| 金属合金溶液热力学模型研究进展 |
| 乐启炽;张新建;崔建忠;路贵民 |
| 东北大学材料电磁过程研究教育部重点实验室; 沈阳 110004 |
|
| Progression of Research on Thermodynamic Model of Metallic Alloy Melts |
| LE Qichi; ZHANG Xinjian; CUI Jianzhong; LU Guimin |
| Key Lab of Electromagnetic Processing of Materials; Ministry of Education; Northeastern University; Shenyang 1110004 |
引用本文:
乐启炽; 张新建; 崔建忠; 路贵民 . 金属合金溶液热力学模型研究进展[J]. 金属学报, 2003, 39(1): 35-42 .
,
,
,
.
Progression of Research on Thermodynamic Model of Metallic Alloy Melts[J]. Acta Metall Sin, 2003, 39(1): 35-42 .
[1] Liang Y J. Physical chemistry. Beijing: Metallurgy Industry Press, 1982: 146(梁英教.物理化学.北京:冶金工业出版社, 1982:146) [2] Darken L S. TMS-AIME, 1967; 239: 80 [3] Van Laar. Z Physik Chem, 1910; 72: 723 [4] Wilson G M. J Amer Chem Soc, 1964; 20: 127 [5] Tsuboka T, Katayama T. J Chem Eng Jpn, 1975; 8: 1975 [6] Tao D P. Acta Metall Sin, 1991; 27: B380(陶东平.金属学报, 1991;27:B380) [7] Tao D P. Matall Trans B, 1992; 23B: 526 [8] Renon H, Prausnitz J M. AIChE J, 1968; 14: 135 [9] Hou H Y, Xie G, Liu G H, Chen S R. Chin J Nonfer Met, 1998; 8(s2) : 707(侯怀宇,谢刚,刘国华,陈书荣.中国有色金属学报,1998;8(s2) :707) [10] Zhang Z C, Su H, Wu Z, Chen N Y, Peng R W. Chin J Rare Met, 1998; 22: 341(张兆春,苏航,吴铸,陈念贻,彭瑞伍.稀有金属,1998;22:341) [11] Hou H Y, Xie G, Liu G H, Chen S R. Acta Metall Sin, 1999; 35: 292(侯怀宇,谢刚,刘国华,陈书荣.金属学报,1999;35:292) [12] Abrams D S, Prausnitz J M. AICHE J, 1975; 21: 116 [13] Walas S M. Phase equilibria in chemical engineering, London: Butterworth Publishers, 1985: 209 [14] Margules M. Sitz-Ber Math-Naturw KL Bayer Akad Wiss Munchen Iia, 1895; 104: 583 [15] Hildebrand J H, Scott R L. Regular solution. New York: Prentiss-Hall, Englewood Cliffs, 1952 [16] Hardy H K A. Acta Met, 1953; 1: 202 [17] Redlich O, Kister A T, Turnquist C E. Chem Eng Prog Symp Ser, 1952; 48: 49 [18] Williams R O. CALPHAD, 1991; 15: 1 [19] Hultgren R, Desai P, Hawkins D, Gleiser M, Kelley K K. Selected Values of Thermodynamic Properties of Metals and Alloys. Ohio: ASM, Metals Park, 1973 [20] Pelton A D, Bale C W. Metall Trans A, 1986; 17A: 1057 [21] Bale C W and Pelton A D. Metall Trans A, 1990; 21A: 1997 [22] Williams R O. Trans AIME, 1969; 245: 2565 [23] Su Y, Wang Z C. Acta Metall Sin, 1995; 31: B255(苏轶,王之昌.金属学报,1995;31:B255) [24] Lumsden J. Thermodynamics of Alloys. London: TheInst. of Metal, 1952: 20 [25] Krupkowski A. Bull De L'ACADEMIE Polo Des Sci,1969; 17: 88 [26] Hajra J P. Metall Trans B, 1980; 11B: 215 [27] Esdaile J D. Metall Trans B, 1982; 12B: 213 [28] Choi S D, Hucke E E. CALPHAD, 1990; 14: 367 [29] Chen S L, Zhou G Z. CALPHAD, 1989; 13: 13 [30] Sommer P. Z Metallkde, 1982; 72: 72 [31] Miedema A R, de Chatel P F, de Boer F R. Physica, 1980;100B: 1 [32] Tanaka T, Gokcen N A, Morita Z. Z Metallkde, 1990; 81:49 [33] Ding X Y, Wang W Z. ACTA Metall Sin, 1994; 30: B444(丁学勇,王文忠.金属学报, 1994;30:B444) [34] Bonnier E, Caboz R. C R Acta Sci, 1960; 520, 527 [35] Hillert M. CALPHAD, 1988; 12: 257 [36] Darken L S.J Am Chem Soc, 1950; 72: 2909 [37] Toop G W. TMS-AIME, 1965; 233: 850 [38] Kohler F. Chemie, 1960; 91: 738 [39] Muggianu Y M Gambino M, Bros J P. J Chimie Physique, 1975; 72: 83 [40] Li R Q. CALPHAD, 1989; 13: 61 [41] Hillert M. CALPHAD, 1980; 4: 1 [42] Zhou G Z. Acta Metall, 1997; 33(2) : 126 [43] Luck R, Gerling U, Predel B. Z Metallkde, 1986; 77: 442 [44] Gather B. Calphad-Conference, Liege, 1983 [45] Zhang S B, Li D Z. The Principle and Calculation of Phase Diagram and its Application in Metallurgy. Beijing: Metallurgy Industry Press, 1986(张圣弼,李道子.相图-原理、计算及在冶金中的应用.北京,冶金工业出版社, 1986) [46] Zhou K G. CALPHAD, 1995; 19: 315 [47] Shen J Y, Hao Y W, Zhou C H, Ling L. Ada Metall Sin, 1996; 32: 943(沈剑韵,郝耀武,周传华,凌铃.金属学报,1996;32:943) [48] Chen S L, Cui J Q, Chen T K, Zhou G Z. CALPHAD,1989; 13: 225 [49] Wang Z C, Luck R, Predel B. CALPHAD, 1990; 14: 217 [50] Wang Z C, Luck R, Predel B. CALPHAD, 1990; 14: 235 [51] Howell W J, Eckert C A. Z Metallkde, 1990; 81: 335 [52] Krylov A S, Katsnelson A M. Z Metallkde, 1993; 84: 641 [53] Ding X Y, Fan P, Han Q Y. Acta Metall Sin, 1994; 30:B49(丁学勇,范鹏,韩其勇.金属学报, 1994;30:B49) [54] Wagner C. Thermodynamics of Alloys Reading, MA:Addison-Wesley, 1962: 51 [55] Wei Q C. Metallurgical Thermodynamics. Chongqing:Chongqing University Press, 1996: 148, 152(魏庆成.冶金热力学.重庆:重庆大学出版社, 1996:148,152) [56] Guggenheim E A. Mixture. Oxford: Oxford ClarendonPress, 1952 [57] Oriant R A. The physical Chemistry of Metallic Solutionsand Intermetollic Compounds, Paper 2A, London: H MStationery Office, 1959: 102 [58] Alcock C B, Richardson F D. Acta Met, 1958; 6: 385 [59] Lupis C H, Elliott J F. Acta Met, 1966; 14: 529 [60] Lupis C H, Elliott J F. Acta Met, 1966; 14: 1019 [61] Darken L S. TMS-AIME, 1967; 239: 90 [62] Schumann R Jr. Metall Trans B, 1985; 16B: 807 [63] Pelton A D, Bale C W. Matall Trans A, 1990; 17A: 1211 [64] Srikanth S, Jacob K T. Metall Trans B, 1988; 19B: 269 [65] Hajra J P, Frohberg M G. Metall Trans B, 1992; 23B: 23 [66] Ma Z T, Ohser J, Janke D. Acta Metall Sin, 1998; 34: 753(马中庭,Ohser J,Janke D.金属学报,1998,34:753) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|