| 冶金炉用填充球蓄热室传热过程的数值模拟及热工特性 |
| 蔡九菊 于娟 |
| 东弱大学材料与冶金学院; 沈阳 110006 |
|
引用本文:
蔡九菊; 于娟 . 冶金炉用填充球蓄热室传热过程的数值模拟及热工特性[J]. 金属学报, 2000, 36(4): 417-421 .
[1] Martin T. Ind Heat, 1988; 55: 12 [2] John N N, Lexington K. Iron Steel Eng, 1987; 64: 20 [3] Lupton D. Steel Times Int, 1989; 13: 21 [4] Yu J. Master Thesis, Northeastern University, Shenyang,1999: 14(于娟.东北大学硕土学位论文,沈阳,1999:14) |
|