| Pb0.5Sr0.5TiO3精细结构的第一性原理分析 |
| 张威虎1;2;3 ;张富春1;2;3 ;张志勇4 ;阎军峰4 |
1. 中国科学院西安光学精密机械研究所; 西安 710068
2. 中国科学院研究生院; 北京 100039
3. 延安大学物理与电子信息学院; 延安 716000
4. 西北大学信息科学与技术学院; 西安 710127 |
|
| FIRST–PRINCIPLE ANALYSYS ON FINE STRUCTURE OF Pb0.5Sr0.5TiO3 |
| ZHANG Weihu 1;2;3; ZHANG Fuchun 1;2;3; ZHANG Zhiyong 4; YAN Junfeng 4 |
1. Xi’an Institute of Optics and Precision Mechanics; Chinese Academy of Sciences; Xi’an 710068
2. Graduate University of Chinese Academy of Sciences; Beijing 100039
3. College of Physics & Electronic Information; Yan’an University; Yan’an 716000
4. Information Science and Technology Institution; Northwest University; Xi’an 710127 |
引用本文:
张威虎 张富春 张志勇 阎军峰. Pb0.5Sr0.5TiO3精细结构的第一性原理分析[J]. 金属学报, 2009, 45(2): 217-222.
.
FIRST–PRINCIPLE ANALYSYS ON FINE STRUCTURE OF Pb0.5Sr0.5TiO3[J]. Acta Metall Sin, 2009, 45(2): 217-222.
| [1] Kang D H, Kim J H, Park J H, Yoon K H. Mater Res Bull, 2001; 36: 265
[2] Chung H J, Woo S I. J Vac Sci Technol, 2001; 19B: 275
[3] Kim G H, Kim K T, Kim D P, Kim C I. Thin Solid Films, 2004; 447–448: 688
[4] Hamata Y. J Electron Ceram Jpn, 1988; 19: 3
[5] Cohen R E. Nature, 1992; 358: 136
[6] Bungaro C, Rabe K M. Phys Rev, 2005; 71B: 035420
[7] Iniguez J, Vanderbilt D, Bellaiche L, Vanderbilt D, Bellaiche L. Phys Rev, 2003; 67B: 224107
[8] Peng Y P, Wang Y X, Zhang L, Zhang P L, Zhong W L. Acta Phys Sin, 2000; 49: 1140
(彭毅萍, 王渊序, 张 磊, 张沛霖, 钟维烈. 物理学报, 2000; 49: 1140)
[9] Wang Y X, Zhong W L, Wang C L, Zhang P L. Acta Phys Sin, 2002; 51: 171
(王渊旭, 钟维烈, 王春雷, 张沛霖. 物理学报, 2002; 51: 171)
[10] Kang H D, Kim J H, Park J H, Yoon K H. Mater Res Bull, 2001; 36: 265
[11] Jain A, Majumder S B, Guo R, Bhalla A S, Katiyar R S. Mater Lett, 2002; 56: 692
[12] Kim K T, Kim C I. Thin Solid Films, 2002; 420–421: 544
[13] Segall M D, Lindan P J D, Probert M J. J Phys Condens Matter, 2002; 14: 2717
[14] Marlo M. Phys Rev, 2000; 62B: 2899
[15] Perdew J P, Chevary J A, Vosko S H, Jackson K A, Pederson M R, Singh D J. Phys Rev, 1992; 46B: 66713
[16] Somiya Y, Bhalla A S, Eric L. Cross Int J Inorg Mater, 2001; 3: 709
[17] Xing X, Chen J, Deng J X, Liu G. J Alloys Compd, 2003; 360: 286
[18] Burstein E. Phys Rev, 1954; 93: 632
[19] Cohen R E, Krakauer H. Phys Rev, 1990; 42B: 6416 |
|