materials, B5-1, 1989
30 Wang Fuhe, Zhang Haifeng, Wang Chongyu. Phys Rev, submitted
31 Wang Fuhe, Wang Chongyu. J Phys, submitted
32 Wang Chongyu, Yu Tao, Duan Wenhui, Wang Ligen. Phys Lett, 1995; A197:449
33 Mie G. Ann Phys, 1903; 11:657
34 Machlin E S. Acta Metall, 1974; 22:95
35 Girifalco L A, Weizer V G. Phys Rev, 1959; 114: 687
36 Melstein E. Phvs Status Solidi, 1971; B48:681
37 Maeda K, Vitek V, Sutton A P. Acta Metall, 1982; 30:2001
38 Finnis M W, Sinclair J S. Philos Mag, 1984; A50: 45
39 Daw M S, Baskes M I. Phys Rev, 1984; B29: 6443
40 Chen H P, Ellis D E. Phys Rev, 1989; B39: 12469
41 Blaisten-barojas E, Khanna S N. Phys Rev Lett, 1988; 61:1477
42 Tersoff J. Phys Rev Lett, 1986; 56:632
43 Chelikovesky J R, Phillips J C, Kamal M, Strauss M. Phys Rev Lett, 1989; 62: 292
44 Pettifor D G. Phys Rev Lett, 1989; 63: 2480
45 Moriarty J A. Phys Rev, 1989; B38:3199
46 Norskov J K, Lang N D. Phys Rev, 1980; B20: 2131
47 Scott M J, Zaremba E. Phys Rev, 1980; B22: 1564
48 Jacobsen K W, Norskov J K, Puska M J. Phys Rev, 1987; B35:7423
49 Jacobsen K W, Norskov J K. Phys Rev Lett, 1988; 60: 24964
50 Ellis D E, Painter G S. Phy Rev, 1970; B2: 2887
51 Delley B, Ellis D E, Freeman A J. Phys Rev, 1983; B27: 2132
52 Yang Jinlong, Wang Kelin. Phys Rev, 1993; B47: 4205
53 Seeger A, Schumacher D, Schilling W, Diehl J. Vacancler and interstitials in metals Amesterdam,North-Holland, 1970
54 Wycisk W, Feller-Kniepmeier M. J Nucl Mater, 1978; 69 / 70: 616
55 Kittel C. Introduction to solid state Physics. New York, Wiley, 1971
56 Heine V. In: Ehrenreich H, Seitz F, Turnbull D. Solid State Physics, New York: Academic, 1980:1
57 Johannes R L et al. Phys Rev Lett, 1976; 36: 372
58 Olson G B. In: Olson G B, Azrin M, Wright E S eds., Innovations in Ultrahigh-strength Steel Technology, Proceedings of Sagamore Conference, No.34(Sagamore Army Material Research Conference, LakeGeorge, New York), 1987: 3, and References therein
59 Aust A T, Hanneman R E, Nissen P et al. Acta Metall 1968; 16:291
60 Williams T M, Stoneham A M, Harries D R. Met Sci, 1976; 10:14
61 Paintendre N et al. In: Bett, W et al eds., Hteh Temperature AHy for Gas Turbins and otherApllication, Part 2, Reidel, Dordrecht, 1986:877
62 Wang Ligen, Wang Chongyu. Phys Rev, submitted
63 Wang Ligen, Wang Chongyu. J Phys, submitted
64 Wu R Q, Freeman A J, Olson G B. Phys Rev, 1994; B50:75
65 Wu R Q, Freeman A J, Olson G B. J Mater Res, 1992; 7:2433
66 Tang S P, Freeman A J, Olson G B. Phys Rev, 1993; B47:2441
67 Wu R Q, Freeman A J, Olson G B. Phys Rev, 1993; B47:6855
68 Tang S P, Freeman A J, Olson G B. Phys Rev, 1994; B50: 1
69 Briant C L, Messmer R P. Philos Mag, 1980; B42:569
70 Losch W. Acta Metall, 1979; 27: 1885, Scr Metall, 1979; 13: 661
71 Haydock R. J Phys Colloq, 1981; (C14): 3807
72 Eberhart M E, Johnson K H, Latanision R M. Acta Metall, 1984; 32: 955
73 Eberhart M E, Latanision R M, Johnson K H. Acta Metall, 1985: 33: 1769
74 Eberhart M E, Vvedensky D D. Phys Rev Lett, 1987; 61: 58
75 Vvedensky D D, Eberhart M E. Philos Mag Lett, 1987; 157: 55
76 Frisch H L, Patel J R. Phvs Rev Lett, 1967; 18: 784
77 Masuda-Jindo K. Mater Sci Forum. 1989; 97: 37
78 Morinaga M et al. Acta Metall Mater, 1990; 38: 25
79 Morinaga M et al. Modeltw Simmu Mater Sci Eng, 1993; 151: 1
80 Messmer R P, Briant C L. Acta Metall, 1982: 30: 457
81 Messmer R P, Briant C L. Acta Metall, 1982; 30: 181 1
82 Song Quanming, Wang Chongyu, Wen Shulin. J APPl Phys, submitted
83 Troiano A R. Trans ASM, 1960: 54:52
84 Krasko G L. Scr Met Mater, 1993: 1543:28
85 Krasko G L, Olson G B. Solid State Commun, 1990; 147:76
86 Liu C T. Scr Metall Mater, 1991; 25: 1231
87 Aoki K, Izumi O. Nippon Kinzoku Gakkaishi, 1979; 43: 1190
88 Takasugi T, Izumi O. Acta Metall, 1985; 33: 1259
89 Aoki K. Mater Trans JIM, 1990; 31:443
90 Masuda-Jindo K J. J Phys Colloq, 1982; 43:921
91 Liu C T, White C L, Horton J A. Acla Metall, 1985; 33:213
92 Chen S P, Voter A V, Albers R C, Boring A M, Hay P J. J Mater Res, 1990; 5:955
93 Greenberg B A. Phys Status Solidi, 1973; B55:59
94 Shechtman D et al. Metall Trans, 1974; A5: 1373
95 Lipsitt H A et al. Metall Trans, 1975; A6: 1991
96 Kawabata T et al. AcIa Metall, 1985; 33: 1355
97 Hug G et al. Philos Mag, 1986; A54:47
98 Hug G et al. Philos Mag, 1988; A57:499
99 Court S A et al. Philos Mag, 1990; A61: 141
100 Seehra S. J Mater Res, 1993: 8:989
101 Morihiko Nakamura, J Mater Res, 1993; 8:68
102 Zhang X D, Loretto M H. Philos Mag, 1995; A71:421
103 Hanamura T et al. J Mater Res, 1988; 3:656
104 Hanamura T et aI. J Mater Sci Lett, 1989; 8:24
105 Huang S C el al. MRS Meettw, Boston, 1988
106 Kawabata T et al. MRS Meettw, Boston, 1988
107 Greenberg B F et al. Scr Metall, 1988; 22:859
108 Fox A G. AcIa Meall MatIer, 1994; 42:3929
109 Anisimov V I et al. Phys Met Metall, 1987; 63: 192
110 Erschbaumer H, Podloucky R, R0gl P, Temnitschka G, Wagner R. Intermetallics, 1:99
111 Xu J X. J Mater Res, 1994; 9: 1755
112Fu CL,Yoo M H.Philos Mag Lett,1990;62:159
113Jund P,Zhong W,Tomanek D Phys Rev,1995;B51:9569
114Zhou J,Fu C L,Yoo M H.Intermetallics,1995; 3:265
115Hanamura T et al.J Mater Res,1988;3:656
116Hanamura T et al.J Mater Sci Lett, 1989; 824
[1] 皇甫顥, 王子龙, 刘永利, 孟凡顺, 宋久鹏, 祁阳. W1 - x Ir x 固溶合金几何结构、电子结构、力学和热力学性能的第一性原理计算[J]. 金属学报, 2022, 58(2): 231-240.
[2] 王硕, 王俊升. Al-Li合金中 δ′/θ′/δ′复合沉淀相结构演化及稳定性的第一性原理探究[J]. 金属学报, 2022, 58(10): 1325-1333.
[3] 陈丽群, 邱正琛, 于涛. Ru对NiAl[100](010)刃型位错电子结构的影响[J]. 金属学报, 2019, 55(2): 223-228.
[4] 毛萍莉,于波,刘正,王峰,鞠阳. Mg-Zn-Ca合金中AB2型金属间化合物电子结构和弹性性质的第一性原理计算[J]. 金属学报, 2013, 49(10): 1227-1233.
[5] 黄炼,高坤元,文胜平,黄晖,王为,聂祚仁. Al3M(M=Ti, Zr, Hf)亚稳相和平衡相的价电子结构分析[J]. 金属学报, 2012, 48(4): 492-501.
[6] 周惦武 刘金水 徐少华 彭平. Al2Sr和Mg2Sr相结构稳定性与弹性性能的第一原理计算[J]. 金属学报, 2011, 47(10): 1315-1320.
[7] 周惦武 徐少华 张福全 彭平 刘金水. ZA62镁合金中AB2型金属间化合物的结构稳定性与弹性性能的第一原理计算[J]. 金属学报, 2010, 46(1): 97-103.
[8] 张国英 张辉 方戈亮 杨丽娜. Al--Zn--Mg--Cu 系铝合金中不同区域电子结构及应力腐蚀机理分析[J]. 金属学报, 2009, 45(6): 687-691.
[9] 梁初; 许灵艳; 姚春贤; 蓝志强; 黎光旭; 郭进 . Co对ZrMn2合金贮氢性能影响的第一性原理研究[J]. 金属学报, 2008, 44(3): 351-356 .
[10] 刘贵立 . 基于递归法钛合金应力腐蚀机理研究[J]. 金属学报, 2007, 43(3): 249-253 .
[11] 陈丽群; 邱正琛 . Fe中刃型位错扭折处掺S的电子结构[J]. 金属学报, 2007, 43(10): 1015-1019 .
[12] 姚强; 张羽; 孙坚 . 过渡金属元素在NbCr2 Laves相中晶格占位的第一性原理计算[J]. 金属学报, 2006, 42(8): 801-804 .
[13] 陶辉锦; 谢佑卿; 彭红建; 余方新; 刘锐锋; 李晓波 . fcc,压稳hcp和bcc-Cu的原子状态及物理性质随温度的变化关系[J]. 金属学报, 2006, 42(6): 565-571 .
[14] 菅晓玲; 黄存可; 郑定山; 韦文楼; 郭进 . ZrMn2合金及其氢化物的电子结构与成键特性的第一原理研究[J]. 金属学报, 2006, 42(2): 123-128 .
[15] 袁宏宽; 陈洪 . V12M团簇的电子结构和磁性的第一性原理研究[J]. 金属学报, 2006, 42(12): 1285-1290 .