| NiTi形状记忆合金热压缩变形行为及本构关系 |
| 张红钢;何勇;刘雪峰;谢建新 |
| 北京科技大学材料科学与工程学院; 北京 100083 |
|
| HOT DEFORMATION BEHAVIOR AND CONSTITUTIVE RELATIONSHIP OF NiTi SHAPE MEMORY ALLOY DURING COMPRESSION AT ELEVATED TEMPERATURES |
| ;;; |
| 北京科技大学 |
引用本文:
张红钢; 何勇; 刘雪峰; 谢建新 . NiTi形状记忆合金热压缩变形行为及本构关系[J]. 金属学报, 2007, 43(9): 930-936 .
,
,
,
.
HOT DEFORMATION BEHAVIOR AND CONSTITUTIVE RELATIONSHIP OF NiTi SHAPE MEMORY ALLOY DURING COMPRESSION AT ELEVATED TEMPERATURES[J]. Acta Metall Sin, 2007, 43(9): 930-936 .
[1]Kawaguchi Y,Katsube K,Murahashi M,Yamada Y.Wire J Int,1991;24:53 [2]Liu X F,He Y,Bi C W,Xie J X.Chin J Rare Met,2005; 29:762 (刘雪峰,何勇,毕重武,谢建新.稀有金属,2005;29:762) [3]Zhang S H,Wang Z T,Zhang W H.Machinist Met Form- ing,2005;(7):16 (张士宏,王忠堂,张伟红.机械工人:热加工,2005;(7):16) [4]Zhang W H,Zhang S H.Acta Metall Sin,2006;42:1036 (张伟红,张士宏.金属学报,2006;42:1036) [5]Li L,Zhou J,Duszczyk J.J Mater Process Technol,2006; 172:372 [6]Krauss G.Defornation Processing and Structure.Metals Park,OH:American Society for Metals,1984:109 [7]Rao K P,Prasad Y K D V,Hawbolt E B.J Mater Process Technol,1996;56:897 [8]Rao K P,Hawbolt E B.ASME J Eng Mater Technoly, 1992;114:116 [9]Yuan H,Liu W C.Mater Sci Eng,2005;A408:281 [10]Lyszkowski R,Bystrzycki J.Intermetallics,2006;14:1231 [11]Otsuka K,Ren X B.lntermetallics,1999;7:511 [12]Chen G L,Lin J P.Physical Metallography Basis of Or- dered Intermetallic Compound Structure Materials.Bei- jing:Metallurgical Industry Press,1999:140 (陈国良,林均品.有序金属间化合物结构材料物理金属学基础.北京:冶金工业出版社,1999:139) [13]Lou B Y,Liu M S,Mao Z Y.Mater Sci Eng,1995;13(2): 19 (楼白杨,刘茂森,毛志远.材料科学与工程,1995;13(2):19) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |