| Zr-Ti-Cu-Ni-Be-Fe大块非晶合金晶化动力学效应 |
| 赵德乾 C.H.Shek 汪卫华 |
| 香港城市大学物理及材料科学系; 香港 |
|
引用本文:
赵德乾; C.H.Shek; 汪卫华 . Zr-Ti-Cu-Ni-Be-Fe大块非晶合金晶化动力学效应[J]. 金属学报, 2001, 37(7): 754-758 .
[1] Peker A, Johnson W L. Appl Phys Lett, 1993, 63: 2342 [2] Wang W H, Wang W K, Bai H Y. Sci Chin, 1998; 41A:756 [3] Inoue A, Zhang T, Nishiyama N, Ohba K, Masumoto T.Mater Trans JIM, 1993; 34: 1234 [4] Shen T D, Schwarz R B. Appl Phys Lett, 1999; 75: 49 [5] Zhao D Q, Zhuang Y X, Zhang Y, Pan M X, Wu G H,Meng L Q, Wang W H. Acta Metall Sin, 2000; 36: 329 (赵德乾,庄艳歆,张勇,潘明祥,吴光恒,孟丽琴,汪卫华.金属学报,2000;36:329) [6] Busch R, Kim Y J, Johnson W L. J Appl Phys, 1995; 77:4039 [7] Tsao S S, Spaepen F. Acta Metall, 1989; 33: 881 [8] Wang W H, Wei Q, Friedrich S. Phys Rev,1998; 57B: 8211 [9] Guo Y C, Wang Z X. Amorphous Physics. Beijing: Science Press. 1984: 140 (郭贻诚,王震西.非晶态物理学.北京:科学出版社,1984:140) [10] Zhuang Y X, Zhao D Q, Zhang Y, Wang W H. Pan M X.Sci Chin, 2000; 43A: 1195 [11] Schroers J, Masuhr A, Johnson W L, Busch R. Phys Rev,1999; 60B: 11855 [12] Frank W, Horner A, Scharwaechter P, Kronmuller H.Mater Sci Eng, 1994; 179/180A: 36 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|