Zr55Al10Ni5Cu30块状非晶合金靠近玻璃转变点的等温纳米晶化 |
张庆生 邓玉福 贺连龙 |
中科院金属所沈阳材料科学国家(联合)实验室 110016 |
|
引用本文:
张庆生; 邓玉福; 贺连龙 . Zr55Al10Ni5Cu30块状非晶合金靠近玻璃转变点的等温纳米晶化[J]. 金属学报, 2003, 39(3): 301-304 .
[1] Zhang T, Inoue A, Masumoto T, Mater Trans JIM, 1991;32: 1005 [2] Peker A. Johnson W L. Appl Phys Lett. 1993; 63: 2342 [3] Inoue A. Ada Mater, 2000; 48: 279 [4] Kato H, Inoue A. Mater Trans JIM, 1997: 38: 793 [5] Choi-Yim H, Johnson W L. Appl Phys Lett, 1997; 71:3808 [6] Dandliker R B, Conner R D, Johnson W L. J Mater Ras,1998; 13: 2896 [7] Choi-Yim H, Busch R, Kostcr V, Johnson W L. ActaMater, 1999; 47: 2455 [8] Inoue A. Intermetallics, 2000; 8: 455 [9] Inoue A, Zhang T, Chen M W, Sakurai T. ,7 Mater Res,2000; 15: 2195 [10] Xing L Q, Bertram! C, Dallas J-P, Cornet M, Mater SciEng, 1998; 241A: 216 [11] Xing L Q, Li Y, Tamesh K T, Li J, Hufnagel T C. PhysRev, 2001; 64B: 18202 [12] Schneider S, Thiyagarajan P, Johnson W L. Appl PhysLett, 1996; 68: 493 [13] Yavari A R, Le Moulec A, Botta W J, Inoue A, Rej-mankova P, Kvick A. J Non-Cryst Solids, 1999; 247: 31 [14] Yavari A R, Inoue A, Zhang T, Botta F W J, Kvick A.Scr Mater, 2001; 44: 1239 [15] Hufnagel T C, Gu X F, Munkholm A. Metall Mater Trans,2001; 42: 562 [16] Kulik T. J Non-Cryst Solids, 2001; 287: 145 [17] Xing L Q, Eckert J, Loser W, Schultz L, Herlach D M. Philos Mag, 1999; 79A: 1095 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|